Effect of high-temperature heat treatment duration on the purity and microstructure of MWCNTs
The effect of high-temperature heat treatment on purity and structural changes of multiwalled carbon nanotubes (MWCNTs) were studied by subjecting the raw MWCNTs (pristine MWCNTs) to 2600 ∘ C for 60 and 120 min. Thermogravimetric analysis (TGA), X-ray diffraction, Raman spectroscopy, transmission el...
Saved in:
Published in | Bulletin of materials science Vol. 39; no. 1; pp. 41 - 46 |
---|---|
Main Authors | , , , , , |
Format | Journal Article |
Language | English |
Published |
Bangalore, India
Indian Academy of Sciences
01.02.2016
Springer Nature B.V |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | The effect of high-temperature heat treatment on purity and structural changes of multiwalled carbon nanotubes (MWCNTs) were studied by subjecting the raw MWCNTs (pristine MWCNTs) to 2600
∘
C for 60 and 120 min. Thermogravimetric analysis (TGA), X-ray diffraction, Raman spectroscopy, transmission electron microscopy (TEM) and scanning electron microscopy (SEM) were used to study the effect of heat-treatment duration on the purity and structural changes of MWCNTs. Results show that high-temperature heat treatment can be used to purify MWCNTs with proper optimization of treatment time. It was observed that 60 min heat treatment of raw MWCNTs imparts high purity and structural perfection to MWCNTs, while 120 min heat treatment imparts structural degradation to MWCNTs with collapse of the innermost shells. The present study indicates that metal impurities act as moderators in controlling the degradation of MWCNTs up to certain duration, and once the metal impurities escape completely, further heat treatment degrades the structure of MWCNTs. |
---|---|
AbstractList | The effect of high-temperature heat treatment on purity and structural changes of multiwalled carbon nanotubes (MWCNTs) were studied by subjecting the raw MWCNTs (pristine MWCNTs) to 2600∘C for 60 and 120 min. Thermogravimetric analysis (TGA), X-ray diffraction, Raman spectroscopy, transmission electron microscopy (TEM) and scanning electron microscopy (SEM) were used to study the effect of heat-treatment duration on the purity and structural changes of MWCNTs. Results show that high-temperature heat treatment can be used to purify MWCNTs with proper optimization of treatment time. It was observed that 60 min heat treatment of raw MWCNTs imparts high purity and structural perfection to MWCNTs, while 120 min heat treatment imparts structural degradation to MWCNTs with collapse of the innermost shells. The present study indicates that metal impurities act as moderators in controlling the degradation of MWCNTs up to certain duration, and once the metal impurities escape completely, further heat treatment degrades the structure of MWCNTs. The effect of