Chemistry directs the conservation of paper cultural relics

•Chemical principles are used to direct the preservation and conservation of paper cultural relics.•The mechanisms of acidic, alkaline and oxidative degradation of cellulose, hemicellulose and lignin in paper are summarized.•The intrinsic and extrinsic factors affecting the degradation process of pa...

Full description

Saved in:
Bibliographic Details
Published inPolymer degradation and stability Vol. 207; p. 110228
Main Authors Zhang, Xu, Yan, Yueer, Yao, Jingjing, Jin, Shutong, Tang, Yi
Format Journal Article
LanguageEnglish
Published Elsevier Ltd 01.01.2023
Subjects
Online AccessGet full text

Cover

Loading…
Abstract •Chemical principles are used to direct the preservation and conservation of paper cultural relics.•The mechanisms of acidic, alkaline and oxidative degradation of cellulose, hemicellulose and lignin in paper are summarized.•The intrinsic and extrinsic factors affecting the degradation process of paper are addressed.•The advantages and disadvantages of remedial and preventive conservation methods for paper relics are discussed. Paper cultural relics, with the great historic and artistic value, experience aging and degradation during their long-term preservation. The degradation of paper involves various chemical reactions with complicated mechanisms due to the multiple components of paper itself and the complex factors that promote paper aging process. Therefore, it is of great importance to deeply understand the chemical essence and scientific principle of paper degradation, so as to propose the effective conservation methods for paper relics. This review summarized the chemical mechanisms of acidic, alkaline and oxidative degradation of cellulose, hemicellulose and lignin in paper, and discussed the intrinsic and extrinsic factors that affect paper degradation systematically. Moreover, the interaction among the three types of degradation routes was analyzed for the first time, and the evolution of kinetic models for paper degradation was introduced to evaluate the durability and expected lifetime of paper. On this basis, the advantages and disadvantages of remedial and preventive conservation methods for paper relics are summarized, and the fundamental scientific principles was prospected to guide the further development of paper conservation methods.
AbstractList •Chemical principles are used to direct the preservation and conservation of paper cultural relics.•The mechanisms of acidic, alkaline and oxidative degradation of cellulose, hemicellulose and lignin in paper are summarized.•The intrinsic and extrinsic factors affecting the degradation process of paper are addressed.•The advantages and disadvantages of remedial and preventive conservation methods for paper relics are discussed. Paper cultural relics, with the great historic and artistic value, experience aging and degradation during their long-term preservation. The degradation of paper involves various chemical reactions with complicated mechanisms due to the multiple components of paper itself and the complex factors that promote paper aging process. Therefore, it is of great importance to deeply understand the chemical essence and scientific principle of paper degradation, so as to propose the effective conservation methods for paper relics. This review summarized the chemical mechanisms of acidic, alkaline and oxidative degradation of cellulose, hemicellulose and lignin in paper, and discussed the intrinsic and extrinsic factors that affect paper degradation systematically. Moreover, the interaction among the three types of degradation routes was analyzed for the first time, and the evolution of kinetic models for paper degradation was introduced to evaluate the durability and expected lifetime of paper. On this basis, the advantages and disadvantages of remedial and preventive conservation methods for paper relics are summarized, and the fundamental scientific principles was prospected to guide the further development of paper conservation methods.
ArticleNumber 110228
Author Yao, Jingjing
Jin, Shutong
Yan, Yueer
Tang, Yi
Zhang, Xu
Author_xml – sequence: 1
  givenname: Xu
  surname: Zhang
  fullname: Zhang, Xu
  organization: Institute for Preservation and Conservation of Chinese Ancient Books, Fudan University Library, Fudan University, Shanghai 200433, China
– sequence: 2
  givenname: Yueer
  surname: Yan
  fullname: Yan, Yueer
  email: yueeryan@fudan.edu.cn
  organization: Institute for Preservation and Conservation of Chinese Ancient Books, Fudan University Library, Fudan University, Shanghai 200433, China
– sequence: 3
  givenname: Jingjing
  surname: Yao
  fullname: Yao, Jingjing
  organization: Shanghai Institute of Quality Inspection and Technical Research, Shanghai 201114, China
– sequence: 4
  givenname: Shutong
  surname: Jin
  fullname: Jin, Shutong
  organization: Department of Chemistry, Fudan University, Shanghai 200438, China
– sequence: 5
  givenname: Yi
  surname: Tang
  fullname: Tang, Yi
  email: yitang@fudan.edu.cn
  organization: Department of Chemistry, Fudan University, Shanghai 200438, China
BookMark eNqNkEFLwzAUx4NMcJt-h1w8tuYlre0QD1J0CgMveg6vSeoyuqYk2aDf3s562mmPx3un_w_-vwWZda4zhNwDS4HB48Mu7V077LX58ahDxDrljPMUYLzlFZlDWYiECw4zMmeQQSJWwG7IIoQdGyfLYU6eqq3Z2xD9QLX1RsVA49ZQ5bpg_BGjdR11De2xN56qQxsPHlvqTWtVuCXXDbbB3P3_Jfl-e_2q3pPN5_qjetkkSggRE1R1g1lRFDqHrCixqBEQodErVrIcRZ2vuNaFysZSNWR5rVDwXDdM47gcxJI8T1zlXQjeNLL3do9-kMDkyYTcyTMT8mRCTibGfHWWVzb-VYsebXsxZT1RzFj1aI2XQVnTKTN5k9rZC0m_nXaLMA
CitedBy_id crossref_primary_10_3390_molecules30020417
crossref_primary_10_59116_lamre_1394494
crossref_primary_10_1038_s41598_024_57228_2
