Raw material formula of luminous waterstone
The invention belongs to the field of building materials, and aims to provide a raw material formula of a luminous waterstone. The raw material formula comprises the following components in parts by weight: 100 parts of metakaolin, 10 to 20 parts of an alkali-activator, 80 to 120 parts of an inorgan...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
12.10.2016
|
Subjects | |
Online Access | Get full text |
Cover
Summary: | The invention belongs to the field of building materials, and aims to provide a raw material formula of a luminous waterstone. The raw material formula comprises the following components in parts by weight: 100 parts of metakaolin, 10 to 20 parts of an alkali-activator, 80 to 120 parts of an inorganic aggregate, 5 to 20 parts of luminous stones and 30 to 50 parts of water, wherein the alkali-activator is NaOH or Na2O nSiO2, and n is equal to 1.0 to 2.0. With a geopolymer serving as a gel material, the raw material formula is low in energy consumption and low in environmental pollution; the prepared luminous waterstone is high in breaking strength and low in water absorption rate, and can be widely applied.
本发明属于建筑材料领域,旨在提供种夜光水磨石的原料配方。包括下述按重量比计算的各组分:偏高岭土100份、碱激发剂10~20份、无机骨料80~120份、夜光石5~20份、水30~50份,所述碱激发剂为NaOH或Na2O·nSiO2,n=1.0~2.0。本发明以地聚合物为胶凝材料,能耗少、环境污染小;制备所得的水磨石抗折强度高,吸水率低,应用领域广泛。 |
---|---|
Bibliography: | Application Number: CN20161345138 |