high-temperature heat treatment on purity and structural changes of multiwalled carbon nanotubes (MWCNTs) were studied by subjecting the raw MWCNTs (pristine MWCNTs) to 2600 ∘ C for 60 and 120 min. Thermogravimetric analysis (TGA), X-ray diffraction, Raman spectroscopy, transmission electron microscopy (TEM) and scanning electron microscopy (SEM) were used to study the effect of heat-treatment duration on the purity and structural changes of MWCNTs. Results show that high-temperature heat treatment can be used to purify MWCNTs with proper optimization of treatment time. It was observed that 60 min heat treatment of raw MWCNTs imparts high purity and structural perfection to MWCNTs, while 120 min heat treatment imparts structural degradation to MWCNTs with collapse of the innermost shells. The present study indicates that metal impurities act as moderators in controlling the degradation of MWCNTs up to certain duration, and once the metal impurities escape completely, further heat treatment degrades the structure of MWCNTs. |
Author | GHOSAL, P PADMAVATHI, N SRIKANTH, I PRASAD, P S R JAIN, R K SUBRAHMANYAM, CH |
Author_xml | – sequence: 1 givenname: I surname: SRIKANTH fullname: SRIKANTH, I email: i_srikanth@yahoo.co.uk organization: Indian Institute of Technology, Advanced Systems Laboratory – sequence: 2 givenname: N surname: PADMAVATHI fullname: PADMAVATHI, N organization: Advanced Systems Laboratory – sequence: 3 givenname: P S R surname: PRASAD fullname: PRASAD, P S R organization: National Geophysical Research Institute (CSIR-NGRI) – sequence: 4 givenname: P surname: GHOSAL fullname: GHOSAL, P organization: Defence Metallurgical Research Laboratory – sequence: 5 givenname: R K surname: JAIN fullname: JAIN, R K organization: Indian Institute of Technology – sequence: 6 givenname: CH surname: SUBRAHMANYAM fullname: SUBRAHMANYAM, CH organization: Indian Institute of Technology |
BookMark | eNp1kE1LAzEQhoNUsFZ_gLeA5-hMkk12j1LqB1S9VDxJ2I-k3WJ3a5I99N-buoInYZgJw_u8E95zMun6zhJyhXCDAPo2IAchGWDGIC-Q8RMyhUILppUqJunNM2BSgz4j5yFsAbCQEqfkY-GcrSPtHd206w2Ldre3voyDt3Rjy0ijT31nu0ibIe3bvqOp4sbS_eDbeKBl19BdW_s-RD_UP2Aye36fv6zCBTl15Wewl79zRt7uF6v5I1u-PjzN75asFlkRWVVqIbiUsqkAJKiscqrCHHK0zqoatVS8aqDOnUanucgxb5ziKATmwrpKzMj16Lv3_ddgQzTbfvBdOml4gYVGrTKVVDiqjp8N3jqz9-2u9AeDYI4pmjFFk1I0xxQNTwwfmZC03dr6P-f_oW9M0XZY |
CitedBy_id | crossref_primary_10_1016_j_ijhydene_2020_11_041 crossref_primary_10_1016_j_jallcom_2019_02_217 crossref_primary_10_1016_j_carbon_2024_119004 crossref_primary_10_1021_acs_cgd_0c01464 crossref_primary_10_3390_catal10080927 crossref_primary_10_1016_j_carbon_2020_06_004 crossref_primary_10_1007_s10973_020_10458_8 crossref_primary_10_1007_s11664_020_07995_1 crossref_primary_10_3390_en17102437 crossref_primary_10_1007_s10853_021_06523_8 crossref_primary_10_1016_j_apsusc_2021_152148 crossref_primary_10_1016_j_diamond_2019_107485 crossref_primary_10_1016_j_surfin_2021_101361 |
