Processing method for glass mold

The invention discloses a processing method for a glass mold. The processing method comprises the following steps that 1, the drawing design is conducted on the glass mold, and the preparation of therequired raw materials is achieved; 2, heating melting at the temperature of 1227-1538 DEG C is condu...

Full description

Saved in:
Bibliographic Details
Main Authors TIAN MINXUAN, XU DEZHANG, NI MINGFA, LI HUAIZHENG
Format Patent
LanguageChinese
English
Published 31.05.2019
Subjects
Online AccessGet full text

Cover

Loading…
Abstract The invention discloses a processing method for a glass mold. The processing method comprises the following steps that 1, the drawing design is conducted on the glass mold, and the preparation of therequired raw materials is achieved; 2, heating melting at the temperature of 1227-1538 DEG C is conducted on the prepared raw materials, the raw materials are cooled to a metal billet, and the manufacturing environment temperature and humidity are set; and 3, mechanical-forging and forging are conducted on the metal billet in the step 2, the metal billet produces plastic deformation, then the temperature is heated to 500-550 DEG C, the annealing treatment with the insulation time of 2-8 h is conducted, and a mold billet is obtained. By means of the processing method for the glass mold, the shape of the glass mold is forged through the mechanical-forging, an inner cavity of the glass mold is processed through the shape processing and mold cavity processing, and integrated molding is achieved accordingly, the pre-pr
AbstractList The invention discloses a processing method for a glass mold. The processing method comprises the following steps that 1, the drawing design is conducted on the glass mold, and the preparation of therequired raw materials is achieved; 2, heating melting at the temperature of 1227-1538 DEG C is conducted on the prepared raw materials, the raw materials are cooled to a metal billet, and the manufacturing environment temperature and humidity are set; and 3, mechanical-forging and forging are conducted on the metal billet in the step 2, the metal billet produces plastic deformation, then the temperature is heated to 500-550 DEG C, the annealing treatment with the insulation time of 2-8 h is conducted, and a mold billet is obtained. By means of the processing method for the glass mold, the shape of the glass mold is forged through the mechanical-forging, an inner cavity of the glass mold is processed through the shape processing and mold cavity processing, and integrated molding is achieved accordingly, the pre-pr
Author NI MINGFA
XU DEZHANG
TIAN MINXUAN
LI HUAIZHENG
Author_xml – fullname: TIAN MINXUAN
– fullname: XU DEZHANG
– fullname: NI MINGFA
– fullname: LI HUAIZHENG
BookMark eNrjYmDJy89L5WRQCCjKT04tLs7MS1fITS3JyE9RSMsvUkjPSSwuVsjNz0nhYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBpYWRkbGBiaOxsSoAQAr2ibq
ContentType Patent
DBID EVB
DatabaseName esp@cenet
DatabaseTitleList
Database_xml – sequence: 1
  dbid: EVB
  name: esp@cenet
  url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP
  sourceTypes: Open Access Repository
DeliveryMethod fulltext_linktorsrc
Discipline Medicine
Chemistry
Sciences
DocumentTitleAlternate 一种玻璃模具的加工方法
ExternalDocumentID CN109822304A
GroupedDBID EVB
ID FETCH-epo_espacenet_CN109822304A3
IEDL.DBID EVB
IngestDate Fri Jul 19 15:59:41 EDT 2024
IsOpenAccess true
IsPeerReviewed false
IsScholarly false
Language Chinese
English
LinkModel DirectLink
MergedId FETCHMERGED-epo_espacenet_CN109822304A3
Notes Application Number: CN201910293375
OpenAccessLink https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20190531&DB=EPODOC&CC=CN&NR=109822304A
ParticipantIDs epo_espacenet_CN109822304A
PublicationCentury 2000
PublicationDate 20190531
PublicationDateYYYYMMDD 2019-05-31
PublicationDate_xml – month: 05
  year: 2019
  text: 20190531
  day: 31
PublicationDecade 2010
PublicationYear 2019
RelatedCompanies HEXIAN JINGJING GLASS PRODUCTS CO., LTD
RelatedCompanies_xml – name: HEXIAN JINGJING GLASS PRODUCTS CO., LTD
Score 3.3319762
Snippet The invention discloses a processing method for a glass mold. The processing method comprises the following steps that 1, the drawing design is conducted on...
SourceID epo
SourceType Open Access Repository
SubjectTerms COMBINED OPERATIONS
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
OTHER WORKING OF METAL
PERFORMING OPERATIONS
TRANSPORTING
UNIVERSAL MACHINE TOOLS
Title Processing method for glass mold
URI https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20190531&DB=EPODOC&locale=&CC=CN&NR=109822304A
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwY2BQMUlLMUgGJhxdI-PUJF3Q1Bkwz1mAdqMlpiRZpJikGVqANgr7-pl5hJp4RZhGMDFkwfbCgM8JLQcfjgjMUcnA_F4CLq8LEINYLuC1lcX6SZlAoXx7txBbFzVo7xhYuwHTlJqLk61rgL-Lv7Oas7Ots5-aXxCwrQs6qA7Yd3dkZmAFNaNB5-y7hjmBdqUUIFcpboIMbAFA0_JKhBiYqjKEGTidYTevCTNw-EInvIFMaN4rFmFQgK7pB9Y1CpB7nxWADU4FcPNXITc_J0WUQdHNNcTZQxdoVTzcX_HOfghXGYsxsAD7-6kSDArmKZbJluaGaSnJSUYmyWYpFmnARl2yQVKKoXmqJbD1IMkghdscKXyS0gxcoDCCTH7LMLCUFJWmygLr1JIkOXBgAABGuHoO
link.rule.ids 230,309,786,891,25594,76904
linkProvider European Patent Office
linkToHtml http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwY2BQMUlLMUgGJhxdI-PUJF3Q1Bkwz1mAdqMlpiRZpJikGVqANgr7-pl5hJp4RZhGMDFkwfbCgM8JLQcfjgjMUcnA_F4CLq8LEINYLuC1lcX6SZlAoXx7txBbFzVo7xhYuwHTlJqLk61rgL-Lv7Oas7Ots5-aXxCwrQs6qA7Yd3dkZmA1B3YJQefsu4Y5gXalFCBXKW6CDGwBQNPySoQYmKoyhBk4nWE3rwkzcPhCJ7yBTGjeKxZhUICu6QfWNQqQe58VgA1OBXDzVyE3PydFlEHRzTXE2UMXaFU83F_xzn4IVxmLMbAA-_upEgwK5imWyZbmhmkpyUlGJslmKRZpwEZdskFSiqF5qiWw9SDJIIXbHCl8kvIMnB4hvj7xPp5-3tIMXKDwgkyEyzCwlBSVpsoC69eSJDlwwAAAIXp8-Q
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=Processing+method+for+glass+mold&rft.inventor=TIAN+MINXUAN&rft.inventor=XU+DEZHANG&rft.inventor=NI+MINGFA&rft.inventor=LI+HUAIZHENG&rft.date=2019-05-31&rft.externalDBID=A&rft.externalDocID=CN109822304A