Metal dusting behaviour of welded Ni-base alloys with different surface finish

Welded Ni‐base alloys and Alloy 800 were exposed under metal dusting conditions at 600°C and 650°C for up to 6000 hours. Alloy 800 was attacked very strongly already in the first days and Alloy 600 also rather soon and widespread, on both materials attack started mainly in the heat affected zone. Se...

Full description

Saved in:
Bibliographic Details
Published inMaterials and corrosion Vol. 54; no. 10; pp. 785 - 792