crossref_primary_10_3390_coatings14070851
crossref_primary_10_3390_ma17163900
crossref_primary_10_1021_acsami_4c09598
crossref_primary_10_3390_polym16091227
crossref_primary_10_1186_s40494_023_01083_3
crossref_primary_10_1016_j_ijadhadh_2024_103685
crossref_primary_10_1002_cplu_202400170
crossref_primary_10_3390_molecules29235741
crossref_primary_10_1016_j_polymdegradstab_2023_110330
crossref_primary_10_1186_s40494_024_01137_0
crossref_primary_10_1016_j_eurpolymj_2024_113590
crossref_primary_10_3390_molecules29163959
crossref_primary_10_1021_acsami_3c19050
crossref_primary_10_1016_j_snb_2024_137119
crossref_primary_10_1016_j_jece_2024_113195
crossref_primary_10_1002_adfm_202401067
crossref_primary_10_1016_j_polymdegradstab_2024_110953
crossref_primary_10_1038_s40494_025_01601_5
crossref_primary_10_3390_ijms252413541
crossref_primary_10_1515_npprj_2023_0085
crossref_primary_10_1016_j_ijbiomac_2025_141986
crossref_primary_10_1016_j_buildenv_2024_112343
Cites_doi 10.1070/RC1973v042n04ABEH002585
10.1007/s10570-008-9259-8
10.1007/s10570-013-9978-3
10.1016/S0010-8545(02)00034-6
10.1016/j.ibiod.2008.01.005
10.1186/s40494-019-0294-6
10.1016/j.scitotenv.2021.148204
10.1177/004051754901900901
10.1016/j.culher.2013.10.008
10.1016/0032-3950(64)90285-0
10.1007/s10570-022-04681-9
10.1139/v05-168
10.1016/j.apcatb.2015.11.039
10.15376/biores.10.4.6305-6309
10.1016/j.polymdegradstab.2005.01.003
10.1007/s10570-015-0699-7
10.1039/jr9570004500
10.1007/s00339-010-5657-5
10.1016/j.ibiod.2008.07.011
10.1002/ente.201600667
10.1016/j.ibiod.2006.02.003
10.1016/S1010-6030(03)00007-8
10.1002/cssc.200800111
10.1016/S0964-8305(02)00137-3
10.1080/03094227.1979.9638520
10.1016/j.polymdegradstab.2013.12.003
10.15376/biores.5.3.1955-2023
10.1179/2047058414Y.0000000158
10.1038/s41598-020-77101-2
10.1016/j.polymdegradstab.2010.12.017
10.1007/s10570-018-1682-x
10.1021/acssuschemeng.8b00486
10.1038/srep27813
10.1007/s10570-019-02375-3
10.1016/j.culher.2003.07.003
10.1016/j.carbpol.2013.10.033
10.1023/A:1024267704794
10.1016/j.jcis.2022.01.123
10.1002/elsc.201800039
10.1007/BF02228806
10.1021/la025964d
10.1007/s10570-005-2206-z
10.1016/j.jcis.2019.03.089
10.1021/ja00021a021
10.1179/019713607806112378
10.1016/S0964-8305(01)00071-3
10.1016/j.chroma.2003.11.069
10.1002/bbb.1517
10.1016/S0964-8305(00)00063-9
10.1186/s40494-016-0071-8
10.1016/j.bbrc.2016.12.174
10.1021/ja00096a012
10.1016/j.scitotenv.2019.03.180
10.1016/j.polymdegradstab.2006.04.033
10.1016/j.culher.2021.01.014
10.1039/cs9962500179
10.1016/j.polymdegradstab.2013.12.028
10.1007/s10570-007-9114-3
10.1016/j.fuel.2009.10.022
10.1016/j.apsusc.2005.02.045
10.1016/j.polymdegradstab.2010.09.002
10.1016/j.polymdegradstab.2007.05.006
10.1007/s10570-017-1450-3
10.2307/3178991
10.1039/C4GC02151G
10.1007/s00339-004-2540-2
10.1016/S0584-8547(02)00056-3
10.1038/s41565-021-00934-z
10.15376/biores.12.2.Hubbe
10.1016/j.culher.2007.12.002
10.1021/la050564m
10.1016/j.carbpol.2020.116534
10.1002/chem.202100675
10.1016/j.cej.2010.10.018
10.1007/BF00818797
10.1016/j.polymdegradstab.2013.05.017
10.1007/s10570-012-9723-3
10.1177/004051754901901003
10.1016/j.ibiod.2018.03.005
10.1021/acssuschemeng.9b06028
10.1093/glycob/cwq171
10.1039/C5RA25954A
10.1016/0141-3910(94)90011-6
10.1016/S1872-2067(20)63569-0
10.1038/274466a0
10.1002/app.1979.070230513
10.1155/2017/8951658
10.3390/polym13071029
10.1021/acssuschemeng.5b00070
10.1021/j100318a039
10.1007/s10570-018-2200-x
10.1021/jp310008z
10.1080/02773819508009510
10.1016/S1010-6030(97)00118-4
10.1080/19447023208661546
10.15376/biores.6.4.5307-5337
10.1016/j.polymdegradstab.2013.12.019
10.1007/BF02228805
10.1007/s10570-016-1112-x
10.1086/613729
ContentType Journal Article
Copyright 2022 Elsevier Ltd
Copyright_xml – notice: 2022 Elsevier Ltd
DBID AAYXX
CITATION
DOI 10.1016/j.polymdegradstab.2022.110228
DatabaseName CrossRef
DatabaseTitle CrossRef
DatabaseTitleList
DeliveryMethod fulltext_linktorsrc
Discipline Engineering
Chemistry
EISSN 1873-2321
ExternalDocumentID 10_1016_j_polymdegradstab_2022_110228
S0141391022004062
GroupedDBID --K
--M
-~X
.~1
0R~
123
1B1
1~.
1~5
29O
4.4
457
4G.
53G
5VS
7-5
71M
8P~
9JN
AABNK
AABXZ
AACTN
AAEDT
AAEDW
AAEPC
AAIAV
AAIKJ
AAKOC
AALRI
AAOAW
AAQFI
AAQXK
AARLI
AAXUO
ABFNM
ABJNI
ABMAC
ABXDB
ABXRA
ABYKQ
ACDAQ
ACGFS
ACIWK
ACNNM
ACRLP
ADBBV
ADECG
ADEZE
ADMUD
AEBSH
AEKER
AENEX
AEZYN
AFKWA
AFRZQ
AFTJW
AFZHZ
AGHFR
AGUBO
AGYEJ
AHHHB
AIEXJ
AIKHN
AITUG
AJBFU
AJOXV
AJSZI
ALMA_UNASSIGNED_HOLDINGS
AMFUW
AMRAJ
ASPBG
AVWKF
AXJTR
AZFZN
BKOJK
BLXMC
CS3
DU5
EBS
EFJIC
EFLBG
EJD
EO8
EO9
EP2
EP3
F5P
FDB
FEDTE
FGOYB
FIRID
FLBIZ
FNPLU
FYGXN
G-2
G-Q
GBLVA
HVGLF
HZ~
IHE
J1W
KOM
M24
M41
MAGPM
MO0
N9A
O-L
O9-
OAUVE
OZT
P-8
P-9
P2P
PC.
Q38
R2-
RIG
RNS
ROL
RPZ
SCB
SDF
SDG
SDP
SES
SEW
SMS
SPC
SPCBC
SSK
SSM
SSZ
T5K
WH7
WUQ
XPP
~G-
AAHBH
AATTM
AAXKI
AAYWO
AAYXX
ABWVN
ACRPL
ACVFH
ADCNI
ADNMO
AEIPS
AEUPX
AFJKZ
AFPUW
AFXIZ
AGCQF
AGQPQ
AGRNS
AIGII
AIIUN
AKBMS
AKRWK
AKYEP
ANKPU
APXCP
BNPGV
CITATION
SSH
ID FETCH-LOGICAL-c333t-acbfa4777d51478a7ba1aa1fd90805a3b592dd7c4101b145bca325df0da0da213
IEDL.DBID .~1
ISSN 0141-3910
IngestDate Thu Apr 24 22:53:45 EDT 2025
Tue Jul 01 02:29:54 EDT 2025
Fri Feb 23 02:40:20 EST 2024
IsPeerReviewed true
IsScholarly true
Keywords Degradation
Paper cultural relics
Cellulose chemistry
Conservation
Language English
LinkModel DirectLink
MergedId FETCHMERGED-LOGICAL-c333t-acbfa4777d51478a7ba1aa1fd90805a3b592dd7c4101b145bca325df0da0da213
ParticipantIDs crossref_primary_10_1016_j_polymdegradstab_2022_110228
crossref_citationtrail_10_1016_j_polymdegradstab_2022_110228
elsevier_sciencedirect_doi_10_1016_j_polymdegradstab_2022_110228
ProviderPackageCode CITATION
AAYXX
PublicationCentury 2000
PublicationDate January 2023
