Bibliography:Short carbon fiber felts with an initial porosity of 89.5% were deposited by isobaric, isothermal chemical vapor infiltration using natural gas as carbon source. The bulk density of the deposited carbon/carbon (C/C) composites was 1.89 g/cm3 after depositing for 150 h. The microstructure and mechanical properties of the C/C composites were studied by polarized light microscopy, X-ray diffraction, scanning electron microscopy and three-point bending test. The results reveal that high textured pyrolytic carbon is deposited as the matrix of the composites, whose crystalline thickness and graphitization degree highly increase after heat treatment. A distinct decrease of the flexural strength and modulus accompanied by the increase of the toughness of the C/C composites is found to be correlated with the structural changes in the composites during the heat treatment process.
43-1239/TG
carbon/carbon composites; high texture; chemical vapor infiltration; graphitization degree; mechanical properties
Wei LI,He-jun LI,Jie WANG,Shou-yang ZHANG,Xi YANG,Jian-feng WEI (C/C Composites Research Center,State Key Laboratory of Solidification Processing,Northwestern Polytechnical University,Xi’an 710072,China)