Method of straightening keratin fibres with heating means and a denaturant agent

Process for uncurling the keratinic fibers comprises: (1) applying an uncurling composition (I) containing a denaturing agent (II) having a molecular mass of greater than 18.1 g/mol and present in a concentration of 1-8M; and heating the keratinic fiber to 110-250[deg]C.