Process for the production of friction materials

A process for producing a friction material under low-temperature conditions using, as a reinforcement, one or more fibers selected from a metal fiber, an organic fiber and an inorganic fiber and, as a binder, a compounded pitch that consists of a mesophase pitch and sulfur and/or an aromatic nitro...

Full description

Saved in:
Bibliographic Details
Main Authors TOKUMURA, HIROSHI, KAMIOKA, NOBUO, SAKAMOTO, HITOSHI, KOJIMA, TAKASHI
Format Patent
LanguageEnglish
French
German
Published 05.05.1993
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A process for producing a friction material under low-temperature conditions using, as a reinforcement, one or more fibers selected from a metal fiber, an organic fiber and an inorganic fiber and, as a binder, a compounded pitch that consists of a mesophase pitch and sulfur and/or an aromatic nitro compound. The content of an optically anisotropic phase in the mesophase pitch is at least 80% and the softening point of the mesophase pitch is not higher than 270 DEG C. The friction material produced exhibits consistent friction characteristics over a broad temperature range.
Bibliography:Application Number: EP19920309899