Cites_doi | 10.1016/j.cplett.2003.09.027 10.1016/S0008-6223(02)00044-1 10.1016/j.cplett.2004.09.024 10.1021/jp060271h 10.1021/jp002817k 10.1021/la047268e 10.1063/1.1468892 10.1021/jp0672914 10.1016/j.carbon.2008.09.009 10.1016/S0008-6223(03)00390-7 10.1557/JMR.1999.0607 10.1016/S0008-6223(03)00330-0 10.1016/S0008-6223(00)00301-8 10.1016/S0008-6223(03)00250-1 10.1016/S0008-6223(03)00076-9 |
ContentType | Journal Article |
Copyright | Indian Academy of Sciences 2016 Indian Academy of Sciences 2016. |
Copyright_xml | – notice: Indian Academy of Sciences 2016 – notice: Indian Academy of Sciences 2016. |
DBID | AAYXX CITATION 7SR 8BQ 8FD 8FE 8FG ABJCF AFKRA BENPR BGLVJ CCPQU D1I DWQXO HCIFZ JG9 KB. PDBOC PQEST PQQKQ PQUKI |
DOI | 10.1007/s12034-015-0891-2 |
DatabaseName | CrossRef Engineered Materials Abstracts METADEX Technology Research Database ProQuest SciTech Collection ProQuest Technology Collection Materials Science & Engineering Collection ProQuest Central UK/Ireland ProQuest Central Technology Collection ProQuest One Community College ProQuest Materials Science Collection ProQuest Central Korea SciTech Premium Collection Materials Research Database Materials Science Database Materials Science Collection ProQuest One Academic Eastern Edition (DO NOT USE) ProQuest One Academic ProQuest One Academic UKI Edition |
DatabaseTitle | CrossRef ProQuest Materials Science Collection Materials Research Database Technology Collection Technology Research Database ProQuest One Academic Eastern Edition Materials Science Collection SciTech Premium Collection ProQuest One Community College ProQuest Technology Collection ProQuest SciTech Collection METADEX ProQuest Central Engineered Materials Abstracts ProQuest One Academic UKI Edition ProQuest Central Korea Materials Science & Engineering Collection Materials Science Database ProQuest One Academic |
DatabaseTitleList | ProQuest Materials Science Collection |
Database_xml | – sequence: 1 dbid: 8FG name: ProQuest Technology Collection url: https://search.proquest.com/technologycollection1 sourceTypes: Aggregation Database |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Engineering |
EISSN | 0973-7669 |
EndPage | 46 |
ExternalDocumentID | 10_1007_s12034_015_0891_2 |
GeographicLocations | Netherlands |
GeographicLocations_xml | – name: Netherlands |
GroupedDBID | -4Y -58 -5G -BR -EM -Y2 -~C .86 .VR 06C 06D 0R~ 0VY 1SB 2.D 203 23N 28- 2J2 2JN 2JY 2KG 2KM 2LR 2VQ 2WC 2~H 30V 4.4 406 408 40E 5GY 5VS 67Z 6J9 6NX 8TC 8UJ 95- 95. 