Menetelmä epikloorihydriinihartsin valmistamiseksi

Disclosed is a two-step process for making an epichlorohydrin resin involving reacting the epichlorohydrin with a polyamine in a mixture first at a temperature of 25-40 DEG C and then heating the mixture at 25-85 DEG C.

Saved in:
Bibliographic Details
Main Author BOWER,BARTON K
Format Patent
LanguageFinnish
Swedish
Published 15.09.2003
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Disclosed is a two-step process for making an epichlorohydrin resin involving reacting the epichlorohydrin with a polyamine in a mixture first at a temperature of 25-40 DEG C and then heating the mixture at 25-85 DEG C.
Bibliography:Application Number: FI19910005481