2023-01-00
PublicationDateYYYYMMDD 2023-01-01
PublicationDate_xml – month: 01
  year: 2023
  text: January 2023
PublicationDecade 2020
PublicationTitle Polymer degradation and stability
PublicationYear 2023
Publisher Elsevier Ltd
Publisher_xml – name: Elsevier Ltd
References Zotti, Ferroni, Calvini (bib0088) 2008; 62
Calvini (bib0100) 2005; 12
Liers, Schwerdt (bib0119) 1995; 16
Heitner, Dimmel, Schmidt (bib0048) 2016
Fan, Gharpuray, Lee (bib0014) 2012
Dufour, Havermans (bib0069) 2001; 22
Choi (bib0085) 2007; 46
Lu, Lu, Hu, Xie, Wei, Fan (bib0049) 2017; 2017
Zuliani, Bandelli, Chelazzi, Giorgi, Baglioni (bib0154) 2022; 614
Begin, Deschatelets, Grattan, Gurnagul, Iraci, Kaminska, Woods, Zou (bib0022) 1999; 20
Ipert, Rousset, Cheradame (bib0122) 2005; 26
Zervos (bib0073) 2010
Zervos, Alexopoulou (bib0095) 2015; 22
Ahn, Henniges, Blüher, Banik, Potthast (bib0041) 2011; 32
Malesic, Marinsek, Cigic (bib0120) 2022; 29
Dupont, Lavedrine, Cheradame (bib0123) 2010; 95
Zhou, Yang, Xu, Shi, Wang, Chen, Xu (bib0065) 2015; 17
Valentin (bib0156) 1986; 10
Havermans, Vandeventer, Steemers (bib0113) 1995; 16
Kapu, Trajano (bib0019) 2014; 8
French (bib0004) 2017; 24
Hubbe, Smith, Zou, Katuscak, Potthast, Ahn (bib0110) 2017; 12
Lienardy, Damme (bib0140) 1990; 11
Machell, Richards (bib0039) 1957
Arnold (bib0074) 1998
Felı́cio, Machado, Castellan, Nourmamode, Perez, Ruggiero (bib0051) 2003; 156
Graminski, Parks, Toth (bib0033) 1976
Nair, Dhar, Vinu (bib0052) 2016; 6
Bégin, Deschatelets, Grattan, Gurnagul, Iraci, Kaminska, Woods, Zou (bib0076) 1998; 19
Magaudda (bib0159) 2004; 5
Williams (bib0130) 1971; 12
Malešič, Kadivec, Kunaver, Skalar, Cigić (bib0135) 2019; 7
Kelly Jr, Tang, Krasnow (bib0129) 1977
Shahani, Lee, Hengemihle (bib0104) 2001
Graminski, Parks, Toth (bib0034) 1978; 2
Kolar, Novak (bib0127) 1996; 17
Pavasars, Hagberg, Boren, Allard (bib0040) 2003; 11
Ipert, Dupont, Lavedrine, Begin, Rousset, Cheradame (bib0112) 2006; 91
Maitland (bib0147) 2009; 28
Yamamoto, Koga, Nagaoka (bib0061) 2012; 116
Zou, Gurnagul (bib0077) 1995; 15
Giorgi, Bozzi, Dei, Gabbiani, Ninham, Baglioni (bib0134) 2005; 21
Meynell, Newsam (bib0083) 1978; 274
Šelih, Strlič, Kolar, Pihlar (bib0058) 2007; 92
Afsharpour, Hadadi (bib0151) 2014; 15
Golova, Nosova (bib0063) 1973; 42
Baty, Sinnott (bib0021) 2005; 83
Davidson (bib0067) 1932; 23
Cunha (bib0114) 1987
Bukovsky (bib0075) 2000; 21
Calvo, Alfaro, Miranda, Felissia, Area (bib0158) 2010
Ekenstam (bib0097) 1936; 69
Arai (bib0091) 2000; 46
Corte, Ferroni, Salvo (bib0086) 2003; 51
Vinu, Polisetti, Madras (bib0053) 2010; 165
Vellingiri, Szulejko, Kumar, Kwon, Kim, Deep, Boukhvalov, Brown (bib0153) 2016; 6
Jablonsky, Sima (bib0009) 2021; 48
Potthast, Ahn (bib0115) 2016; 24
Curran, Mozir, Underhill, Gibson, Fearn, Strlič (bib0027) 2014; 107
Couturier, Berrin (bib0081) 2013
Kolar, Mozir, Balazic, Strlič, Ceres, Conte, Mirruzzo, Steemers, de Bruin (bib0146) 2008; 29
Press (bib0092) 2001; 48
Hey (bib0131) 1979; 4
Malachowska, Pawcenis, Danczak, Paczkowska, Przybysz (bib0036) 2021; 13
Area, Cheradame (bib0010) 2011; 6
Bicchieri, Pappalardo, Romano, Sementilli, De Acutis (bib0093) 2001; 22
LiÉNardy (bib0116) 1994; 15
Kolar, Mozir, Strlič, de Bruin, Pihlar, Steemers (bib0143) 2007; 4
Bicchieri, Ronconi, Romano, Pappalardo, Corsi, Cristoforetti, Legnaioli, Palleschi, Salvetti, Tognoni (bib0090) 2002; 57
Daniels (bib0002) 1996; 25
Chelazzi, Chevalier, Pizzorusso, Giorgi, Menu, Baglioni (bib0028) 2014; 107
Zervos, Moropoulou (bib0007) 2006; 27
Ahn, Zaccaron, Zwirchmayr, Hettegger, Hofinger, Bacher, Henniges, Hosoya, Potthast, Rosenau (bib0071) 2019; 26
Sjostrom (bib0038) 1993
Cunha (bib0133) 1989; 25
Duan, Kasper (bib0059) 2011; 21
Lee, Feller (bib0098) 1986
Duplooy (bib0037) 1981; 34
Szulc, Otlewska, Ruman, Kubiak, Karbowska-Berent, Kozielec, Gutarowska (bib0087) 2018; 132
Lattuati-Derieux, Bonnassies-Termes, Lavedrine (bib0101) 2004; 1026
Conte, Pulci, Knapik, Bagniuk, Del Sole, Lojewska, Missori (bib0070) 2012; 108
Entwistle, Cole, Wooding (bib0068) 1949; 19
Rakotonirainy, Dupont, Lavedrine, Ipert, Cheradame (bib0126) 2008; 9
Buzio, Calvini, Ferroni, Valbusa (bib0084) 2004; 79
Bredereck, Haberditzl, BlÜHer (bib0128) 1990; 11
Bors, Michel, Saran (bib0046) 1981; 17
Kotsidi, Gorgolis, Carbone, Anagnostopoulos, Paterakis, Poggi, Manikas, Trakakis, Baglioni, Galiotis (bib0152) 2021; 16
Negahdar, Delidovich, Palkovits (bib0018) 2016; 184
Eronen, Österberg, Jääskeläinen (bib0043) 2008; 16
Jablonsky, Šima, Lelovsky (bib0020) 2020; 245
Zhang, Dong, Zhao, Wang, Meng (bib0060) 2019; 670
Rousset, Ipert, Cheradame (bib0121) 2004; 25
Giorgi, Dei, Ceccato, Schettino, Baglioni (bib0132) 2002; 18
Dasilva, Moraes, Nishikawa, Gatti, Vallimdealencar, Brandao, Nobrega (bib0160) 2006; 57
Dence, Reeve (bib0079) 1996
Philipp, Jacopian, Loth, Hirte, Schulz (bib0015) 1979
Mitchell, Higgitt, Gibson (bib0026) 2014; 107
Shafizadeh, Bradbury (bib0099) 1979; 23
Rasch, Scribner (bib0103) 1934
Shi, Zhang, Mao, Wang, Zheng, Zhao (bib0145) 2017; 483
Liu (bib0148) 2022; 3
Baty, Maitland, Minter, Hubbe, Jordan-Mowery (bib0011) 2010; 5
Ahn, Hennniges, Banik, Potthast (bib0042) 2012; 19
Mayat, Nikolayeva, Golova (bib0064) 1964; 6
Batterham, Rai (bib0109) 2008
Hubbe (bib0117) 2015; 10
Zhang, Bommuswamy, Sinnott (bib0013) 1994; 116
Zou, Uesaka, Gurnagul (bib0106) 1996; 3
Neevel (bib0142) 1995; 16
Banik (bib0124) 2005; 26
Zou, Gurnagul, Uesaka, Bouchard (bib0096) 1994; 43
Camerini, Poggi, Chelazzi, Ridi, Giorgi, Baglioni (bib0136) 2019; 547
Ahn, Rosenau, Potthast (bib0045) 2013; 20
Savoldelli, Catto, Villa, Saracchi, Troiano, Cortesi, Cappitelli (bib0082) 2021; 790
Cedzova, Gallova, Katuscak (bib0111) 2006; 27
