고압 다이캐스팅으로 제조된 Al-10Si-0.3Mg-0.6Mn 합금에서 blister 발생과 강도의 균형을 고려한 최적 열처리 공정 설계
The aim of this study was to optimize a solid solution treatment for a high pressure die casting Al-10Si-0.3Mg-0.6Mn alloy to avoid blistering and to improve the strength of the alloy. To achieve this goal, the number density of the blisters and the strength of the alloy under various solid solution...
Saved in:
Published in | 한국주조공학회지 Vol. 40; no. 3; pp. 66 - 75 |
---|---|
Main Authors | , , , , , , , |
Format | Journal Article |
Language | Korean |
Published |
한국주조공학회
30.06.2020
|
Subjects | |
Online Access | Get full text |
ISSN | 1598-706X 2288-8381 |
Cover
Abstract | The aim of this study was to optimize a solid solution treatment for a high pressure die casting Al-10Si-0.3Mg-0.6Mn alloy to avoid blistering and to improve the strength of the alloy. To achieve this goal, the number density of the blisters and the strength of the alloy under various solid solution treatment (SST) conditions were evaluated. The SST was performed at 470, 490, 510 and 530℃ for 20, 60, 120, 240 and 480 min on the alloy. The number density of the blisters increased with the increasing temperature and time of the SST and the defect area fraction. The yield strength of the alloy after the T6 heat treatment increased with the increasing SST temperature and time. Based on the results, it is suggested that SST should be performed at 510℃ within 60 min. or at 470 and 490℃ within 240 min. to avoid blistering and to improve the strength. |
---|---|
AbstractList | The aim of this study was to optimize a solid solution treatment for a high pressure die casting Al-10Si-0.3Mg-0.6Mn alloy to avoid blistering and to improve the strength of the alloy. To achieve this goal, the number density of the blisters and the strength of the alloy under various solid solution treatment (SST) conditions were evaluated. The SST was performed at 470, 490, 510 and 530℃ for 20, 60, 120, 240 and 480 min on the alloy. The number density of the blisters increased with the increasing temperature and time of the SST and the defect area fraction. The yield strength of the alloy after the T6 heat treatment increased with the increasing SST temperature and time. Based on the results, it is suggested that SST should be performed at 510℃ within 60 min. or at 470 and 490℃ within 240 min. to avoid blistering and to improve the strength. The aim of this study was to optimize a solid solution treatment for a high pressure die casting Al-10Si-0.3Mg-0.6Mn alloy to avoid blistering and to improve the strength of the alloy. To achieve this goal, the number density of the blisters and the strength of the alloy under various solid solution treatment (SST) conditions were evaluated. The SST was performed at 470, 490, 510 and 530o C for 20, 60, 120, 240 and 480 min on the alloy. The number density of the blisters increased with the increasing temperature and time of the SST and the defect area fraction. The yield strength of the alloy after the T6 heat treatment increased with the increasing SST temperature and time. Based on the results, it is suggested that SST should be performed at 510o C within 60 min. or at 470 and 490o C within 240 min. to avoid blistering and to improve the strength. KCI Citation Count: 0 |
