Preparation method of lightweight composite board
The invention discloses a preparation method of a lightweight composite board. The preparation method comprises following steps: raw material mixing, die material distribution, normal temperature pre-compressing, hot pressing solidification, cooling, die-opening, aging, trimming and cutting, thickne...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
30.11.2018
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | The invention discloses a preparation method of a lightweight composite board. The preparation method comprises following steps: raw material mixing, die material distribution, normal temperature pre-compressing, hot pressing solidification, cooling, die-opening, aging, trimming and cutting, thickness fixing and sanding, standard size cutting, polishing, and board surface composite treatment. Theobtained lightweight composite board is nontoxic, possesses no radioactivity, reaches flame resistance A2 grade, possesses oil resistance, stain resistance, mildew resistance, antibacterial performance, wear resistance, impact resistance, is abundant in color, uniform in color, high and uniform in texture density, extremely high in natural texture performance, strength, and hardness, and can be used for UV coating or other surface composite processing based on different application requirements; maintenance is convenient; seamless splicing can be realized; and the moulding can be changed.
本发明公开了种轻质复合板材的制备方法,步骤包括:原料混合、 |
---|---|
AbstractList | The invention discloses a preparation method of a lightweight composite board. The preparation method comprises following steps: raw material mixing, die material distribution, normal temperature pre-compressing, hot pressing solidification, cooling, die-opening, aging, trimming and cutting, thickness fixing and sanding, standard size cutting, polishing, and board surface composite treatment. Theobtained lightweight composite board is nontoxic, possesses no radioactivity, reaches flame resistance A2 grade, possesses oil resistance, stain resistance, mildew resistance, antibacterial performance, wear resistance, impact resistance, is abundant in color, uniform in color, high and uniform in texture density, extremely high in natural texture performance, strength, and hardness, and can be used for UV coating or other surface composite processing based on different application requirements; maintenance is convenient; seamless splicing can be realized; and the moulding can be changed.
本发明公开了种轻质复合板材的制备方法,步骤包括:原料混合、 |
Author | LI XUEYE SHENG XIAODONG |
Author_xml | – fullname: SHENG XIAODONG – fullname: LI XUEYE |
BookMark | eNrjYmDJy89L5WQwDChKLUgsSizJzM9TyE0tychPUchPU8jJTM8oKU8FkQrJ-bkF-cWZJakKSfmJRSk8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSTe2c_QwMLS0NDcwsDRmBg1ALsTLdI |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | 种轻质复合板材的制备方法 |
ExternalDocumentID | CN108911780A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_CN108911780A3 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 15:47:47 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | Chinese English |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_CN108911780A3 |
Notes | Application Number: CN201710755972 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20181130&DB=EPODOC&CC=CN&NR=108911780A |
ParticipantIDs | epo_espacenet_CN108911780A |
PublicationCentury | 2000 |
PublicationDate | 20181130 |
PublicationDateYYYYMMDD | 2018-11-30 |
PublicationDate_xml | – month: 11 year: 2018 text: 20181130 day: 30 |
PublicationDecade | 2010 |
PublicationYear | 2018 |
RelatedCompanies | BEIJING HOMO TECHNOLOGY DEVELOPMENT CO., LTD |
RelatedCompanies_xml | – name: BEIJING HOMO TECHNOLOGY DEVELOPMENT CO., LTD |
Score | 3.3001945 |
Snippet | The invention discloses a preparation method of a lightweight composite board. The preparation method comprises following steps: raw material mixing, die... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY PERFORMING OPERATIONS REFRACTORIES SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG, OR MIXTURESCONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER SLAG TRANSPORTING TREATMENT OF NATURAL STONE WORKING CEMENT, CLAY, OR STONE |
Title | Preparation method of lightweight composite board |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20181130&DB=EPODOC&locale=&CC=CN&NR=108911780A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwY2BQSUw2tEw0Bk2yphlZ6pqYJSbpAmvFFN1EYGVrkpZsnphqCNqN7Otn5hFq4hVhGsHEkAXbCwM-J7QcfDgiMEclA_N7Cbi8LkAMYrmA11YW6ydlAoXy7d1CbF3UoL1jYHUFLJPVXJxsXQP8Xfyd1ZydbZ391PyCgG1dC2C2NrcwcGRmYAU1o0Hn7LuGOYF2pRQgVyluggxsAUDT8kqEGJiqMoQZOJ1hN68JM3D4Qie8gUxo3isWYTAMKEqFHNSdn6cAufhZIT9NIQfUuy4HD3AqgNaHgxZhpSok5QNjXpRB0c01xNlDF2h3PNyj8c5-CGcaizGw5OXnpUowKJibJpkZG1gkW6QZA1sLRgaWqcZpJsB2XLKFSYqpSUqqJIMUbnOk8ElKM3CBAg1ylKEMA0tJUWmqLLCSLUmSA4cOAFwcgIQ |
link.rule.ids | 230,309,786,891,25594,76904 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwY2BQSUw2tEw0Bk2yphlZ6pqYJSbpAmvFFN1EYGVrkpZsnphqCNqN7Otn5hFq4hVhGsHEkAXbCwM-J7QcfDgiMEclA_N7Cbi8LkAMYrmA11YW6ydlAoXy7d1CbF3UoL1jYHUFLJPVXJxsXQP8Xfyd1ZydbZ391PyCgG1dC2C2NrcwcGRmYDUHdglB5-y7hjmBdqUUIFcpboIMbAFA0_JKhBiYqjKEGTidYTevCTNw-EInvIFMaN4rFmEwDChKhRzUnZ-nALn4WSE_TSEH1LsuBw9wKoDWh4MWYaUqJOUDY16UQdHNNcTZQxdodzzco_HOfghnGosxsOTl56VKMCiYmyaZGRtYJFukGQNbC0YGlqnGaSbAdlyyhUmKqUlKqiSDFG5zpPBJyjNweoT4-sT7ePp5SzNwgQIQcqyhDANLSVFpqiywwi1JkgOHFACEs4Nv |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=Preparation+method+of+lightweight+composite+board&rft.inventor=SHENG+XIAODONG&rft.inventor=LI+XUEYE&rft.date=2018-11-30&rft.externalDBID=A&rft.externalDocID=CN108911780A |