Method for producing aerated building block with phosphogypsum as main raw material
The invention discloses a method for producing an aerated building block with phosphogypsum as a main raw material. The method comprises the steps of: adding phosphogypsum, industrial waste residues, mineral activator main components and aluminum powder or aluminum paste to a stirrer with adjust rot...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
27.06.2012
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention discloses a method for producing an aerated building block with phosphogypsum as a main raw material. The method comprises the steps of: adding phosphogypsum, industrial waste residues, mineral activator main components and aluminum powder or aluminum paste to a stirrer with adjust rotation speed, adding water, stirring, slowly stirring for 3min, then rapidly stirring for 2min, then adding mineral activator auxiliary components and auxiliary agents, rapidly stirring for 3min, pouring the obtained slurry to a mold, foaming for 30-40min, then standing and maintaining at 50-55 DEG C for 4h, demolding, cutting, and carrying out normal-pressure steam maintaining for 16-24h to obtain the aerated block. Compared with the prior art, the method has the advantages that the obtained aerated building block has stable physical performance and good heat insulation property, the utilization rate of phosphogypsum is high, the process is simple, the cost is low, natural resources are saved, and the like. The obt |
---|---|
Bibliography: | Application Number: CN201110410826 |