Łojewski, Zięba, Knapik, Bagniuk, Lubańska, Łojewska (bib0072) 2010; 100
Clapp (bib0138) 1987
Vilcocq, Rebmann, Cheah, Fongarland (bib0047) 2018; 6
DeRosa, Crutchley (bib0050) 2002; 233
Nosaka, Fox (bib0057) 1988; 92
Entwistle, Cole, Wooding (bib0066) 1949; 19
Zhou, Li, Mabon, Broadbelt (bib0005) 2017; 5
Malachowska, Dubowik, Boruszewski, Lojewska, Przybysz (bib0078) 2020; 10
Pelzer, Sturgeon, Yanez, Chupka, O'Brien, Katahira, Cortright, Woods, Beckham, Broadbelt (bib0006) 2015; 3
Baglioni, Chelazzi (bib0001) 2021; 27
Jeong, Bogolitsyna, Jo, Kang, Rosenau, Potthast (bib0107) 2014; 101
Jiang, Weng, Jia, Yang, Zhang (bib0032) 2018; 25
Zou, Uesaka, Gurnagul (bib0105) 1996; 3
Ceres, Conte, Mirruzzo, Kolar, Strlič (bib0144) 2008; 1
Strlič, Cigic, Mozir, de Bruin, Kolar, Cassar (bib0025) 2011; 96
McCormick-Goodhart, Wilhelm (bib0035) 2004; 1
Grau-Bove, Budic, Cigic, Thickett, Signorello, Strlič (bib0030) 2016; 4
(bib0139) 1994
Botti, Mantovani, Orru, Ruggiero (bib0137) 2006; 27
Wen, Yuan, Qu, Wang, Wang (bib0054) 2020; 8
Malešič, Kolar, Strlič, Kočar, Fromageot, Lemaire, Haillant (bib0055) 2005; 89
Cheradame, Ipert, Rousset (bib0125) 2003; 24
Neves, Schafer, Phillips, Canejo, Macedo (bib0157) 2009; 63
Bartl, Maskova, Paulusova, Smolik, Bartlova, Vodicka (bib0029) 2016; 61
Vassilev, Baxter, Andersen, Vassileva (bib0003) 2010; 89
Havermans (bib0023) 1995; 16
Iiams, Beckwith (bib0094) 1935; 5
Ding, Wang (bib0108) 2007; 14
Rebrikova, Manturovskaya (bib0089) 2000; 21
Li, Li, Shen, Zhan (bib0044) 2019; 26
Smith (bib0155) 1986; 10
Dupont, Barthez, Jerosch, Lavedrine (bib0118) 2002; 23
Mills, Le Hunte (bib0056) 1997; 108
Kolar, Strlič, Novak, Pihlar (bib0017) 1998; 24
Emsley, Stevens (bib0008) 1994; 1
Ahn, Banik, Potthast (bib0141) 2012; 33
Tetreault, Dupont, Begin, Paris (bib0024) 2013; 98
Gu, Liu (bib0062) 2020; 41
Calvini, Gorassini, Merlani (bib0102) 2007; 28
Williams (bib0016) 1981; 30
Zhu (bib0150) 2015; 3
Laguardia, Vassallo, Cappitelli, Mesto, Soelini, Bonizzoni (bib0161) 2005; 252
Banait, Jencks (bib0012) 1991; 113
Andlar, Rezic, Mardetko, Kracher, Ludwig, Šantek (bib0080) 2018; 18
Welf, Venditti, Hubbe, Pawlak (bib0031) 2005; 14
Zhang, Zhang, Zhang (bib0149) 2017; 46
Calvini (10.1016/j.polymdegradstab.2022.110228_bib0100) 2005; 12
Ipert (10.1016/j.polymdegradstab.2022.110228_bib0112) 2006; 91
Malachowska (10.1016/j.polymdegradstab.2022.110228_bib0078) 2020; 10
Ekenstam (10.1016/j.polymdegradstab.2022.110228_bib0097) 1936; 69
Machell (10.1016/j.polymdegradstab.2022.110228_bib0039) 1957
Zou (10.1016/j.polymdegradstab.2022.110228_bib0106) 1996; 3
Cedzova (10.1016/j.polymdegradstab.2022.110228_bib0111) 2006; 27
Buzio (10.1016/j.polymdegradstab.2022.110228_bib0084) 2004; 79
Calvo (10.1016/j.polymdegradstab.2022.110228_bib0158) 2010
DeRosa (10.1016/j.polymdegradstab.2022.110228_bib0050) 2002; 233
Malachowska (10.1016/j.polymdegradstab.2022.110228_bib0036) 2021; 13
Graminski (10.1016/j.polymdegradstab.2022.110228_bib0033) 1976
Kolar (10.1016/j.polymdegradstab.2022.110228_bib0143) 2007; 4
Vellingiri (10.1016/j.polymdegradstab.2022.110228_bib0153) 2016; 6
Shi (10.1016/j.polymdegradstab.2022.110228_bib0145) 2017; 483
Zou (10.1016/j.polymdegradstab.2022.110228_bib0077) 1995; 15
Zhou (10.1016/j.polymdegradstab.2022.110228_bib0065) 2015; 17
Curran (10.1016/j.polymdegradstab.2022.110228_bib0027) 2014; 107
Bartl (10.1016/j.polymdegradstab.2022.110228_bib0029) 2016; 61
Kolar (10.1016/j.polymdegradstab.2022.110228_bib0017) 1998; 24
Camerini (10.1016/j.polymdegradstab.2022.110228_bib0136) 2019; 547
Williams (10.1016/j.polymdegradstab.2022.110228_bib0130) 1971; 12
Daniels (10.1016/j.polymdegradstab.2022.110228_bib0002) 1996; 25
Tetreault (10.1016/j.polymdegradstab.2022.110228_bib0024) 2013; 98
Vinu (10.1016/j.polymdegradstab.2022.110228_bib0053) 2010; 165
Dufour (10.1016/j.polymdegradstab.2022.110228_bib0069) 2001; 22
Bredereck (10.1016/j.polymdegradstab.2022.110228_bib0128) 1990; 11
Pelzer (10.1016/j.polymdegradstab.2022.110228_bib0006) 2015; 3
Zou (10.1016/j.polymdegradstab.2022.110228_bib0105) 1996; 3
Bukovsky (10.1016/j.polymdegradstab.2022.110228_bib0075) 2000; 21
Iiams (10.1016/j.polymdegradstab.2022.110228_bib0094) 1935; 5
Dupont (10.1016/j.polymdegradstab.2022.110228_bib0123) 2010; 95
Hubbe (10.1016/j.polymdegradstab.2022.110228_bib0117) 2015; 10
Yamamoto (10.1016/j.polymdegradstab.2022.110228_bib0061) 2012; 116
Calvini (10.1016/j.polymdegradstab.2022.110228_bib0102) 2007; 28
Felı́cio (10.1016/j.polymdegradstab.2022.110228_bib0051) 2003; 156
Wen (10.1016/j.polymdegradstab.2022.110228_bib0054) 2020; 8
Ahn (10.1016/j.polymdegradstab.2022.110228_bib0042) 2012; 19
Havermans (10.1016/j.polymdegradstab.2022.110228_bib0113) 1995; 16
McCormick-Goodhart (10.1016/j.polymdegradstab.2022.110228_bib0035) 2004; 1
Entwistle (10.1016/j.polymdegradstab.2022.110228_bib0066) 1949; 19
Laguardia (10.1016/j.polymdegradstab.2022.110228_bib0161) 2005; 252
Press (10.1016/j.polymdegradstab.2022.110228_bib0092) 2001; 48
Golova (10.1016/j.polymdegradstab.2022.110228_bib0063) 1973; 42
Mitchell (10.1016/j.polymdegradstab.2022.110228_bib0026) 2014; 107
Hubbe (10.1016/j.polymdegradstab.2022.110228_bib0110) 2017; 12
Neevel (10.1016/j.polymdegradstab.2022.110228_bib0142) 1995; 16
Bégin (10.1016/j.polymdegradstab.2022.110228_bib0076) 1998; 19
Conte (10.1016/j.polymdegradstab.2022.110228_bib0070) 2012; 108
Williams (10.1016/j.polymdegradstab.2022.110228_bib0016) 1981; 30
Szulc (10.1016/j.polymdegradstab.2022.110228_bib0087) 2018; 132
Jeong (10.1016/j.polymdegradstab.2022.110228_bib0107) 2014; 101
Banik (10.1016/j.polymdegradstab.2022.110228_bib0124) 2005; 26
Baty (10.1016/j.polymdegradstab.2022.110228_bib0011) 2010; 5
