PROCESS FOR THE CONTINUOUS PRODUCTION OF NIOBIUM PENTACHLORIDE OF AT LEAST 99 MASS PERCENT PURITY

Ferroniobium and chlorine gas are heated to 600-800 deg.C to form a mixture of (NbCl5)2, Fe2Cl6, Al2Cl6 and SiCl4 gases that are purified by passing through a column of hot NaCl pieces (at 280-300 deg.C). The impurities react with NaCl and collect at the bottom of the column in liquid form, the puri...

Full description

Saved in:
Bibliographic Details
Main Authors JUHASZ,ERZSEBET,HU, NEMETH,JANOS,HU, IVAN,LASZLO,HU
Format Patent
LanguageEnglish
Published 30.06.1986
Edition4
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Ferroniobium and chlorine gas are heated to 600-800 deg.C to form a mixture of (NbCl5)2, Fe2Cl6, Al2Cl6 and SiCl4 gases that are purified by passing through a column of hot NaCl pieces (at 280-300 deg.C). The impurities react with NaCl and collect at the bottom of the column in liquid form, the purified (NbCl5)2 steam is then condensed at below 280 deg.C. The granules of NaCl are of 30-40 mm dia. and are replaced regularly.
Bibliography:Application Number: HU19840002066