Author | 조영희 이정무 Jung-moo Lee Min-su Jo Young-hee Cho 조민수 Soo-bae Kim 김수배 |
Author_xml | – sequence: 1 fullname: 김수배 – sequence: 2 fullname: Soo-bae Kim – sequence: 3 fullname: 조영희 – sequence: 4 fullname: Young-hee Cho – sequence: 5 fullname: 조민수 – sequence: 6 fullname: Min-su Jo – sequence: 7 fullname: 이정무 – sequence: 8 fullname: Jung-moo Lee |
BackLink | https://www.kci.go.kr/kciportal/ci/sereArticleSearch/ciSereArtiView.kci?sereArticleSearchBean.artiId=ART002607817$$DAccess content in National Research Foundation of Korea (NRF) |
BookMark | eNo9j01LG1EUhi-iYBr9BW7upgsXI_cjmXtnGaS2fiHYLNxd7nzJkHRSZty4FKdQqmA2o1lMYIRQKHQRjKKIv2jm5D_0UkXO4byL8_Aczge0GA_iYAE1GJPSklzSRdSgbUdagthHy2g1TSOXEErbVAq7ga6rWQl5juuLCYzv4XkIvybzyx9QvNS3BYaygNtpPSxwp29R8jWyyAbfPzbT3o_xPP9TPf2EmyFkBXb7UXoSJLieFnA-rmYvuJrm9VUG4xGuHsv5KIdxhs21upzMc6N-KKA8w3BzD3ej-vdfs3qAMseQTapZtoKWQt1Pg9W3bKLu1qfu5hdr7-Dz9mZnz-rJlrAYpX7A3cCRwqVSc6-lZSu0Q-0EwqGUhML3dBB6vi1aNnNDz_NZyLnWlLrE4Yw30fqrNk5C1fMiNdDR_zweqF6iOofdbeW0ObGJMOzHV7ZnHo1U7Kd9tdPZPWDElCPaQjDJTTfR2juXqu9J9E0np4pLJo2E_wNAHKC9 |
ContentType | Journal Article |
DBID | HZB Q5X JDI ACYCR |
DEWEY | 671.2 |
DatabaseName | Korea Information Science Society (KISS) Korean Studies Information Service System (KISS) B-Type KoreaScience Korean Citation Index |
DatabaseTitleList | |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Engineering |
DocumentTitleAlternate | 고압 다이캐스팅으로 제조된 Al-10Si-0.3Mg-0.6Mn 합금에서 blister 발생과 강도의 균형을 고려한 최적 열처리 공정 설계 Optimization of Solid Solution Treatment Process for a High Pressure Die Casting Al-10Si-0.3Mg-0.6Mn alloy to avoid Blistering and Improve the Strength of the Alloy |
EISSN | 2288-8381 |
EndPage | 75 |
ExternalDocumentID | oai_kci_go_kr_ARTI_9530607 JAKO202029757728328 3828073 |
GroupedDBID | .UV HZB Q5X ALMA_UNASSIGNED_HOLDINGS JDI ACYCR |
ID | FETCH-LOGICAL-k847-211de3be987b18a3c4a84f6fa9e79110f7dcaefcd67462bfccd2f33aa11b09323 |
ISSN | 1598-706X |
IngestDate | Mon Jan 29 08:27:02 EST 2024 Fri Dec 22 12:01:01 EST 2023 Wed Jul 30 02:15:12 EDT 2025 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | true |
Issue | 3 |
Keywords | 3Mg-0 6Mn Solid solution treatment Blistering Yield strength Al-10Si-0 Die casting |
Language | Korean |
LinkModel | OpenURL |
MergedId | FETCHMERGED-LOGICAL-k847-211de3be987b18a3c4a84f6fa9e79110f7dcaefcd67462bfccd2f33aa11b09323 |
Notes | The Korean Foundrymen`s Society KISTI1.1003/JNL.JAKO202029757728328 |
OpenAccessLink | http://click.ndsl.kr/servlet/LinkingDetailView?cn=JAKO202029757728328&dbt=JAKO&org_code=O481&site_code=SS1481&service_code=01 |
PageCount | 10 |
ParticipantIDs | nrf_kci_oai_kci_go_kr_ARTI_9530607 kisti_ndsl_JAKO202029757728328 kiss_primary_3828073 |
PublicationCentury | 2000 |
PublicationDate | 20200630 |
PublicationDateYYYYMMDD | 2020-06-30 |
PublicationDate_xml | – month: 06 year: 2020 text: 20200630 day: 30 |
PublicationDecade | 2020 |
PublicationTitle | 한국주조공학회지 |
PublicationTitleAlternate | 한국주조공학회지 (주조) |
PublicationYear | 2020 |
Publisher | 한국주조공학회 |
Publisher_xml | – name: 한국주조공학회 |
SSID | ssib001151876 ssib053377469 ssib010775658 ssib008451706 ssib012146324 ssib020092134 |
Score | 2.1077943 |