Liu (10.1016/j.polymdegradstab.2022.110228_bib0148) 2022; 3
Batterham (10.1016/j.polymdegradstab.2022.110228_bib0109) 2008
Hey (10.1016/j.polymdegradstab.2022.110228_bib0131) 1979; 4
Vassilev (10.1016/j.polymdegradstab.2022.110228_bib0003) 2010; 89
Emsley (10.1016/j.polymdegradstab.2022.110228_bib0008) 1994; 1
Afsharpour (10.1016/j.polymdegradstab.2022.110228_bib0151) 2014; 15
Li (10.1016/j.polymdegradstab.2022.110228_bib0044) 2019; 26
Šelih (10.1016/j.polymdegradstab.2022.110228_bib0058) 2007; 92
Vilcocq (10.1016/j.polymdegradstab.2022.110228_bib0047) 2018; 6
Davidson (10.1016/j.polymdegradstab.2022.110228_bib0067) 1932; 23
Savoldelli (10.1016/j.polymdegradstab.2022.110228_bib0082) 2021; 790
Ahn (10.1016/j.polymdegradstab.2022.110228_bib0041) 2011; 32
Heitner (10.1016/j.polymdegradstab.2022.110228_bib0048) 2016
Liers (10.1016/j.polymdegradstab.2022.110228_bib0119) 1995; 16
Nosaka (10.1016/j.polymdegradstab.2022.110228_bib0057) 1988; 92
Dence (10.1016/j.polymdegradstab.2022.110228_bib0079) 1996
Mayat (10.1016/j.polymdegradstab.2022.110228_bib0064) 1964; 6
Mills (10.1016/j.polymdegradstab.2022.110228_bib0056) 1997; 108
Chelazzi (10.1016/j.polymdegradstab.2022.110228_bib0028) 2014; 107
Cunha (10.1016/j.polymdegradstab.2022.110228_bib0133) 1989; 25
Malešič (10.1016/j.polymdegradstab.2022.110228_bib0135) 2019; 7
Magaudda (10.1016/j.polymdegradstab.2022.110228_bib0159) 2004; 5
Kolar (10.1016/j.polymdegradstab.2022.110228_bib0127) 1996; 17
Couturier (10.1016/j.polymdegradstab.2022.110228_bib0081) 2013
Fan (10.1016/j.polymdegradstab.2022.110228_bib0014) 2012
Nair (10.1016/j.polymdegradstab.2022.110228_bib0052) 2016; 6
Kelly Jr (10.1016/j.polymdegradstab.2022.110228_bib0129) 1977
Lienardy (10.1016/j.polymdegradstab.2022.110228_bib0140) 1990; 11
Philipp (10.1016/j.polymdegradstab.2022.110228_bib0015) 1979
Choi (10.1016/j.polymdegradstab.2022.110228_bib0085) 2007; 46
Cunha (10.1016/j.polymdegradstab.2022.110228_bib0114) 1987
Zou (10.1016/j.polymdegradstab.2022.110228_bib0096) 1994; 43
Dasilva (10.1016/j.polymdegradstab.2022.110228_bib0160) 2006; 57
Welf (10.1016/j.polymdegradstab.2022.110228_bib0031) 2005; 14
Ahn (10.1016/j.polymdegradstab.2022.110228_bib0045) 2013; 20
Pavasars (10.1016/j.polymdegradstab.2022.110228_bib0040) 2003; 11
Entwistle (10.1016/j.polymdegradstab.2022.110228_bib0068) 1949; 19
Ahn (10.1016/j.polymdegradstab.2022.110228_bib0141) 2012; 33
Kolar (10.1016/j.polymdegradstab.2022.110228_bib0146) 2008; 29
Meynell (10.1016/j.polymdegradstab.2022.110228_bib0083) 1978; 274
Banait (10.1016/j.polymdegradstab.2022.110228_bib0012) 1991; 113
Smith (10.1016/j.polymdegradstab.2022.110228_bib0155) 1986; 10
Area (10.1016/j.polymdegradstab.2022.110228_bib0010) 2011; 6
Baglioni (10.1016/j.polymdegradstab.2022.110228_bib0001) 2021; 27
Arai (10.1016/j.polymdegradstab.2022.110228_bib0091) 2000; 46
Dupont (10.1016/j.polymdegradstab.2022.110228_bib0118) 2002; 23
Bors (10.1016/j.polymdegradstab.2022.110228_bib0046) 1981; 17
Valentin (10.1016/j.polymdegradstab.2022.110228_bib0156) 1986; 10
Begin (10.1016/j.polymdegradstab.2022.110228_bib0022) 1999; 20
Malesic (10.1016/j.polymdegradstab.2022.110228_bib0120) 2022; 29
Potthast (10.1016/j.polymdegradstab.2022.110228_bib0115) 2016; 24
Botti (10.1016/j.polymdegradstab.2022.110228_bib0137) 2006; 27
Zhang (10.1016/j.polymdegradstab.2022.110228_bib0013) 1994; 116
Bicchieri (10.1016/j.polymdegradstab.2022.110228_bib0090) 2002; 57
Bicchieri (10.1016/j.polymdegradstab.2022.110228_bib0093) 2001; 22
Rousset (10.1016/j.polymdegradstab.2022.110228_bib0121) 2004; 25
Maitland (10.1016/j.polymdegradstab.2022.110228_bib0147) 2009; 28
Ipert (10.1016/j.polymdegradstab.2022.110228_bib0122) 2005; 26
Jablonsky (10.1016/j.polymdegradstab.2022.110228_bib0020) 2020; 245
Jablonsky (10.1016/j.polymdegradstab.2022.110228_bib0009) 2021; 48
Havermans (10.1016/j.polymdegradstab.2022.110228_bib0023) 1995; 16
Zuliani (10.1016/j.polymdegradstab.2022.110228_bib0154) 2022; 614
Kapu (10.1016/j.polymdegradstab.2022.110228_bib0019) 2014; 8
Duplooy (10.1016/j.polymdegradstab.2022.110228_bib0037) 1981; 34
Gu (10.1016/j.polymdegradstab.2022.110228_bib0062) 2020; 41
Rasch (10.1016/j.polymdegradstab.2022.110228_bib0103) 1934
Andlar (10.1016/j.polymdegradstab.2022.110228_bib0080) 2018; 18
Zhang (10.1016/j.polymdegradstab.2022.110228_bib0149) 2017; 46
Kotsidi (10.1016/j.polymdegradstab.2022.110228_bib0152) 2021; 16
Strlič (10.1016/j.polymdegradstab.2022.110228_bib0025) 2011; 96
Jiang (10.1016/j.polymdegradstab.2022.110228_bib0032) 2018; 25
LiÉNardy (10.1016/j.polymdegradstab.2022.110228_bib0116) 1994; 15
Lattuati-Derieux (10.1016/j.polymdegradstab.2022.110228_bib0101) 2004; 1026
French (10.1016/j.polymdegradstab.2022.110228_bib0004) 2017; 24
Graminski (10.1016/j.polymdegradstab.2022.110228_bib0034) 1978; 2
Sjostrom (10.1016/j.polymdegradstab.2022.110228_bib0038) 1993
Ceres (10.1016/j.polymdegradstab.2022.110228_bib0144) 2008; 1
Lee (10.1016/j.polymdegradstab.2022.110228_bib0098) 1986
(10.1016/j.polymdegradstab.2022.110228_bib0139) 1994
Neves (10.1016/j.polymdegradstab.2022.110228_bib0157) 2009; 63
Lu (10.1016/j.polymdegradstab.2022.110228_bib0049) 2017; 2017
Malešič (10.1016/j.polymdegradstab.2022.110228_bib0055) 2005; 89
Negahdar (10.1016/j.polymdegradstab.2022.110228_bib0018) 2016; 184
Ahn (10.1016/j.polymdegradstab.2022.110228_bib0071) 2019; 26
Zhu (10.1016/j.polymdegradstab.2022.110228_bib0150) 2015; 3
Corte (10.1016/j.polymdegradstab.2022.110228_bib0086) 2003; 51
Grau-Bove (10.1016/j.polymdegradstab.2022.110228_bib0030) 2016; 4
Zervos (10.1016/j.polymdegradstab.2022.110228_bib0073) 2010
Zotti (10.1016/j.polymdegradstab.2022.110228_bib0088) 2008; 62
Giorgi (10.1016/j.polymdegradstab.2022.110228_bib0132) 2002; 18
