Stretchable Gas Barrier Achieved with Partially Hydrogen-Bonded Multilayer Nanocoating
Super gas barrier nanocoatings are recently demonstrated by combining polyelectrolytes and clay nanoplatelets with layer‐by‐layer deposition. These nanobrick wall thin films match or exceed the gas barrier of SiOx and metallized films, but they are relatively stiff and lose barrier with significant...
Saved in:
Published in | Macromolecular rapid communications. Vol. 35; no. 10; pp. 960 - 964 |
---|---|
Main Authors | , , , , , |
Format | Journal Article |
Language | English |
Published |
Weinheim
Blackwell Publishing Ltd
01.05.2014
Wiley |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Super gas barrier nanocoatings are recently demonstrated by combining polyelectrolytes and clay nanoplatelets with layer‐by‐layer deposition. These nanobrick wall thin films match or exceed the gas barrier of SiOx and metallized films, but they are relatively stiff and lose barrier with significant stretching (≥10% strain). In an effort to impart stretchability, hydrogen‐bonding polyglycidol (PGD) layers are added to an electrostatically bonded thin film assembly of polyethylenimine (PEI) and montmorillonite (MMT) clay. The oxygen transmission rate of a 125‐nm thick PEI‐MMT film increases more than 40x after being stretched 10%, while PGD‐PEI‐MMT trilayers of the same thickness maintain its gas barrier. This stretchable trilayer system has an OTR three times lower than the PEI‐MMT bilayer system after stretching. This report marks the first stretchable high gas barrier thin film, which is potentially useful for applications that require pressurized elastomers.
A stretchable, clay‐filled thin film that imparts oxygen barrier is produced using layer‐by‐layer assembly of electrostatic and hydrogen‐bonding polymers/platelets. This stretchable nanocoating is compared with a brittle film of the same thickness on PET. The brittle film is initially a better barrier, but after 10% strain its barrier properties are diminished by 4350%. The stretchable film retains its original barrier and is three times better than the brittle film after stretching. |
---|---|
Bibliography: | Texas A&M Engineering Experiment Station ArticleID:MARC201400104 istex:B9642F57E38DA5C1079C92199A31ACEBED7AF629 ark:/67375/WNG-Z872VTRG-5 ObjectType-Article-1 SourceType-Scholarly Journals-1 ObjectType-Feature-2 content type line 23 ObjectType-Article-2 ObjectType-Feature-1 |