Waterborne ultra-thin steel structure fire retardant coating and preparation method thereof
Provided is a waterborne ultra-thin steel structure fire retardant coating and a preparation method thereof. The raw material ratio of the coating includes 15-50% by weight of polymer latex, 15-30% by weight of ammonium polyphosphate, 5-15% by weight of pentaerythritol, 3-10% by weight of cyanurtria...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
26.12.2012
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | Provided is a waterborne ultra-thin steel structure fire retardant coating and a preparation method thereof. The raw material ratio of the coating includes 15-50% by weight of polymer latex, 15-30% by weight of ammonium polyphosphate, 5-15% by weight of pentaerythritol, 3-10% by weight of cyanurtriamide, 5-12% by weight of titanium dioxide, 2-13% inorganic filler, 0-5% by weight of expansiveness graphite, 1-10% by weight of plasticizer, 0.4-1.5% by weight of wetting dispersant, 0.2-0.5% by weight of defoamer, 1-6% by weight of coalescing agents and 5-15% by weight of water, and total raw material ratio is 100%. A high-speed dispersion method or a grinding dispersion method is adopted in preparation of the coating. A coating layer of the fire retardant coating can form a carbonization layer which is good in foaming effect, small and uniform in air holes and high in expansion times when in heating. The final fire retardant performance of the coating is far higher than technical requirements of a national standa |
---|---|
AbstractList | Provided is a waterborne ultra-thin steel structure fire retardant coating and a preparation method thereof. The raw material ratio of the coating includes 15-50% by weight of polymer latex, 15-30% by weight of ammonium polyphosphate, 5-15% by weight of pentaerythritol, 3-10% by weight of cyanurtriamide, 5-12% by weight of titanium dioxide, 2-13% inorganic filler, 0-5% by weight of expansiveness graphite, 1-10% by weight of plasticizer, 0.4-1.5% by weight of wetting dispersant, 0.2-0.5% by weight of defoamer, 1-6% by weight of coalescing agents and 5-15% by weight of water, and total raw material ratio is 100%. A high-speed dispersion method or a grinding dispersion method is adopted in preparation of the coating. A coating layer of the fire retardant coating can form a carbonization layer which is good in foaming effect, small and uniform in air holes and high in expansion times when in heating. The final fire retardant performance of the coating is far higher than technical requirements of a national standa |
Author | FAN FANGQIANG XIA ZHENGBIN LI QINGYING |
Author_xml | – fullname: FAN FANGQIANG – fullname: LI QINGYING – fullname: XIA ZHENGBIN |
BookMark | eNqNij0OglAQBl-hhX93WA9AglKIpSEaKysTCwuywoeQ4O7LstxfCg9gM5NJZhlmooJFeD7YYS81AY29GyfedkKDA_1EGysfDdR0EwzOVrM4VcreyZtYaoqGyDa1Cn3grdbkLQzarMO84X7A5udV2F7O9-KaIGqJIXIFgZfFbZfu8yw_podT9s_zBSSzPhE |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
ExternalDocumentID | CN102838907A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_CN102838907A3 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 12:12:09 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | Chinese English |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_CN102838907A3 |
Notes | Application Number: CN20121306682 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20121226&DB=EPODOC&CC=CN&NR=102838907A |
ParticipantIDs | epo_espacenet_CN102838907A |
PublicationCentury | 2000 |
PublicationDate | 20121226 |
PublicationDateYYYYMMDD | 2012-12-26 |
PublicationDate_xml | – month: 12 year: 2012 text: 20121226 day: 26 |
PublicationDecade | 2010 |
PublicationYear | 2012 |
RelatedCompanies | SOUTH CHINA UNIVERSITY OF TECHNOLOGY |
RelatedCompanies_xml | – name: SOUTH CHINA UNIVERSITY OF TECHNOLOGY |
Score | 2.9845743 |
Snippet | Provided is a waterborne ultra-thin steel structure fire retardant coating and a preparation method thereof. The raw material ratio of the coating includes... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | ADHESIVES CHEMICAL PAINT OR INK REMOVERS CHEMISTRY COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS CORRECTING FLUIDS DYES FILLING PASTES INKS METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS PAINTS PASTES OR SOLIDS FOR COLOURING OR PRINTING POLISHES USE OF MATERIALS THEREFOR WOODSTAINS |
Title | Waterborne ultra-thin steel structure fire retardant coating and preparation method thereof |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20121226&DB=EPODOC&locale=&CC=CN&NR=102838907A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1bS8MwFD7MKeqbTkXnhQjSt2Lt2q4-FHHpxhDWDZk68GGkScomIy1dh-Cv96TbnC_61guE5AvfuSTnAnAjhG9xR3J0S4Q0HR7bJpohMb5K6XmognxX5w73Iq_74jyN3FEFPta5MGWd0M-yOCIyiiPfi1JeZ5tDrLCMrZzfxlP8lD50hkForLzjOxTEtmeEraA96Id9alAa0MiInoNSj_roCT5uwTaa0U3NhvZrS2elZL9VSucAdgY4mioOofI1qcEeXXdeq8Fub3XhjY8r7s2P4P2NaQzSXEmymBU5M4vJVBHcJTkjyzKwi1ySBGUY0UGEuUDQCE-ZDmwmTAmS5XJZ6TtVZNk5mmjzT6bJMVx32kPaNXGW4x9IxjTaLKhxAlWVKnkKhLn3tsdd23KThpM0LRa7XEhmSRt56gvnDOp_j1P_7-c57Gt4dSCH7V1AFVclL1EdF_FVieM3yuCRaA |
link.rule.ids | 230,309,783,888,25576,76876 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1bT8IwFD5BNOKbokbxVhOzt8U5tjEfFiMdBBUGMagkPpCt7QKGdGSMmPjrPR0gvujbLknTfs13Lu25AFxx7hrMEgzdEi50i0WmjmZIhK9COA6qINdWucOdwGm9WI8De1CAj1UuTF4n9DMvjoiMYsj3LJfX0_Uhlp_HVs6uozF-Su6afc_Xlt7xDQpi09H8utfodf0u1Sj1aKAFz16uR130BO83YBNN7JpiQ-O1rrJSpr9VSnMXtno4msz2oPA1KkOJrjqvlWG7s7zwxscl92b78P4WKgySVAoyn2RpqGejsSS4S2JCFmVg56kgMcowooIIU46gEZaEKrCZhJKTaSoWlb4TSRado4ky_0QSH8Bls9GnLR1nOfyBZEiD9YKqh1CUiRRHQEL71nSYbRp2XLXimhFGNuMiNISJPHW5dQyVv8ep_PfzAkqtfqc9bD8ETyewo6BWQR2mcwpFXKE4Q9WcRec5pt_JP5Rb |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=Waterborne+ultra-thin+steel+structure+fire+retardant+coating+and+preparation+method+thereof&rft.inventor=FAN+FANGQIANG&rft.inventor=LI+QINGYING&rft.inventor=XIA+ZHENGBIN&rft.date=2012-12-26&rft.externalDBID=A&rft.externalDocID=CN102838907A |