Shahani (10.1016/j.polymdegradstab.2022.110228_bib0104) 2001
Clapp (10.1016/j.polymdegradstab.2022.110228_bib0138) 1987
Zhou (10.1016/j.polymdegradstab.2022.110228_bib0005) 2017; 5
Eronen (10.1016/j.polymdegradstab.2022.110228_bib0043) 2008; 16
Łojewski (10.1016/j.polymdegradstab.2022.110228_bib0072) 2010; 100
Arnold (10.1016/j.polymdegradstab.2022.110228_bib0074) 1998
Cheradame (10.1016/j.polymdegradstab.2022.110228_bib0125) 2003; 24
Shafizadeh (10.1016/j.polymdegradstab.2022.110228_bib0099) 1979; 23
Baty (10.1016/j.polymdegradstab.2022.110228_bib0021) 2005; 83
Rebrikova (10.1016/j.polymdegradstab.2022.110228_bib0089) 2000; 21
Ding (10.1016/j.polymdegradstab.2022.110228_bib0108) 2007; 14
Giorgi (10.1016/j.polymdegradstab.2022.110228_bib0134) 2005; 21
Zervos (10.1016/j.polymdegradstab.2022.110228_bib0007) 2006; 27
Rakotonirainy (10.1016/j.polymdegradstab.2022.110228_bib0126) 2008; 9
Zervos (10.1016/j.polymdegradstab.2022.110228_bib0095) 2015; 22
Duan (10.1016/j
References_xml – volume: 245
  year: 2020
  ident: bib0020
  article-title: Considerations on factors influencing the degradation of cellulose in alum-rosin sized paper
  publication-title: Carbohydr. Polym.
– volume: 10
  start-page: 46
  year: 1986
  end-page: 47
  ident: bib0155
  article-title: Fumigation quandary: more overkill or common sense?
  publication-title: Unification Elem. Forces Gauge Theor., Pap. Ben Lee Meml. Int. Conf. Parity Nonconserv., Weak Neutral Curr. Gauge Theor.
– volume: 19
  start-page: 609
  year: 1949
  end-page: 624
  ident: bib0068
  article-title: The autoxidation of alkali cellulose
  publication-title: Part 2., Textile Res. J.
– volume: 4
  start-page: 66
  year: 1979
  end-page: 80
  ident: bib0131
  article-title: The washing and aqueous deacidification of paper
  publication-title: The Paper Conservator
– volume: 42
  start-page: 327
  year: 1973
  end-page: 338
  ident: bib0063
  article-title: Degradation of cellulose by alkaline oxidation
  publication-title: Russ. Chem. Rev.
– volume: 25
  start-page: 1539
  year: 2018
  end-page: 1553
  ident: bib0032
  article-title: Microstructural model in COMSOL packages with simulation to aging behavior of paper materials
  publication-title: Cellulose
– volume: 13
  start-page: 1029
  year: 2021
  ident: bib0036
  article-title: Paper ageing: The effect of paper chemical composition on hydrolysis and oxidation
  publication-title: Polymers (Basel)
– volume: 26
  start-page: 429
  year: 2019
  end-page: 444
  ident: bib0071
  article-title: Yellowing and brightness reversion of celluloses: CO or COOH, who is the culprit?
  publication-title: Cellulose
– volume: 20
  start-page: 1
  year: 1999
  end-page: 21
  ident: bib0022
  article-title: The effect of air pollutants on paper stability
  publication-title: Restaurator
– volume: 25
  start-page: 179
  year: 1996
  end-page: 186
  ident: bib0002
  article-title: The chemistry of paper conservation
  publication-title: Chem. Soc. Rev.
– volume: 89
  start-page: 64
  year: 2005
  end-page: 69
  ident: bib0055
  article-title: Photo-induced degradation of cellulose
  publication-title: Polym. Degrad. Stab.
– volume: 51
  start-page: 167
  year: 2003
  end-page: 173
  ident: bib0086
  article-title: Isolation of fungal species from test samples and maps damaged by foxing, and correlation between these species and the environment
  publication-title: Int. Biodeterior. Biodegrad.
– volume: 24
  start-page: 323
  year: 2016
  end-page: 332
  ident: bib0115
  article-title: Critical evaluation of approaches toward mass deacidification of paper by dispersed particles
  publication-title: Cellulose
– volume: 89
  start-page: 913
  year: 2010
  end-page: 933
  ident: bib0003
  article-title: An overview of the chemical composition of biomass
  publication-title: Fuel
– year: 2001
  ident: bib0104
  article-title: Accelerated aging of paper: I. Chemical analysis of degradation products. II. Application of Arrhenius relationship. III. Proposal for a new accelerated aging test: ASTM research program into the effect of aging on printing and writing papers
– volume: 17
  start-page: 1519
  year: 2015
  end-page: 1524
  ident: bib0065
  article-title: Depolymerization of cellulose to glucose by oxidation–hydrolysis
  publication-title: Green Chem.
– volume: 22
  start-page: 20
  year: 2001
  end-page: 40
  ident: bib0069
  article-title: Study of the photo-oxidation of mass-deacidified papers
  publication-title: Restaurator
– year: 1986
  ident: bib0098
  article-title: Historic textile and paper materials
  publication-title: Conserv. Characteriz.
– volume: 10
  start-page: 6305
  year: 2015
  end-page: 6309
  ident: bib0117
  article-title: Oops, I thought that those books had been deacidified
  publication-title: Bioresources
– volume: 547
  start-page: 370
  year: 2019
  end-page: 381
  ident: bib0136
  article-title: The carbonation kinetics of calcium hydroxide nanoparticles: A Boundary Nucleation and Growth description
  publication-title: J. Colloid Interface Sci.
– year: 2013
  ident: bib0081
  article-title: The saccharification step: The main enzymatic components
– volume: 14
  start-page: 1
  year: 2005
  end-page: 9
  ident: bib0031
  article-title: The effects of heating without water removal and drying on the swelling as measured by water retention value and degradation as measured by intrinsic viscosity of cellulose papermaking fibers
  publication-title: Prog. Pap. Recycl.
– volume: 96
  start-page: 608
  year: 2011
  end-page: 615
  ident: bib0025
  article-title: The effect of volatile organic compounds and hypoxia on paper degradation
  publication-title: Polym. Degrad. Stab.
