Preparation method of triangular prism-shaped rare earth-activated yttrium oxide nano-luminescence material
The invention discloses a preparation method of a triangular prism-shaped rare earth-activated yttrium oxide nano-luminescence material, and belongs to preparation of luminescent nanomaterials.The preparation method comprises the following steps that yttrium nitrate (Y(NO3)3) serving as a yttrium so...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
20.07.2016
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | The invention discloses a preparation method of a triangular prism-shaped rare earth-activated yttrium oxide nano-luminescence material, and belongs to preparation of luminescent nanomaterials.The preparation method comprises the following steps that yttrium nitrate (Y(NO3)3) serving as a yttrium source and rare earth (such as europium, erbium and samarium) nitrate are added into deionized water and triethanolamine (TEOA), full stirring is performed, therefore, the molar concentration of Y<3+> is 0.01 M-1 M, and the molar concentration of rare earth ions accounts for 1%-8% of that of the yttrium ions.Heat preservation is performed for 24-80 h at the temperature of 130 DEG C-200 DEG C through a solvothermal method, and the volume ratio of solvent (TEOA) to the deionized water is (0.1-3):1.
种三角柱状稀土激活氧化钇纳米发光材料的制备方法,属于发光纳米材料的制备。包含以下步骤:将硝酸钇(Y(NO))作为钇源与稀土硝酸盐(铕、铒、钐..)加入去离子水与三乙醇胺(TEOA)中,并充分搅拌,使得Y的摩尔浓度为0.01M?1M,稀土离子摩尔浓度为钇离子的1%?8%。利用溶剂热法经过130?200℃保温24?80h处理。溶剂TEOA与去离子水的体积比为(0.1?3):1。 |
---|---|
AbstractList | The invention discloses a preparation method of a triangular prism-shaped rare earth-activated yttrium oxide nano-luminescence material, and belongs to preparation of luminescent nanomaterials.The preparation method comprises the following steps that yttrium nitrate (Y(NO3)3) serving as a yttrium source and rare earth (such as europium, erbium and samarium) nitrate are added into deionized water and triethanolamine (TEOA), full stirring is performed, therefore, the molar concentration of Y<3+> is 0.01 M-1 M, and the molar concentration of rare earth ions accounts for 1%-8% of that of the yttrium ions.Heat preservation is performed for 24-80 h at the temperature of 130 DEG C-200 DEG C through a solvothermal method, and the volume ratio of solvent (TEOA) to the deionized water is (0.1-3):1.
种三角柱状稀土激活氧化钇纳米发光材料的制备方法,属于发光纳米材料的制备。包含以下步骤:将硝酸钇(Y(NO))作为钇源与稀土硝酸盐(铕、铒、钐..)加入去离子水与三乙醇胺(TEOA)中,并充分搅拌,使得Y的摩尔浓度为0.01M?1M,稀土离子摩尔浓度为钇离子的1%?8%。利用溶剂热法经过130?200℃保温24?80h处理。溶剂TEOA与去离子水的体积比为(0.1?3):1。 |
Author | ZHAO BINGXIN DONG LIRAN WANG JINSHU JIA XINJIAN |
Author_xml | – fullname: ZHAO BINGXIN – fullname: WANG JINSHU – fullname: DONG LIRAN – fullname: JIA XINJIAN |
BookMark | eNqNzD0KwkAQhuEUWvh3h_EAC0aRaClBsRILexmSiVncnV1mJ6K3dwsPYPXBy8M3LUYcmCbF8yoUUVBtYPCkfWghdKBikR-DQ4EoNnmTeozUgqAQEIr2Bhu1L9QcP5r54CG8bUvAyMG4wVum1BA3BD6r_OfmxbhDl2jx21mxPB1v9dlQDHdKETMnvdeXcrWtqt2-XB82_5gvw2BEOw |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