95~ 96X AAAVM AABHQ AABYN AAFGU AAGCJ AAHNG AAIAL AAIKT AAJKR AANZL AAPBV AARHV AARTL AATNV AATVU AAUCO AAUYE AAWCG AAYFA AAYIU AAYQN AAYTO ABDBF ABDZT ABECU ABFGW ABFTV ABHQN ABJCF ABJNI ABJOX ABKAS ABKCH ABMNI ABMQK ABNWP ABPTK ABQBU ABSXP ABTEG ABTHY ABTKH ABTMW ABULA ABWNU ABXPI ACBMV ACBRV ACBXY ACBYP ACGFO ACGFS ACHSB ACHXU ACIGE ACIPQ ACIWK ACKNC ACMDZ ACMLO ACOKC ACOMO ACREN ACSNA ACTTH ACVWB ACWMK ADHHG ADHIR ADINQ ADKNI ADKPE ADMDM ADOXG ADRFC ADTPH ADURQ ADYFF ADYOE ADZKW AEBTG AEEQQ AEFTE AEGAL AEGNC AEGXH AEJHL AEJRE AEKMD AENEX AEOHA AEPYU AESKC AESTI AETLH AEVLU AEVTX AEXYK AFEXP AFGCZ AFKRA AFLOW AFNRJ AFQWF AFWTZ AFYQB AFZKB AGAYW AGDGC AGGBP AGGDS AGJBK AGMZJ AGQMX AGWIL AGWZB AGYKE AHAVH AHBYD AHKAY AHSBF AHYZX AIAGR AIAKS AIDUJ AIIXL AILAN AIMYW AITGF AJBLW AJDOV AJGSW AJRNO AKQUC ALMA_UNASSIGNED_HOLDINGS ALWAN AMKLP AMTXH AMXSW AMYLF AMYQR AOCGG ARMRJ ASPBG AVWKF AXYYD AYJHY AZFZN B-. BA0 BBWZM BDATZ BENPR BGLVJ BGNMA C1A CAG CCPQU COF CS3 CSCUP DDRTE DNIVK DPUIP DU5 E3Z EAD EAP EBLON EBS EIOEI EJD ESBYG ESX FEDTE FERAY FFXSO FIGPU FINBP FNLPD FRRFC FSGXE FWDCC G-Y G-Z GGCAI GGRSB GJIRD GNWQR GQ6 GQ7 GROUPED_DOAJ HCIFZ HF~ HG5 HG6 HH5 HMJXF HRMNR HVGLF HZ~ I-F IJ- IKXTQ IWAJR IXC IXD IXE I~X I~Z J-C J0Z JBSCW JZLTJ KB. KDC KOV KQ8 LLZTM M4Y MA- MK~ M~E N2Q NDZJH NF0 NPVJJ NQJWS NU0 O9- O93 O9G O9I O9J OK1 P19 P2P P9N PDBOC PF0 PT4 PT5 Q2X QOK QOR QOS R4E R89 R9I RAB RHV RNI RNS ROL RPX RSV RZK S16 S1Z S26 S27 S28 S3B SAP SC5 SCG SCLPG SCM SDH SDM SHX SISQX SNE SNPRN SNX SOHCF SOJ SPISZ SQXTU SRMVM SSLCW STPWE SZN T13 T16 TR2 TSG TSK TSV TUC TUS U2A UG4 UNUBA UOJIU UTJUX UZXMN VC2 VFIZW W48 W4F WK8 XSB YLTOR Z45 Z5O Z7R Z7S Z7V Z7W Z7X Z7Y Z7Z Z83 Z85 Z86 Z88 Z8M Z8N Z8P Z8Q Z8R Z8T Z8W Z8Z Z92 ZMTXR ~8M ~A9 ~EX AACDK AAEOY AAJBT AASML AAYXX ABAKF ACAOD ACDTI ACZOJ AEFQL AEMSY AFBBN AGJZZ AGQEE AGRTI AIGIU CITATION H13 SJYHP 7SR 8BQ 8FD 8FE 8FG D1I DWQXO JG9 PQEST PQQKQ PQUKI |
ID | FETCH-LOGICAL-c359t-ba7332444db004065bf6b18081efe6c17462bd0c8f71f723818df62133183efb3 |
IEDL.DBID | U2A |
ISSN | 0250-4707 |
IngestDate | Thu Oct 10 22:02:34 EDT 2024 Thu Sep 12 17:44:28 EDT 2024 Sat Dec 16 12:03:20 EST 2023 |
IsDoiOpenAccess | false |
IsOpenAccess | true |
IsPeerReviewed | true |
IsScholarly | true |
Issue | 1 |
Keywords | Carbon nanotubes X-ray diffraction electron microscopy graphitization |
Language | English |
LinkModel | DirectLink |
MergedId | FETCHMERGED-LOGICAL-c359t-ba7332444db004065bf6b18081efe6c17462bd0c8f71f723818df62133183efb3 |
OpenAccessLink | https://www.ias.ac.in/article/fulltext/boms/039/01/0041-0046 |
PQID | 2919717656 |
PQPubID | 326358 |
PageCount | 6 |
ParticipantIDs | proquest_journals_2919717656 crossref_primary_10_1007_s12034_015_0891_2 springer_journals_10_1007_s12034_015_0891_2 |
PublicationCentury | 2000 |
PublicationDate | 2016-02-01 |
PublicationDateYYYYMMDD | 2016-02-01 |
PublicationDate_xml | – month: 02 year: 2016 text: 2016-02-01 day: 01 |
PublicationDecade | 2010 |
PublicationPlace | Bangalore, India |
PublicationPlace_xml | – name: Bangalore, India – name: Bangalore |
PublicationSubtitle | Published by the Indian Academy of Sciences |