– volume: 19
  start-page: 1149
  year: 2012
  end-page: 1159
  ident: bib0042
  article-title: Is cellulose degradation due to β-elimination processes a threat in mass deacidification of library books?
  publication-title: Cellulose
– volume: 252
  start-page: 1159
  year: 2005
  end-page: 1166
  ident: bib0161
  article-title: Investigation of the effects of plasma treatments on biodeteriorated ancient paper
  publication-title: Appl. Surf. Sci.
– volume: 91
  start-page: 3448
  year: 2006
  end-page: 3455
  ident: bib0112
  article-title: Mass deacidification of papers and books. IV - A study of papers treated with aminoalkylalkoxysilanes and their resistance to ageing
  publication-title: Polym. Degrad. Stab.
– volume: 29
  start-page: 6889
  year: 2022
  end-page: 6905
  ident: bib0120
  article-title: Evaluation of Bookkeeper mass deacidification based on historical book papers
  publication-title: Cellulose
– volume: 12
  start-page: 4410
  year: 2017
  end-page: 4477
  ident: bib0110
  article-title: Deacidification of acidic books and paper by means of non-aqueous dispersions of alkaline particles: A review focusing on completeness of the reaction
  publication-title: Bioresources
– volume: 28
  start-page: 47
  year: 2007
  end-page: 54
  ident: bib0102
  article-title: Autocatalytic degradation of cellulose paper in sealed vessels
  publication-title: Restaurator
– volume: 116
  start-page: 7557
  year: 1994
  end-page: 7563
  ident: bib0013
  article-title: Kinetic isotope effect study of transition states for the hydrolyses of α- and β-glucopyranosyl fluorides
  publication-title: J. Am. Chem. Soc.
– volume: 23
  start-page: 1431
  year: 1979
  end-page: 1442
  ident: bib0099
  article-title: Thermal-degradation of cellulose in air and nitrogen at low-temperatures
  publication-title: J. Appl. Polym. Sci.
– volume: 165
  start-page: 784
  year: 2010
  end-page: 797
  ident: bib0053
  article-title: Dye sensitized visible light degradation of phenolic compounds
  publication-title: Chem. Eng. J.
– volume: 12
  start-page: 16
  year: 1971
  end-page: 32
  ident: bib0130
  article-title: Chemistry of the deacidification of paper
  publication-title: Bull. Am. Group. Int. Institute for Conserv. Historic and Artistic Works
– volume: 20
  start-page: 1989
  year: 2013
  end-page: 2001
  ident: bib0045
  article-title: The influence of alkaline reserve on the aging behavior of book papers
  publication-title: Cellulose
– volume: 614
  start-page: 451
  year: 2022
  end-page: 459
  ident: bib0154
  article-title: Environmentally friendly ZnO/Castor oil polyurethane composites for the gas-phase adsorption of acetic acid
  publication-title: J. Colloid Interface Sci.
– volume: 108
  start-page: 1
  year: 1997
  end-page: 35
  ident: bib0056
  article-title: An overview of semiconductor photocatalysis
  publication-title: J. Photochem. Photobiol. A
– volume: 3
  start-page: 1339
  year: 2015
  end-page: 1347
  ident: bib0006
  article-title: Acidolysis of α-o-4 aryl-ether bonds in lignin model compounds: a modeling and experimental study
  publication-title: ACS Sustain. Chem. Eng.
– volume: 107
  start-page: 328
  year: 2014
  end-page: 340
  ident: bib0026
  article-title: Emissions from polymeric materials: characterised by thermal desorption-gas chromatography
  publication-title: Polym. Degrad. Stab.
– volume: 69
  start-page: 549
  year: 1936
  end-page: 552
  ident: bib0097
  article-title: On the behavior of cellulose in hydrochloric acid solution. I. The determination of molecular weight in phosphoric acid solution
  publication-title: Chem. Ber.
– volume: 27
  start-page: 9
  year: 2006
  end-page: 23
  ident: bib0137
  article-title: The effect of sodium and calcium ions in the deacidification of paper - A chemo-physical study using thermal analysis
  publication-title: Restaurator
– volume: 8
  start-page: 2688
  year: 2020
  end-page: 2697
  ident: bib0054
  article-title: Evaluation of ultraviolet light and hydrogen peroxide enhanced ozone oxidation treatment for the production of cellulose nanofibrils
  publication-title: ACS Sustain. Chem. Eng.
– volume: 108
  year: 2012
  ident: bib0070
  article-title: Role of cellulose oxidation in the yellowing of ancient paper
  publication-title: Phys. Rev. Lett.
– volume: 11
  start-page: 165
  year: 1990
  end-page: 178
  ident: bib0128
  article-title: Paper deacidification in large workshops: effectiveness and practicability
  publication-title: Restaurator
– volume: 16
  start-page: 1
  year: 1995
  end-page: 9
  ident: bib0119
  article-title: The battelle mass deacidification process equipment and technology
  publication-title: Restaurator
– start-page: 4500
  year: 1957
  end-page: 4506
  ident: bib0039
  article-title: The alkaline degradation of polysaccharides. Part 2. The alkali-stable residue from the action of sodium hydroxide on cellulose
  publication-title: J. Chem. Soc.
– volume: 4
  start-page: 19
  year: 2007
  end-page: 24
  ident: bib0143
  article-title: Stabilisation of iron gall ink: aqueous treatment with magnesium phytate
  publication-title: e-Preserv. Sci.
– volume: 11
  start-page: 39
  year: 2003
  end-page: 47
  ident: bib0040
  article-title: Alkaline degradation of cellulose: mechanisms and kinetics
  publication-title: J. Polym. Environ.
– volume: 83
  start-page: 1516
  year: 2005
  end-page: 1524
  ident: bib0021
  article-title: The kinetics of the spontaneous, proton-and AlIII-catalysed hydrolysis of 1, 5-anhydrocellobiitol models for cellulose depolymerization in paper aging and alkaline pulping, and a benchmark for cellulase efficiency
  publication-title: Can. J. Chem.
– volume: 23
  start-page: 39
  year: 2002
  end-page: 47
  ident: bib0118
  article-title: Testing CSC Book Saver (R), a commercial deacidification spray
  publication-title: Restaurator
– volume: 27
  start-page: 219
  year: 2006
  end-page: 274
  ident: bib0007
  article-title: Methodology and criteria for the evaluation of paper conservation interventions - a literature review
  publication-title: Restaurator
– volume: 1
  start-page: 176
  year: 2004
  end-page: 182
  ident: bib0035
  article-title: The design and operation of a passive humidity-controlled cold storage vault using conventional freezer technology and moisture-sealed cabinets
  publication-title: Society for Imaging Sci. Technol.
– volume: 3
  start-page: 29
  year: 2022
  end-page: 34
  ident: bib0148
  article-title: Proper exhibition and preventive protection of books and paper
  publication-title: Library Work and Study
– volume: 30
  start-page: 203
  year: 1981
  end-page: 224
  ident: bib0016
  article-title: A review of paper quality and paper chemistry
  publication-title: Library Trends
– volume: 62
  start-page: 186
  year: 2008
  end-page: 194
  ident: bib0088
  article-title: Microfungal biodeterioration of historic paper: Preliminary FTIR and microbiological analyses
  publication-title: Int. Biodeterior. Biodegrad.
– volume: 100
  start-page: 809
  year: 2010
  end-page: 821
  ident: bib0072
  article-title: Evaluating paper degradation progress. Cross-linking between chromatographic, spectroscopic and chemical results
  publication-title: Appl. Phys. A
– volume: 10
  start-page: 19998
  year: 2020
  ident: bib0078
  article-title: Influence of lignin content in cellulose pulp on paper durability
  publication-title: Scientific Rep.