DocumentTitleAlternate | 种三角柱状稀土激活氧化钇纳米发光材料的制备方法 |
ExternalDocumentID | CN105778912A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_CN105778912A3 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 17:09:55 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | Chinese English |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_CN105778912A3 |
Notes | Application Number: CN20161352926 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20160720&DB=EPODOC&CC=CN&NR=105778912A |
ParticipantIDs | epo_espacenet_CN105778912A |
PublicationCentury | 2000 |
PublicationDate | 20160720 |
PublicationDateYYYYMMDD | 2016-07-20 |
PublicationDate_xml | – month: 07 year: 2016 text: 20160720 day: 20 |
PublicationDecade | 2010 |
PublicationYear | 2016 |
RelatedCompanies | BEIJING UNIVERSITY OF TECHNOLOGY |
RelatedCompanies_xml | – name: BEIJING UNIVERSITY OF TECHNOLOGY |
Score | 3.162066 |
Snippet | The invention discloses a preparation method of a triangular prism-shaped rare earth-activated yttrium oxide nano-luminescence material, and belongs to... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | ADHESIVES CHEMISTRY DYES MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS PAINTS POLISHES |
Title | Preparation method of triangular prism-shaped rare earth-activated yttrium oxide nano-luminescence material |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20160720&DB=EPODOC&locale=&CC=CN&NR=105778912A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1bT8IwFD5BNOqbokbxkpqYvTWysevDYqSDEBMGMWh4I9vaBTVuZAxvv97TAuKLvjVt08tJT2_nnO8DuHL0VHhubFIe84iaToNTz3QSmrqxSK3I1QWXFt1eaHcfzLuRNarA8yoWRuGEvitwRNSoBPW9VPv1dP2JFSjfytl1_IRZ-U1n6Afa8nUs0dKMhha0_PagH_SZxpjPQi289yWdreN6unG7AZt4jXak-1f7sSWjUqa_j5TOHmwNsLWs3IfK16QGO2zFvFaD7d7S4I3Jpe7NDuBlUIgFUHeekQXxM8lTImk3MsknXxAFaUhnk2gqOMFHsCC4jMsJlbELb9gZJ58lVp-_kvwD506yKMspbk7S8z2RvRC8vqoVeQiXnfaQdSmOevwjojEL1xNsHkE1yzNxDKTJDctNZUQg90w9ibzUs52Ix6blRbadJCdQ_7ud-n-Fp7ArxS1_OY3GGVTLYi7O8Xgu4wsl1292AJhN |
link.rule.ids | 230,309,783,888,25578,76884 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1bT8IwFD5BNOKbokbxVhOzt0Y2dn1YjGwQVBjEoOGNbGsX1NgRGN5-vacDxBd9a9rmtD05p_fzfQAXlppwx450yiIWUt2qMuroVkwTO-KJEdoqZ_JFtxOYrQf9dmAMCvC8jIXJcULfc3BE9KgY_T3L5-vx6hLLz_9WTi-jJ8xKr5p911cWp2OJlqZVFb_uNnpdv-spnud6gRLcu5LO1rIdVbteg3XcYtsSZ7_xWJdRKePfS0pzGzZ6KE1kO1D4GpWh5C2Z18qw2Vk8eGNy4XvTXXjpTfgcqDsVZE78TNKESNoNIfnkJySHNKTTUTjmjOAhmBM042xEZezCGzbGyGeG1WevJP3AsRMRipTi5CR_vseyFYLb19wi9-C82eh7LYq9Hv6oaOgFqwHW9qEoUsEPgNSYZtiJjAhkjq7GoZM4phWySDec0DTj-BAqf8up_Fd4BqVWv9Metm-CuyPYkqqXN55a9RiK2WTGT3CpzqLTXMffw1ObPQ |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=Preparation+method+of+triangular+prism-shaped+rare+earth-activated+yttrium+oxide+nano-luminescence+material&rft.inventor=ZHAO+BINGXIN&rft.inventor=WANG+JINSHU&rft.inventor=DONG+LIRAN&rft.inventor=JIA+XINJIAN&rft.date=2016-07-20&rft.externalDBID=A&rft.externalDocID=CN105778912A |