Steel production method for improving rack machining performance
The invention discloses a steel production method for improving the machining performance of a rack, and relates to the technical field of steel production, cogging heating is conducted, specifically, the heating temperature ranges from 950 DEG C to 1270 DEG C, and the total heating time is longer t...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
04.08.2023
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a steel production method for improving the machining performance of a rack, and relates to the technical field of steel production, cogging heating is conducted, specifically, the heating temperature ranges from 950 DEG C to 1270 DEG C, and the total heating time is longer than or equal to 240 min; high-pressure water is adopted for descaling, and the pressure is larger than or equal to 13 MPa; second-fire rolling heating, wherein the heating temperature is 980-1240 DEG C, and the total heating time is larger than or equal to 180 min; second-fire rolling dephosphorization is conducted, specifically, high-pressure water is adopted for descaling, and the pressure is larger than or equal to 13 MPa; finish rolling: the finish rolling temperature is 800-900 DEG C; ultrasonic flaw detection and magnetic flux leakage detection are carried out, wherein the ultrasonic flaw detection precision meets the A-level requirement of GB/T 4162. The machining performance of the rack is improved by optim |
---|---|
Bibliography: | Application Number: CN202310569363 |