Snippet | The aim of this study was to optimize a solid solution treatment for a high pressure die casting Al-10Si-0.3Mg-0.6Mn alloy to avoid blistering and to improve... |
SourceID | nrf kisti kiss |
SourceType | Open Website Open Access Repository Publisher |
StartPage | 66 |
SubjectTerms | 3Mg-0 6Mn Al-10Si-0 Blistering Die casting Solid solution treatment Yield strength 금속공학 |
Title | 고압 다이캐스팅으로 제조된 Al-10Si-0.3Mg-0.6Mn 합금에서 blister 발생과 강도의 균형을 고려한 최적 열처리 공정 설계 |
URI | https://kiss.kstudy.com/ExternalLink/Ar?key=3828073 http://click.ndsl.kr/servlet/LinkingDetailView?cn=JAKO202029757728328&dbt=JAKO&org_code=O481&site_code=SS1481&service_code=01 https://www.kci.go.kr/kciportal/ci/sereArticleSearch/ciSereArtiView.kci?sereArticleSearchBean.artiId=ART002607817 |
Volume | 40 |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
ispartofPNX | 한국주조공학회지, 2020, 40(3), , pp.66-75 |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwpR1daxNB8Kh98kUqVawf5RDvKURu73PvcS9JqZXogxX6dtxnKSlp6ceLD4IYQVSwL7F9SCCFIAg-FNuiSH9RsvkPzuzdJVepUBXCsjezO7szs5udOW5nJOkBHKp-gi_dNbwhY6hhUg5UGpZppMUOMQJihXhRuP7EWnxuLK2YK1PTM4WvlnZ3gofhiwvvlfyLVgEGesVbsn-h2TFRAEAd9AslaBjKS-lYqTHF1RWmKrWK4pjwKyk1V6GuwgwBqiquqLhMcUQjygSqqlCom6INYCvYixGolxAE9ACKFaK4KuIchJTYOvydPlsrgwteX4XSqsPKAVowMnPEXKhCqSBq5-MZ2BHfdGEwRiTl5sSpjvNLOXBxYCZwpuBgAXumHDg0xdmCT3wWjQSOGqWCDFwsU_ZQGCkzrpkzo4LVXMpml4lFQ2rYz1JYJSflmrkQzFLGAxIVuDTRXG7Nj0cSWJBCVfTUhUTH4hsTTRs7osJQA9jGxm9NYJ0bUNLia2_R0UEszoFmMwWCrjppMh6kgnhKBO2qMgmoeU6NbCGbmSBXbDJeKSxXAQPxGMV3Qpqaf8CY7eL_5L54HGK0WVXkmgRrQcA0DXYh1dNEO9mxZ1kFAyrNhHM-tPlvJse54OaNcM1b3fAaWx64cI88xwQvFuNDXNEJHlz1l7WJfQ_2KS3Yz9QwMfxT_kwwnmMhmBHBrPWFdAQiwhiZxEMEVwe8H5H2cswpmGbguW2Dr4oO3BqYnM2tpGByLs9I1zJfUWbpxr8uTTU2ZqVPg-Meb7fl4fs-757wn3v8XX_04Q3vnA0POzLvdfjh0XCvI1-wWeVR-8vgx1u-v8dbHTnblPLwqMNfdwfHZ_LgqD382OLdA3nwvTc6aPNuS4bRhr3-qA2kTzu890rm-yf828Hw81dAnfJeW-at_uC4dUNaXqgtVxbLWXKVcoNicBZColgPYofaAaG-Hho-NRIr8Z3YBvtHTewo9OMkjCwQkBYkYRhpia77PiGBCj6fflOabm4041uSnAQxAZRh-TYxImpQIwr1xHHAFrDswNfnpFmUqLeZhs_xdIoRuAA8LyTsNaPtdW-JPX6KKxkv-oPDD3YGnZPug-jF8vjzMrl9mUZ3pKuTXXJXmt7Z2o3vgS-xE8yL9fULab7uLA |
linkProvider | ISSN International Centre |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=%EA%B3%A0%EC%95%95+%EB%8B%A4%EC%9D%B4%EC%BA%90%EC%8A%A4%ED%8C%85%EC%9C%BC%EB%A1%9C+%EC%A0%9C%EC%A1%B0%EB%90%9C+Al-10Si-0.3Mg-0.6Mn+%ED%95%A9%EA%B8%88%EC%97%90%EC%84%9C+blister+%EB%B0%9C%EC%83%9D%EA%B3%BC+%EA%B0%95%EB%8F%84%EC%9D%98+%EA%B7%A0%ED%98%95%EC%9D%84+%EA%B3%A0%EB%A0%A4%ED%95%9C+%EC%B5%9C%EC%A0%81+%EC%97%B4%EC%B2%98%EB%A6%AC+%EA%B3%B5%EC%A0%95+%EC%84%A4%EA%B3%84&rft.jtitle=%ED%95%9C%EA%B5%AD%EC%A3%BC%EC%A1%B0%EA%B3%B5%ED%95%99%ED%9A%8C%EC%A7%80%2C+40%283%29&rft.au=%EA%B9%80%EC%88%98%EB%B0%B0&rft.au=%EC%A1%B0%EC%98%81%ED%9D%AC&rft.au=%EC%A1%B0%EB%AF%BC%EC%88%98&rft.au=%EC%9D%B4%EC%A0%95%EB%AC%B4&rft.date=2020-06-30&rft.pub=%ED%95%9C%EA%B5%AD%EC%A3%BC%EC%A1%B0%EA%B3%B5%ED%95%99%ED%9A%8C&rft.issn=1598-706X&rft.eissn=2288-8381&rft.spage=66&rft.epage=75&rft.externalDBID=n%2Fa&rft.externalDocID=oai_kci_go_kr_ARTI_9530607 |
thumbnail_l | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=1598-706X&client=summon |
thumbnail_m | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=1598-706X&client=summon |
thumbnail_s | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=1598-706X&client=summon |