A dispersion strengthened aluminum alloy is produced by continuously casting an aluminum alloy containing 4 - 15% Si and other optional constituents in the form of a slab at a growth rate in excess of 25 cm/min. to solidify silicon in the form of elongated rods in a size range of 0.05 - 0.5 microns...