Coarse grain flotation method for carbonic acid type phosphorite
The invention discloses a carbonate type phosphorite coarse grain flotation method, and relates to the technical field of phosphorite flotation. The ore with the particle size being-500 mm is crushed to be-1 mm; adding a regulator for size mixing, then adding a coarse-fraction collecting agent for s...
Saved in:
Main Authors | , , , , , , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
20.10.2023
|
Subjects | |
Online Access | Get full text |
Cover
Summary: | The invention discloses a carbonate type phosphorite coarse grain flotation method, and relates to the technical field of phosphorite flotation. The ore with the particle size being-500 mm is crushed to be-1 mm; adding a regulator for size mixing, then adding a coarse-fraction collecting agent for size mixing, then carrying out air flotation for 3-5 minutes to obtain roughed phosphate concentrate and tailings, and directly discarding the tailings; concentrating the rough phosphate concentrate, grinding the rough phosphate concentrate to-0.425 mm, carrying out re-separation operation, adding a regulator and a coarse-grained collecting agent, carrying out flotation for 1-3 minutes, and carrying out scavenging operation and tailing discarding on the concentrated phosphate concentrate, tailings and the tailings or directly discarding the tailings; and carrying out 0.23 mm grading treatment on the concentrated phosphate concentrate, returning the concentrate with the particle size larger than 0.23 mm to be subject |
---|---|
Bibliography: | Application Number: CN202310883074 |