Method for co-producing needle coke and spinnable asphalt
The invention provides a method for co-producing needle coke and spinnable asphalt, which comprises the following steps: (1) carrying out solid removal treatment on an aromatic-rich raw material to obtain solid-removed oil slurry; (2) hydrofining the solid-removed oil slurry to obtain hydrogenated o...
Saved in:
Main Authors | , , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
05.03.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention provides a method for co-producing needle coke and spinnable asphalt, which comprises the following steps: (1) carrying out solid removal treatment on an aromatic-rich raw material to obtain solid-removed oil slurry; (2) hydrofining the solid-removed oil slurry to obtain hydrogenated oil; (3) carrying out reduced pressure distillation on the hydrogenated oil, and dividing the hydrogenated oil into light distillate oil, middle distillate oil and heavy distillate oil; (4) carrying out delayed coking on the middle distillate oil to obtain needle coke; a coke drawing medium in the delayed coking is a mixture of the light distillate oil and coker diesel oil; and (5) carrying out polymerization reaction and oxidation reaction on the heavy distillate oil to obtain the spinnable asphalt. According to the method, aromatic-rich resources such as catalytic slurry oil are fully and completely utilized, needle coke products and spinnable asphalt products with high additional values are obtained, byproducts a |
---|---|
Bibliography: | Application Number: CN202311656267 |