PublicationTitle | Bulletin of materials science |
PublicationTitleAbbrev | Bull Mater Sci |
PublicationYear | 2016 |
Publisher | Indian Academy of Sciences Springer Nature B.V |
Publisher_xml | – name: Indian Academy of Sciences – name: Springer Nature B.V |
References | KatayamaTArakiHYoshinoKJ. Appl. Phys.200291667510.1063/1.1468892 ZhangHSunCHLiFLiHXChengHMJ. Phys. Chem. B2006110947710.1021/jp060271h KoshioAYudasakaMIjimaSJ. Phys. Chem. C20071111010.1021/jp0672914 PengXHLiuCChengHMCarbon200846200310.1016/j.carbon.2008.09.009 MartinezMTCallejasMABenitoAMCochetMSeegerTAnsonACarbon200341224710.1016/S0008-6223(03)00250-1 KimYAMuramatsuHHayashiTEndoMTerronesMDresselhausMSChem. Phys. Lett.20043988710.1016/j.cplett.2004.09.024 Sato Y, Ogawa T, Motomiya K, Shinoda K, Jeyadevan B and Tohji K 2001 J. Phys. Chem. B105 3387 KimYAHayashiTOsawaKDresselhasuMSEndoMChem. Phys. Lett.200338031910.1016/j.cplett.2003.09.027 MetenierKBonnamySBeguinFJournetCBermierPLamy de la ChapelleMChauvetOLefrantSCarbon200240176510.1016/S0008-6223(02)00044-1 EndoMNishimuraKKimYAHakamadaKMatushitaTDresselhausMSDresselhausGJ. Mater. Res.199914447410.1557/JMR.1999.0607 YadusakaMIchihashiTKasuyaDKaturaHIjimaSCarbon200341127310.1016/S0008-6223(03)00076-9 Endo M, Saito R, Dresselhaus M S and Dresselhaus G 1997 Carbon nanotubes: preparation and properties Ebbesen T W (ed) (USA: CRC Press) p 35 XingYLiLChusueiCHullRVLangmuir200521418510.1021/la047268e WangYWuJWeiFCarbon200341293910.1016/S0008-6223(03)00390-7 HuangWWangYLuoGWeiFCarbon200341258510.1016/S0008-6223(03)00330-0 AndrewsRJacquesDQianDDickyECCarbon200139168110.1016/S0008-6223(00)00301-8 W Huang (891_CR7) 2003; 41 Y Wang (891_CR10) 2003; 41 891_CR5 YA Kim (891_CR13) 2003; 380 M Endo (891_CR16) 1999; 14 891_CR1 MT Martinez (891_CR3) 2003; 41 A Koshio (891_CR11) 2007; 111 R Andrews (891_CR8) 2001; 39 M Yadusaka (891_CR12) 2003; 41 T Katayama (891_CR6) 2002; 91 H Zhang (891_CR9) 2006; 110 Y Xing (891_CR4) 2005; 21 K Metenier (891_CR15) 2002; 40 YA Kim (891_CR14) 2004; 398 XH Peng (891_CR2) 2008; 46 |
References_xml | – volume: 380 start-page: 319 year: 2003 ident: 891_CR13 publication-title: Chem. Phys. Lett. doi: 10.1016/j.cplett.2003.09.027 contributor: fullname: YA Kim – volume: 40 start-page: 1765 year: 2002 ident: 891_CR15 publication-title: Carbon doi: 10.1016/S0008-6223(02)00044-1 contributor: fullname: K Metenier – volume: 398 start-page: 87 year: 2004 ident: 891_CR14 publication-title: Chem. Phys. Lett. doi: 10.1016/j.cplett.2004.09.024 contributor: fullname: YA Kim – ident: 891_CR1 – volume: 110 start-page: 9477 year: 2006 ident: 891_CR9 publication-title: J. Phys. Chem. B doi: 10.1021/jp060271h contributor: fullname: H Zhang – ident: 891_CR5 doi: 10.1021/jp002817k – volume: 21 start-page: 4185 year: 2005 ident: 891_CR4 publication-title: Langmuir doi: 10.1021/la047268e contributor: fullname: Y