DECREASE OF CRACK-FORMATION IN LOW-CARBON CONSTRUCTIONAL HIGH-QUALITY BAR OF THE CONTINUOUSLY CAST SLUG

Features formation of cracks in steel 18хГТ are investigated. It is established that in the course of crystallization the peritectic transformation goes on phase reactions: formation of primary ferrite from liquid and formation of peritectic austenite from this ferrite and residual liquid.

Saved in:
Bibliographic Details
Published inLitʹë i metallurgiâ no. 2; pp. 66 - 70
Main Authors S. M. Borschov, V. A. Lutsenko, T. N. Golubenko, I. A. Kovalyova, A. V. Vengura, A. N. Hodosovskaya, V. I. Gritsaenko
Format Journal Article
LanguageEnglish
Published Belarusian National Technical University 01.05.2012
Online AccessGet full text

Cover

Loading…
Abstract Features formation of cracks in steel 18хГТ are investigated. It is established that in the course of crystallization the peritectic transformation goes on phase reactions: formation of primary ferrite from liquid and formation of peritectic austenite from this ferrite and residual liquid.
AbstractList Features formation of cracks in steel 18хГТ are investigated. It is established that in the course of crystallization the peritectic transformation goes on phase reactions: formation of primary ferrite from liquid and formation of peritectic austenite from this ferrite and residual liquid.
Author A. V. Vengura
I. A. Kovalyova
S. M. Borschov
V. A. Lutsenko
V. I. Gritsaenko
A. N. Hodosovskaya
T. N. Golubenko
Author_xml – sequence: 1
  fullname: S. M. Borschov
  organization: Byelorussian Steel Works
– sequence: 2
  fullname: V. A. Lutsenko
  organization: Iron and Steel Institute of NAS Ukraine
– sequence: 3
  fullname: T. N. Golubenko
  organization: Iron and Steel Institute of NAS Ukraine
– sequence: 4
  fullname: I. A. Kovalyova
  organization: Byelorussian Steel Works
– sequence: 5
  fullname: A. V. Vengura
  organization: Byelorussian Steel Works
– sequence: 6
  fullname: A. N. Hodosovskaya
  organization: Белорусский металлургический завод
– sequence: 7
  fullname: V. I. Gritsaenko
  organization: Byelorussian Steel Works
BookMark eNqtjNFOgzAARRszE9HtH_oDTQqlBR-7WkYj0qyUmD01HXQLZg4Dvvj3ivETfLq599yce7C6jtdwA6IkjVOEU8xWIIpZThDDjN6BzTwPR0xYQlmSkAicn6QwkjcS6gIKw8UzKrR54VbpGqoaVvoVCW62P03ourGmFQviFSzVrkT7llfKHuCWm0VgS7ncrKpb3TbVAQreWNhU7W4Nbk_-MofNXz4AVUgrStSP_s19TMO7n77c6Af3O4zT2fnpc-guwVEap7gPAbPQp32cPWY46_IQOnKiR5Jj8p-ub66dW0I
ContentType Journal Article
DBID DOA
DatabaseName Directory of Open Access Journals
DatabaseTitleList
Database_xml – sequence: 1
  dbid: DOA
  name: Directory of Open Access Journals
  url: https://www.doaj.org/
  sourceTypes: Open Website
DeliveryMethod fulltext_linktorsrc
Discipline Engineering
EISSN 2414-0406
EndPage 70
ExternalDocumentID oai_doaj_org_article_55140dee06ed4d179707c8eec3f5b380
GroupedDBID ALMA_UNASSIGNED_HOLDINGS
GROUPED_DOAJ
M~E
ID FETCH-doaj_primary_oai_doaj_org_article_55140dee06ed4d179707c8eec3f5b3803
IEDL.DBID DOA
ISSN 1683-6065
IngestDate Tue Oct 22 15:14:37 EDT 2024
IsOpenAccess true
IsPeerReviewed true
IsScholarly true
Issue 2
Language English
LinkModel DirectLink
MergedId FETCHMERGED-doaj_primary_oai_doaj_org_article_55140dee06ed4d179707c8eec3f5b3803
OpenAccessLink https://doaj.org/article/55140dee06ed4d179707c8eec3f5b380
ParticipantIDs doaj_primary_oai_doaj_org_article_55140dee06ed4d179707c8eec3f5b380
PublicationCentury 2000
PublicationDate 2012-05-01
PublicationDateYYYYMMDD 2012-05-01
PublicationDate_xml – month: 05
  year: 2012
  text: 2012-05-01
  day: 01
PublicationDecade 2010
PublicationTitle Litʹë i metallurgiâ
PublicationYear 2012
Publisher Belarusian National Technical University
Publisher_xml – name: Belarusian National Technical University
SSID ssib036256223
ssj0001928113
ssib023638480
ssib027512848
ssib044751577
Score 3.6877353
Snippet Features formation of cracks in steel 18хГТ are investigated. It is established that in the course of crystallization the peritectic transformation goes on...
SourceID doaj
SourceType Open Website
StartPage 66
Title DECREASE OF CRACK-FORMATION IN LOW-CARBON CONSTRUCTIONAL HIGH-QUALITY BAR OF THE CONTINUOUSLY CAST SLUG
URI https://doaj.org/article/55140dee06ed4d179707c8eec3f5b380
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwrZ1LT4QwEMcb40kPxmd8pwevjaWlgEe2sgvKQsIj7p4Ij2LiYTVm_f5O6Ubx5EGPNKRMhmnnP037K0I3dU97TUIjdaMYseHHwpjzOFF13di1Kzpq6QPO88QJS_thIRajq770njCDBzaOu9UZnXZKUUd1dgfh41K39ZRqeS8a7plqnd6NiimIJMYhrEYgM-YKPQ9_RRrM2pD3vxOjpt5ZYnMi88XoHs8a7la2HLAcVL74AfUfss90H-1tZCP2jbkHaEutDtHuCCZ4hJ7vA5kFfh7gdIpl5stHAhXefFiDwlGC4_SJSD-bwJNMk7zISmlAuDiMZiEBaRtHxRJP_Ex3UISBfq2IkjIt83iJpZ8XOI_L2TGKpkEhQ6LtrN4MraLS_OihAbxabbxa_eZVfoK2V68rdYowcxsNsGlbBkPXVr3XMM5rBypLRrnw2jM0-fv3zv-jkwu0A3KGme2Il2h7_f6hrkAyrJvrITo-AZGSta0
link.rule.ids 315,783,787,2109
linkProvider Directory of Open Access Journals
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=DECREASE+OF+CRACK-FORMATION+IN+LOW-CARBON+CONSTRUCTIONAL+HIGH-QUALITY+BAR+OF+THE+CONTINUOUSLY+CAST+SLUG&rft.jtitle=Lit%CA%B9%C3%AB+i+metallurgi%C3%A2&rft.au=S.+M.+Borschov&rft.au=V.+A.+Lutsenko&rft.au=T.+N.+Golubenko&rft.au=I.+A.+Kovalyova&rft.date=2012-05-01&rft.pub=Belarusian+National+Technical+University&rft.issn=1683-6065&rft.eissn=2414-0406&rft.issue=2&rft.spage=66&rft.epage=70&rft.externalDBID=DOA&rft.externalDocID=oai_doaj_org_article_55140dee06ed4d179707c8eec3f5b380
thumbnail_l http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=1683-6065&client=summon
thumbnail_m http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=1683-6065&client=summon
thumbnail_s http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=1683-6065&client=summon