MANUFACTURING METHOD FOR OPTICAL FILM

PROBLEM TO BE SOLVED: To provide a manufacturing method for an optical film of which the residual phase difference brought about by an extrusion method and the flare are small. SOLUTION: The optical film is manufactured by a method wherein a thermoplastic resin film melted and extruded like a sheet...

Full description

Saved in:
Bibliographic Details
Main Authors JIYUNI YASUTO, OKADA YASUMASA
Format Patent
LanguageEnglish
Published 10.06.2004
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
Abstract PROBLEM TO BE SOLVED: To provide a manufacturing method for an optical film of which the residual phase difference brought about by an extrusion method and the flare are small. SOLUTION: The optical film is manufactured by a method wherein a thermoplastic resin film melted and extruded like a sheet is brought into close contact with and cooled by a metallic cooling roll having a glass transition temperature of +20 to -50°C, while an electric charge is given only to the vicinity of the end part of the film at a point where the film comes into contact with the roll, so as to conduct edge pinning, and the film is pulled upward almost vertically to be peeled from the cooling roll, by a rubber roll provided above the cooling roll and having the rotational torque controlled. The tension of this optical film is 98 N or below per 1 m width thereof and the temperature thereof just before the contact with the rubber roll is a room temperature to the room temperature + 50°C. The wrap angle of the thermoplastic resin film to the rubber roll is made 90-240 degrees. COPYRIGHT: (C)2004,JPO
AbstractList PROBLEM TO BE SOLVED: To provide a manufacturing method for an optical film of which the residual phase difference brought about by an extrusion method and the flare are small. SOLUTION: The optical film is manufactured by a method wherein a thermoplastic resin film melted and extruded like a sheet is brought into close contact with and cooled by a metallic cooling roll having a glass transition temperature of +20 to -50°C, while an electric charge is given only to the vicinity of the end part of the film at a point where the film comes into contact with the roll, so as to conduct edge pinning, and the film is pulled upward almost vertically to be peeled from the cooling roll, by a rubber roll provided above the cooling roll and having the rotational torque controlled. The tension of this optical film is 98 N or below per 1 m width thereof and the temperature thereof just before the contact with the rubber roll is a room temperature to the room temperature + 50°C. The wrap angle of the thermoplastic resin film to the rubber roll is made 90-240 degrees. COPYRIGHT: (C)2004,JPO
Author JIYUNI YASUTO
OKADA YASUMASA
Author_xml – fullname: JIYUNI YASUTO
– fullname: OKADA YASUMASA
BookMark eNrjYmDJy89L5WRQ9XX0C3VzdA4JDfL0c1fwdQ3x8HdRcPMPUvAPCPF0dvRRcPP08eVhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGBiaGZgYWhpaOxkQpAgDMbyVs
ContentType Patent
DBID EVB
DatabaseName esp@cenet
DatabaseTitleList
Database_xml – sequence: 1
  dbid: EVB
  name: esp@cenet
  url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP
  sourceTypes: Open Access Repository
DeliveryMethod fulltext_linktorsrc
Discipline Medicine
Chemistry
Sciences
Edition 7
ExternalDocumentID JP2004160819A
GroupedDBID EVB
ID FETCH-epo_espacenet_JP2004160819A3
IEDL.DBID EVB
IngestDate Fri Jul 19 15:58:09 EDT 2024
IsOpenAccess true
IsPeerReviewed false
IsScholarly false
Language English
LinkModel DirectLink
MergedId FETCHMERGED-epo_espacenet_JP2004160819A3
Notes Application Number: JP20020328814
OpenAccessLink https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20040610&DB=EPODOC&CC=JP&NR=2004160819A
ParticipantIDs epo_espacenet_JP2004160819A
PublicationCentury 2000
PublicationDate 20040610
PublicationDateYYYYMMDD 2004-06-10
PublicationDate_xml – month: 06
  year: 2004
  text: 20040610
  day: 10
PublicationDecade 2000
PublicationYear 2004
RelatedCompanies SEKISUI CHEM CO LTD
RelatedCompanies_xml – name: SEKISUI CHEM CO LTD
Score 2.6016972
Snippet PROBLEM TO BE SOLVED: To provide a manufacturing method for an optical film of which the residual phase difference brought about by an extrusion method and the...
SourceID epo
SourceType Open Access Repository
SubjectTerms AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
Title MANUFACTURING METHOD FOR OPTICAL FILM
URI https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20040610&DB=EPODOC&locale=&CC=JP&NR=2004160819A
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1bS8MwFD7MKeqbTkU3lSLat2JT05Y-FOnSllrsBWllb2NpK4gwh6vs73sSV93T3kICJxc4t-T7TgBuRYEWY-bMJP1Mo5TrqFKUaqZj2IQ4FUYkguCcpFZU0nhiTnrw0XFhZJ3QlSyOiBpVob630l4v_i-xfImtXN7zd-z6fAwL11e77Fi4J131x26QZ37GVMbcOFfTFzlGLOH_vB3YxTjaFviv4HUsaCmLTZ8SHsFejuLm7TH0mvkADlj39doA9pP1izc218q3PIG7xEvL0GNFKRAMShIUUeYrmMUpWV6IsgZK-PScnMJNGBQs0nC-6d_upnG-sbaHM-hj2t-cg_JW1Y6hcwzAuE1pbfLatEllNYIpWhNiX8Boi6Dh1tERHP4iUCw0w5fQb7--myt0ri2_lofyA_bPd1g
link.rule.ids 230,309,783,888,25578,76884
linkProvider European Patent Office
linkToHtml http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1JS8NAFH7UKtabVkWtSxDNLZiJk8QcgqRZSGM2JJHeQrMIItRiI_5934yN9tTbMANvFnjbzPu-AbhhBC3KzJhx-JlEaSmjSlEqqYaiE2JUGJEwgHMUa35Og6k67cF7h4XhPKHfnBwRNapCfW-5vV78X2I5vLZyeVe-YdfHo5eZjthlx8w9yaIzNt00cRJbtG0zSMX4mY8Rjfk_awu2McZ-YET77suYwVIW6z7F24edFMXN2wPoNfMhDOzu67Uh7EarF29srpRveQi3kRXnnmVnOatgECI38xNHwCxOSNKM0RoI3iSMjuDaczPbl3C-4m93RZCure3-GPqY9jcnILxWtaHIJQZgpU5prZa1qpNKaxhStCZEP4XRBkFnG0evYOBnUViEk_hpBHu_1SgamuRz6LefX80FOtq2vOQH9AO3QXpI
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=MANUFACTURING+METHOD+FOR+OPTICAL+FILM&rft.inventor=JIYUNI+YASUTO&rft.inventor=OKADA+YASUMASA&rft.date=2004-06-10&rft.externalDBID=A&rft.externalDocID=JP2004160819A