Xing – volume: 91 start-page: 6675 year: 2002 ident: 891_CR6 publication-title: J. Appl. Phys. doi: 10.1063/1.1468892 contributor: fullname: T Katayama – volume: 111 start-page: 10 year: 2007 ident: 891_CR11 publication-title: J. Phys. Chem. C doi: 10.1021/jp0672914 contributor: fullname: A Koshio – volume: 46 start-page: 2003 year: 2008 ident: 891_CR2 publication-title: Carbon doi: 10.1016/j.carbon.2008.09.009 contributor: fullname: XH Peng – volume: 41 start-page: 2939 year: 2003 ident: 891_CR10 publication-title: Carbon doi: 10.1016/S0008-6223(03)00390-7 contributor: fullname: Y Wang – volume: 14 start-page: 4474 year: 1999 ident: 891_CR16 publication-title: J. Mater. Res. doi: 10.1557/JMR.1999.0607 contributor: fullname: M Endo – volume: 41 start-page: 2585 year: 2003 ident: 891_CR7 publication-title: Carbon doi: 10.1016/S0008-6223(03)00330-0 contributor: fullname: W Huang – volume: 39 start-page: 1681 year: 2001 ident: 891_CR8 publication-title: Carbon doi: 10.1016/S0008-6223(00)00301-8 contributor: fullname: R Andrews – volume: 41 start-page: 2247 year: 2003 ident: 891_CR3 publication-title: Carbon doi: 10.1016/S0008-6223(03)00250-1 contributor: fullname: MT Martinez – volume: 41 start-page: 1273 year: 2003 ident: 891_CR12 publication-title: Carbon doi: 10.1016/S0008-6223(03)00076-9 contributor: fullname: M Yadusaka |
SSID | ssj0019441 |
Score | 2.2145648 |
Snippet | The effect of high-temperature heat treatment on purity and structural changes of multiwalled carbon nanotubes (MWCNTs) were studied by subjecting the raw... |
SourceID | proquest crossref springer |
SourceType | Aggregation Database Publisher |
StartPage | 41 |
SubjectTerms | Acids Carbon Chemistry and Materials Science Decomposition Degradation Electron microscopy Engineering Heat treating Heat treatment High temperature Impurities Materials Science Methods Multi wall carbon nanotubes Purity Raman spectroscopy Scanning electron microscopy Thermogravimetric analysis |
SummonAdditionalLinks | – databaseName: ProQuest Central dbid: BENPR link: http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1LS8NAEB60vehBfGK1yh48KYvJZjePk6i0FKFFpMVeJGRfN9NK6_93Ntk0KijkFjKHbzM73-zMfgNwxZLAJDJybRWKU56GlmIYKdDjObJZXRhrXaI4nsSjGX-ai7k_cFv5tspmT6w2ar1Q7oz8lmVhhqkH0o-75Qd1U6NcddWP0NiGLsNMgXWg-zCYPL9s6ggZr2ZXukBPeRIkTV2zujzHgsh1YAgapFlI2c_I1NLNXxXSKvAM92HPM0ZyXy_xAWyZ8hB2v-kIHsFbrUFMFpY4-WHq9Ka8WDJxmy3ZtJMT_VkvOcEHuR9ZVtPrSFFq8u5682o9WfchGhu_Pk6mq2OYDQfTxxH1cxOoikS2prJIIuRJnOvKR2MhbSxDN2LDWBMrzEFiJnWgUpuENqlitrYxw2wV_dtYGZ1Ap1yU5hRIqpVQGMJDUSieZnGRSqu0KNCMMIUMenDdYJYva3mMvBVCdgDnCHDuAM5ZD_oNqrn3lFXermsPbhqk29d_Gjv739g57CC18f3VfeggeOYC6cNaXvp_5AvVQsF7 priority: 102 providerName: ProQuest |
Title | Effect of high-temperature heat treatment duration on the purity and microstructure of MWCNTs |
URI | https://link.springer.com/article/10.1007/s12034-015-0891-2 https://www.proquest.com/docview/2919717656 |
