Preparation method of super-retarded concrete
The invention provides a preparation method of super-retarded concrete. Adding the coarse aggregate and the fine aggregate into a stirrer, and stirring for 30 seconds; adding Portland cement and fly ash, and stirring for 30s; adding water, a polycarboxylic acid water reducing agent and a glue reduci...
Saved in:
Main Authors | , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
05.04.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | The invention provides a preparation method of super-retarded concrete. Adding the coarse aggregate and the fine aggregate into a stirrer, and stirring for 30 seconds; adding Portland cement and fly ash, and stirring for 30s; adding water, a polycarboxylic acid water reducing agent and a glue reducing agent, stirring for 60 seconds, and standing for 1 hour; and adding the reinforcing-retarding particles, and stirring for 60 seconds to obtain the super-retarding concrete. The reinforcing-retarding particles are adopted, so that the retarding effect on the concrete is achieved, and meanwhile, the effect of enhancing the mechanical property of the concrete is also achieved. The reinforcing-retarding particles are formed by grafting pyrophyllite with a super absorbent material, the super absorbent material has a large number of hydroxyl groups and carboxyl groups, and the carboxyl groups react with free Ca < 2 + > in an alkaline environment of hydration of Portland cement to generate an unstable complex, so that |
---|---|
AbstractList | The invention provides a preparation method of super-retarded concrete. Adding the coarse aggregate and the fine aggregate into a stirrer, and stirring for 30 seconds; adding Portland cement and fly ash, and stirring for 30s; adding water, a polycarboxylic acid water reducing agent and a glue reducing agent, stirring for 60 seconds, and standing for 1 hour; and adding the reinforcing-retarding particles, and stirring for 60 seconds to obtain the super-retarding concrete. The reinforcing-retarding particles are adopted, so that the retarding effect on the concrete is achieved, and meanwhile, the effect of enhancing the mechanical property of the concrete is also achieved. The reinforcing-retarding particles are formed by grafting pyrophyllite with a super absorbent material, the super absorbent material has a large number of hydroxyl groups and carboxyl groups, and the carboxyl groups react with free Ca < 2 + > in an alkaline environment of hydration of Portland cement to generate an unstable complex, so that |
Author | LYU CHAOYANG YUAN TING MENG HUICHENG CHEN WENXUAN SHEN LEI LI XIAOTING TANG YUNDAN YOU BAI |
Author_xml | – fullname: LYU CHAOYANG – fullname: CHEN WENXUAN – fullname: LI XIAOTING – fullname: YOU BAI – fullname: YUAN TING – fullname: SHEN LEI – fullname: MENG HUICHENG – fullname: TANG YUNDAN |
BookMark | eNrjYmDJy89L5WTQDShKLUgsSizJzM9TyE0tychPUchPUyguLUgt0i1KLUksSklNUUjOz0sGclJ5GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hobmFoaWlgamjMTFqANc7LDk |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | 一种超缓凝混凝土的制备方法 |
ExternalDocumentID | CN117819905A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_CN117819905A3 |
IEDL.DBID | EVB |
IngestDate | Fri Aug 02 08:59:55 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | Chinese English |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_CN117819905A3 |
Notes | Application Number: CN202311767695 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240405&DB=EPODOC&CC=CN&NR=117819905A |
ParticipantIDs | epo_espacenet_CN117819905A |
PublicationCentury | 2000 |
PublicationDate | 20240405 |
PublicationDateYYYYMMDD | 2024-04-05 |
PublicationDate_xml | – month: 04 year: 2024 text: 20240405 day: 05 |
PublicationDecade | 2020 |
PublicationYear | 2024 |
RelatedCompanies | SUZHOU SHANGJIAN HANGXIN CONCRETE CO., LTD |
RelatedCompanies_xml | – name: SUZHOU SHANGJIAN HANGXIN CONCRETE CO., LTD |
Score | 3.6688657 |
Snippet | The invention provides a preparation method of super-retarded concrete. Adding the coarse aggregate and the fine aggregate into a stirrer, and stirring for 30... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
Title | Preparation method of super-retarded concrete |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240405&DB=EPODOC&locale=&CC=CN&NR=117819905A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV3dS8MwED_mFPVNp6LzgwrSt2C7fj8UcWnLENYVmbK3sbYJ6sNa2g7Bv95L1jlflLyEBC4fcPndJZffAdwxd2FlGuMkH2QpMVnGyEIzUuJ53NYzGwsXVwPj2B69mE8za9aBj81fGMkT-inJEVGjMtT3Rp7X5fYSK5CxlfV9-o5NxUM09QO19Y4RntAAUYOhHyaTYEJVSn0aq_Gzr-sOYp-nWY87sCvMaMGzH74Oxa-U8jekREewl6C0ZXMMna-3HhzQTea1HuyP2wdvrLa6V58ASSq2Juoulso68bNScKVelawiImqwylmuoHuLdmDDTuE2Cqd0RHDc-c8i5zTeTtE4gy46_-wcFMG_xTXb5bqRmqbJvYHDXcsZGCnPBJRcQP9vOf3_Oi_hUGyYjEKxrqDbVCt2jQDbpDdyZ74Bqph_xA |
link.rule.ids | 230,309,786,891,25594,76903 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV3dS8MwED_mFOebTkXnVwXpW7Bdvx-KuHRl6tYNmbK3sWQJ6sNW2g7Bv95rtjlflLyEBC4fcPndL7m7ANwIf-JwQ0gybXJGbMEFmRgWI0EgXZO7WGR5NdBL3M6L_ThyRhX4WMfCqDyhnyo5ImoUR30v1Hmdbi6xIuVbmd-yd2ya38XDMNJX7BjhCQ0QPWqF7UE_6lOd0pAmevIcmqaH2BcYzv0WbHtICRVVem2VUSnpb0iJ92FngNJmxQFUvt7qUKPrn9fqsNtbPXhjdaV7-SGQQSaWibrnM2358bM2l1q-SEVGSq_BbCqmGtJbtAMLcQTXcXtIOwTHHf8sckyTzRStY6gi-RcnoJX5t6Th-tK0mG3bMmh60ne8psUkL6HkFBp_y2n813kFtc6w1x13H5KnM9grN095pDjnUC2yhbhAsC3Ypdqlb8jygq4 |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=Preparation+method+of+super-retarded+concrete&rft.inventor=LYU+CHAOYANG&rft.inventor=CHEN+WENXUAN&rft.inventor=LI+XIAOTING&rft.inventor=YOU+BAI&rft.inventor=YUAN+TING&rft.inventor=SHEN+LEI&rft.inventor=MENG+HUICHENG&rft.inventor=TANG+YUNDAN&rft.date=2024-04-05&rft.externalDBID=A&rft.externalDocID=CN117819905A |