High-density precipitated phase containing low-alloy high-strength steel plate strip and rolling process thereof

The invention discloses a high-density precipitated phase containing low-alloy high-strength steel plate strip and a rolling process thereof. The high-density precipitated phase containing low-alloy high-strength steel plate strip comprises the following chemical compositions in percentage by weight...

Full description

Saved in:
Bibliographic Details
Main Authors QIAO TUANJIE, WANG JIAN, WANG ZHIWEN, ZHANG HUI, WANG HAIMING, KANG LIMING, QIAO LINSUO, WANG XIAOPING, ZHENG YONGCHUN, GAO ZHIGUO, CHENG DEFU
Format Patent
LanguageChinese
English
Published 05.03.2014
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention discloses a high-density precipitated phase containing low-alloy high-strength steel plate strip and a rolling process thereof. The high-density precipitated phase containing low-alloy high-strength steel plate strip comprises the following chemical compositions in percentage by weight: 0.05-0.12% of C, less than or equal to 0.50% of Si, 1.20-2.00% of Mn, less than or equal to 0.020% of P, less than or equal to 0.010% of S, greater than or equal to 0.030% of Alt, 0.060-0.080% of Nb, 0.051-0.070% of V, 0.11-0.15% of Ti, 0.24-0.44% of Mo, greater than 0.23% of Nb+V+Ti, and the balance of Fe and unavoidable impurities. A hot rolling process is implemented as follows: the heating temperature of a steel ingot is 1190-1260 DEG C, the heat preservation time is 1-5 hours, the rough rolling time is 1150-1200 DEG C, the finish rolling temperature is 950-990 DEG C, the final rolling temperature is 850-900 DEG C, the total rolling reduction of two-section rolling is greater than or equal to 80%, and the tem