Method for preparing geopolymer finished product by utilizing Sichuan-Western typical rare earth tailings
The invention relates to a method for preparing a geopolymer finished product by utilizing Sichuan-Western typical rare earth tailings. A formula for solving the problem of low strength of a geopolymer finished product prepared from rare earth tailings comprises the following components in parts by...
Saved in:
Main Authors | , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
17.04.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention relates to a method for preparing a geopolymer finished product by utilizing Sichuan-Western typical rare earth tailings. A formula for solving the problem of low strength of a geopolymer finished product prepared from rare earth tailings comprises the following components in parts by mass: 25-100 parts of Sichuan western typical rare earth tailings, 80-120 parts of metakaolin, 5-50parts of silica fume, 28-40 parts of NaOH, 60-138 parts of water and 0.1-5 parts of a heavy metal source (lead salt Pb (NO3) 2). The preparation method comprises the following steps: roasting kaolin at 800 DEG C for 6 hours to obtain metakaolin with the same mass; NaOH is dissolved in water, silica fume is added and stirred until the silica fume is dissolved, Pb (NO3) 2 is added at the same time,metakaolin and rare earth tailings are added and stirred together when the temperature is reduced to 30-80 DEG C, an obtained evenly mixed slurry is poured into a mold to be formed; the 7d compressivestrength of the prepared g |
---|---|
Bibliography: | Application Number: CN201911255254 |