Volume | 39 |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwlV1LS8NAEB5qe9GD-MRqLXvwpKwkm83rWEsfWFpUWqwHCbub3YuYFlr_v7N5tCp6EAKBPObwJbPzTWbyDcAVCx0dSs-2VShOeeQaimFEoMdzZLOp0MbYRHE8CYYzfj_35zVgm08X2dttVZHMF-rtv27M8WzDhE-dKHYpLrsN5A7ctnHNWGdTOYh5Pq3ShnbKQyesKpm_mfgei7YE80dNNA81_QPYLzki6RQP9RBqOjuCvS_KgcfwWqgOk4UhVnCYWoWpUh6Z2OWVbBrISfpRPGSCG7I9sszn1RGRpeTdduMVCrL2RjQ2fu5OpqsTmPV70-6QlpMSqPL8eE2lCD1kRpynuVcGvjSBdO1QDW10oDDrCJhMHRWZ0DVhHqVTEzDMT9GjtZHeKdSzRabPgESp8hUGbdcXikdxICJpVOoLNONrIZ0mXFeYJctCECPZSh9bgBMEOLEAJ6wJrQrVpPSNVcJiN8YkEolkE24qpLen_zR2_q-rL2AXuU3ZYN2COmKpL5E_rGUbdqL-oA2NzuBl1MP9XW_y8IRHR49RO3-ZPgFcw8Eb |
link.rule.ids | 315,783,787,12779,21402,27938,27939,33387,33758,41095,41537,42164,42606,43614,43819,52125,52248,74371,74638 |
linkProvider | Springer Nature |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV07T8MwELagDMCAeIpCAQ9MIIs87DwmhBClQNupFV2Q5edGW9Ty_zk7TgNIIGWLcsM55-873_k7hC6TPDK5TF1bhaKEFrElACMCIp4Cm9XCWOsSxcEw643p84RNwoHbIrRV1nui36j1TLkz8pukjEtIPYB-3M4_iJsa5aqrYYTGOtqgKQCNuynefVxVEUrqJ1c6mCc0j_K6qumvziVR6vovGImKMibJT1xqyOav-qiHne4u2gl8Ed9VC7yH1sx0H21_UxE8QG-VAjGeWezEh4lTmwpSydhttXjVTI71Z7XgGB5gfnjuZ9dhMdX43XXmVWqy7kMwNni9H44Wh2jcfRjd90iYmkBUysolkSJPgSVRqn2EZkzaTMZuwIaxJlOQgWSJ1JEqbB7b3CO2tlkCuSpEt7EyPUKt6WxqjhEutGIKADxmQtGizEQhrdJMgBlmhIza6Kr2GZ9X4hi8kUF2DubgYO4czJM26tRe5SFOFrxZ1Ta6rj3dvP7T2Mn_xi7QZm806PP-0_DlFG0ByQmd1h3UAkeaMyASS3nu_5Yvv9LDBg |
linkToPdf | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfV1LS8NAEB60BdGD-MRq1T14UpbmsXmdxEdLfTQUabEXCdnXzbbS-v-dTTaNCgq5hcxhdmfnm8y33wBceJGjIu4bWoVglMWupphGcox4hmhW5kprUygO0rA_Zo-TYGL5TwtLq6zOxOKgljNh_pF3vMRNsPRA-NHRlhYxvO9dzz-omSBlOq12nMY6NCOGu6oBzdtuOnxZ9RQSVsyxNEmfssiJqh5ncZHOc3zDxgioEycu9X5mqRp6_uqWFkmotwPbFj2Sm3K5d2FNTfdg65um4D68lXrEZKaJkSKmRnvKCicTc_CSFbWcyM9y-Qk-iAPJvJhkR_KpJO-Gp1dqy5oP0djg9S4dLQ5g3OuO7vrUzlCgwg-SJeV55CNmYkwW8RoGXIfcNeM2lFahwHok9Lh0RKwjV0dF_pY69LByxVhXmvuH0JjOpuoISCxFIDCdu0EuWJyEecy1kEGOZgKVc6cFl5XPsnkplZHVosjGwRk6ODMOzrwWtCuvZjZqFlm9xi24qjxdv_7T2PH_xs5hA7dK9vyQPp3AJiIeS7tuQwP9qE4RVSz5md0uX1uuyKk |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=Effect+of+high-temperature+heat+treatment+duration+on+the+purity+and+microstructure+of+MWCNTs&rft.jtitle=Bulletin+of+materials+science&rft.au=SRIKANTH%2C+I&rft.au=PADMAVATHI%2C+N&rft.au=PRASAD%2C+P+S+R&rft.au=GHOSAL%2C+P&rft.date=2016-02-01&rft.issn=0250-4707&rft.eissn=0973-7669&rft.volume=39&rft.issue=1&rft.spage=41&rft.epage=46&rft_id=info:doi/10.1007%2Fs12034-015-0891-2&rft.externalDBID=n%2Fa&rft.externalDocID=10_1007_s12034_015_0891_2 |
thumbnail_l | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=0250-4707&client=summon |
thumbnail_m | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=0250-4707&client=summon |
thumbnail_s | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=0250-4707&client=summon |