Production method of hot rolled steel coil for ship building
The invention relates to a production method of a hot rolled steel coil for ship building, comprising the following steps of: (1) designing components, preprocessing molten iron, then smelting in a converter, switching between nitrogen and argon, and tapping to obtain molten steel; (2) continuously...
Saved in:
Main Authors | , , , , , , , |
---|---|
Format | Patent |
Language | Chinese English |
Published |
20.07.2011
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | The invention relates to a production method of a hot rolled steel coil for ship building, comprising the following steps of: (1) designing components, preprocessing molten iron, then smelting in a converter, switching between nitrogen and argon, and tapping to obtain molten steel; (2) continuously casting the molten steel to obtain a plate blank, wherein the molten steel quantity of a tundish when the continuous casting tundish is stopped to be poured is controlled at 8-15t, and the liquid level is controlled at 200-350 mm; protecting the pouring in the whole process, wherein the inserting depth of a long water gap is 300-400 mm; (3) heating the plate blank; and (4) finally, rolling the heated plate blank and curling to obtain the hot rolled steel coil for ship building. The contents of C and Mn are reduced greatly by adopting a TMCP (Thermo Mechanical Control Process) and an RPC (Remote Position Control) rolling process and utilizing niobium microalloying, and the production cost is lowered; an E36-grade ho |
---|---|
AbstractList | The invention relates to a production method of a hot rolled steel coil for ship building, comprising the following steps of: (1) designing components, preprocessing molten iron, then smelting in a converter, switching between nitrogen and argon, and tapping to obtain molten steel; (2) continuously casting the molten steel to obtain a plate blank, wherein the molten steel quantity of a tundish when the continuous casting tundish is stopped to be poured is controlled at 8-15t, and the liquid level is controlled at 200-350 mm; protecting the pouring in the whole process, wherein the inserting depth of a long water gap is 300-400 mm; (3) heating the plate blank; and (4) finally, rolling the heated plate blank and curling to obtain the hot rolled steel coil for ship building. The contents of C and Mn are reduced greatly by adopting a TMCP (Thermo Mechanical Control Process) and an RPC (Remote Position Control) rolling process and utilizing niobium microalloying, and the production cost is lowered; an E36-grade ho |
Author | ZHOU YANJUAN LIU WANSHAN ZHANG QINGYU LIU LINGYUE YANG YUNQING CAO TAIPING ZHAO YANLING QIU XIANGGUANG |
Author_xml | – fullname: CAO TAIPING – fullname: ZHAO YANLING – fullname: YANG YUNQING – fullname: LIU LINGYUE – fullname: QIU XIANGGUANG – fullname: ZHANG QINGYU – fullname: ZHOU YANJUAN – fullname: LIU WANSHAN |
BookMark | eNrjYmDJy89L5WSwCSjKTylNLsnMz1PITS3JyE9RyE9TyMgvUSjKz8lJTVEoLklNzVFIzs_MUUjLL1IozsgsUEgqzcxJycxL52FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hgZGhkbmZhaWjsbEqAEA4dQxYA |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
ExternalDocumentID | CN102127689A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_CN102127689A3 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 16:40:42 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | Chinese English |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_CN102127689A3 |
Notes | Application Number: CN2011141873 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110720&DB=EPODOC&CC=CN&NR=102127689A |
ParticipantIDs | epo_espacenet_CN102127689A |
PublicationCentury | 2000 |
PublicationDate | 20110720 |
PublicationDateYYYYMMDD | 2011-07-20 |
PublicationDate_xml | – month: 07 year: 2011 text: 20110720 day: 20 |
PublicationDecade | 2010 |
PublicationYear | 2011 |
RelatedCompanies | NINGBO IRON & STEEL CO., LTD |
RelatedCompanies_xml | – name: NINGBO IRON & STEEL CO., LTD |
Score | 2.9235346 |
Snippet | The invention relates to a production method of a hot rolled steel coil for ship building, comprising the following steps of: (1) designing components,... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | ALLOYS CHEMISTRY CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS FERROUS OR NON-FERROUS ALLOYS GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS METALLURGY METALLURGY OF IRON MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE TREATMENT OF ALLOYS OR NON-FERROUS METALS |
Title | Production method of hot rolled steel coil for ship building |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20110720&DB=EPODOC&locale=&CC=CN&NR=102127689A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV3dS8MwED_mFPVNp6LzgwjSt-Jau36ARVzaMgS7IlP2NtImZZPRjq0i-Nd76YfzRd9CAuGS8EvuLne_A7hJeD9mhsZUxvUUDRTOVEc3U0Q8Z4xZtqxvIaMtQnP4ajxN-pMWvDe5MCVP6GdJjoiIShDvRXlfLzdOLK-MrVzfxnPsyh-CsespvHH39Sy9p3gD149G3ogqlLo0VMIXVyupzE3bedyCbalGS559_20gs1KWv5-U4AB2IpwtKw6h9TXrwB5tKq91YPe5_vDGZo299RHcRxU5K8pGqrrPJE_JLC_IShr_nOB5iQVJ8vmCoCZKZBgWieuq18dwHfhjOlRRjOnPmqc03Eh8dwLtLM_EKRBJRm8bqRBo_BlojcRmomumcLjh2KmW9M6g-_c83f8Gz2G_cpdaCJwLaBerD3GJ720RX5Ub9Q0PqYRx |
link.rule.ids | 230,309,786,891,25594,76906 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV3dS8MwED_mFOebTkXnVwTp23Dtun6ARVy6UnXrikzZ20iblk1GO7aK4F_vpWudL_oWEgiXhF9yd7n7HcBNyDsBU2XWZFyJ0UDhrGkqWoyI54wx3RD1LUS0hae5r-rTuDOuwHuZC5PzhH7m5IiIqBDxnuX39WLjxLLz2MrVbTDDrvTeGVm2xEt3X0tXWpLdtXr-0B5SiVKLepL3Ysk5lblmmA9bsK0Ldl6hOr11RVbK4veT4uzDjo-zJdkBVL6mdajRsvJaHXYHxYc3NgvsrQ7hzl-Ts6JsZF33maQxmaYZWQrjnxM8r2hOwnQ2J6iJEhGGRYKi6vURXDu9EXWbKMbkZ80T6m0kbh9DNUmT6ASIIKM31DiK0PhT0RoJtFCRtcjkqmnEctg6hcbf8zT-G7yCmjsa9Cf9R-_5DPbWrlMdQXQO1Wz5EV3g25sFl_mmfQNqA4de |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=Production+method+of+hot+rolled+steel+coil+for+ship+building&rft.inventor=CAO+TAIPING&rft.inventor=ZHAO+YANLING&rft.inventor=YANG+YUNQING&rft.inventor=LIU+LINGYUE&rft.inventor=QIU+XIANGGUANG&rft.inventor=ZHANG+QINGYU&rft.inventor=ZHOU+YANJUAN&rft.inventor=LIU+WANSHAN&rft.date=2011-07-20&rft.externalDBID=A&rft.externalDocID=CN102127689A |