Steel production method for improving rack machining performance
The invention discloses a steel production method for improving the machining performance of a rack, and relates to the technical field of steel production, cogging heating is conducted, specifically, the heating temperature ranges from 950 DEG C to 1270 DEG C, and the total heating time is longer t...