Yang, X., Lu-ming, H., & Zhao-hui, C. (2014). Degradation of CVD-SiC coated PIP-C/SiC composites exposed to the hot firing test based on MMH/N2O4 bipropellants. Ceramics international, 40(7), 10303-10308. https://doi.org/10.1016/j.ceramint.2014.03.001
Chicago Style (17th ed.) CitationYang, Xiang, Huang Lu-ming, and Chen Zhao-hui. "Degradation of CVD-SiC Coated PIP-C/SiC Composites Exposed to the Hot Firing Test Based on MMH/N2O4 Bipropellants." Ceramics International 40, no. 7 (2014): 10303-10308. https://doi.org/10.1016/j.ceramint.2014.03.001.
MLA (9th ed.) CitationYang, Xiang, et al. "Degradation of CVD-SiC Coated PIP-C/SiC Composites Exposed to the Hot Firing Test Based on MMH/N2O4 Bipropellants." Ceramics International, vol. 40, no. 7, 2014, pp. 10303-10308, https://doi.org/10.1016/j.ceramint.2014.03.001.