– volume: 33
  start-page: 48
  year: 2012
  end-page: 75
  ident: bib0141
  article-title: Sustainability of mass-deacidification. Part II: Evaluation of alkaline reserve
  publication-title: Restaurator
– volume: 24
  start-page: 89
  year: 1998
  end-page: 94
  ident: bib0017
  article-title: Aging and stabilization of alkaline paper
  publication-title: J. Pulp Pap. Sci.
– volume: 8
  start-page: 857
  year: 2014
  end-page: 870
  ident: bib0019
  article-title: Review of hemicellulose hydrolysis in softwoods and bamboo
  publication-title: Biofuels Bioprod. Biorefin.
– volume: 6
  start-page: 1875
  year: 1964
  end-page: 1882
  ident: bib0064
  article-title: Mechanism of the oxidative degradation of cellulose in alkaline media—II. Mechanism of the oxidation of cellulose in an alkaline medium by oxygen
  publication-title: Polym. Sci. U.S.S.R.
– year: 1987
  ident: bib0138
  article-title: Curatorial care of works of art on paper: basic procedures for paper preservation
– volume: 92
  start-page: 1476
  year: 2007
  end-page: 1481
  ident: bib0058
  article-title: The role of transition metals in oxidative degradation of cellulose
  publication-title: Polym. Degrad. Stab.
– volume: 41
  start-page: 1073
  year: 2020
  end-page: 1080
  ident: bib0062
  article-title: Hydroxyl radicals-mediated oxidative cleavage of the glycosidic bond in cellobiose by copper catalysts and its application to low-temperature depolymerization of cellulose
  publication-title: Chin. J. Catal.
– volume: 2
  start-page: 175
  year: 1978
  end-page: 178
  ident: bib0034
  article-title: The effects of temperature and moisture on the accelerated aging of paper
  publication-title: Restaurator
– volume: 63
  start-page: 267
  year: 2009
  end-page: 272
  ident: bib0157
  article-title: Antifungal effect of different methyl and propyl paraben mixtures on the treatment of paper biodeterioration
  publication-title: Int. Biodeterior. Biodegrad.
– volume: 16
  start-page: 209
  year: 1995
  end-page: 233
  ident: bib0023
  article-title: Effects of air pollutants on the accelerated ageing of cellulose-based materials
  publication-title: Restaurator
– volume: 5
  start-page: 113
  year: 2004
  end-page: 118
  ident: bib0159
  article-title: The recovery of biodeteriorated books and archive documents through gamma radiation: Some considerations on the results achieved
  publication-title: J Cult Herit
– volume: 1
  start-page: 26
  year: 1994
  end-page: 56
  ident: bib0008
  article-title: Kinetics and mechanisms of the low-temperature degradation of cellulose
  publication-title: Cellulose
– volume: 6
  start-page: 5555
  year: 2018
  end-page: 5565
  ident: bib0047
  article-title: Hydrolysis of cellobiose and xylan over TiO
  publication-title: ACS Sustain Chem Eng
– volume: 25
  start-page: 104
  year: 2004
  end-page: 118
  ident: bib0121
  article-title: Mass deacidification of paper and books - II: Deacidification in the liquid phase using aminosilanes
  publication-title: Restaurator
– volume: 16
  start-page: 167
  year: 2008
  end-page: 178
  ident: bib0043
  article-title: Effect of alkaline treatment on cellulose supramolecular structure studied with combined confocal Raman spectroscopy and atomic force microscopy
  publication-title: Cellulose
– year: 2016
  ident: bib0048
  article-title: Lignin and lignans: advances in chemistry
– volume: 16
  start-page: 143
  year: 1995
  end-page: 160
  ident: bib0142
  article-title: Phytate - a potential conservation agent for the treatment of ink corrosion caused by iron gall inks
  publication-title: Restaurator
– volume: 6
  start-page: 27813
  year: 2016
  end-page: 27823
  ident: bib0153
  article-title: Metal organic frameworks as sorption media for volatile and semi-volatile organic compounds at ambient conditions
  publication-title: Sci. Rep.
– volume: 2017
  start-page: 1
  year: 2017
  end-page: 15
  ident: bib0049
  article-title: Structural characterization of lignin and its degradation products with spectroscopic methods
  publication-title: J. Spectroscopy
– volume: 6
  start-page: 18204
  year: 2016
  end-page: 18216
  ident: bib0052
  article-title: Production of phenolics via photocatalysis of ball milled lignin–TiO
  publication-title: RSC Adv.
– volume: 233
  start-page: 351
  year: 2002
  end-page: 371
  ident: bib0050
  article-title: Photosensitized singlet oxygen and its applications
  publication-title: Coord. Chem. Rev.
– year: 2012
  ident: bib0014
  article-title: Cellulose hydrolysis
– volume: 34
  start-page: 287
  year: 1981
  end-page: 292
  ident: bib0037
  article-title: The influence of moisture-content and temperature on the aging rate of paper
  publication-title: Appita
– volume: 46
  start-page: 137
  year: 2007
  end-page: 152
  ident: bib0085
  article-title: Foxing on paper: A literature review
  publication-title: J. Am. Inst. Conserv.
– volume: 670
  start-page: 110
  year: 2019
  end-page: 121
  ident: bib0060
  article-title: A review on Fenton process for organic wastewater treatment based on optimization perspective
  publication-title: Sci. Total Environ.
– volume: 48
  start-page: 94
  year: 2001
  end-page: 97
  ident: bib0092
  article-title: Observations on the foxing of paper (Reprinted)
  publication-title: Int. Biodeterior. Biodegrad.
– volume: 19
  start-page: 135
  year: 1998
  end-page: 154
  ident: bib0076
  article-title: The impact of lignin on paper permanence - A comprehensive study of the ageing behaviour of handsheets and commercial paper samples
  publication-title: Restaurator
– volume: 46
  start-page: 181
  year: 2000
  end-page: 188
  ident: bib0091
  article-title: Foxing caused by Fungi: twenty-five years of study
  publication-title: Int. Biodeterior. Biodegrad.
– volume: 17
  start-page: 25
  year: 1996
  end-page: 31
  ident: bib0127
  article-title: Effect of various deacidification solutions on the stability of cellulose pulps
  publication-title: Restaurator
– volume: 113
  start-page: 7951
  year: 1991
  end-page: 7958
  ident: bib0012
  article-title: Reactions of anionic nucleophiles with α-D-glucopyranosyl fluoride in aqueous solution through a concerted, ANDN (SN2) mechanism
  publication-title: J. Am. Chem. Soc.
– volume: 10
  start-page: 40
  year: 1986
  end-page: 45
  ident: bib0156
  article-title: Biodeterioration of library materials. Disinfection methods and new alternatives
  publication-title: Unification Elem. Forces Gauge Theor., Pap. Ben Lee Meml. Int. Conf. Parity Nonconserv., Weak Neutral Curr. Gauge Theor.
– volume: 5
  start-page: 407
  year: 1935
  end-page: 418
  ident: bib0094
  article-title: Notes on the causes and prevention of foxing in books
  publication-title: Libr. Q.
– volume: 9
  start-page: 54
  year: 2008
  end-page: 59
  ident: bib0126
  article-title: Mass deacidification of papers and books: V. Fungistatic properties of papers treated with aminoalkylalkoxysilanes
  publication-title: J Cult Herit
– year: 1934
  ident: bib0103
  article-title: Comparison of natural aging of paper with accelerated aging by heating
– volume: 3
  start-page: 269
  year: 1996
  end-page: 279
  ident: bib0106
  article-title: Prediction of paper permanence by accelerated aging II. Comparison of the predictions with natural aging results
  publication-title: Cellulose
– volume: 43
  start-page: 393
  year: 1994
  end-page: 402
  ident: bib0096
  article-title: Accelerated aging of papers of pure cellulose - Mechanism of cellulose degradation and paper embrittlement
  publication-title: Polym. Degrad. Stab.
– volume: 4
  start-page: 1
  year: 2016
  end-page: 8
  ident: bib0030
  article-title: The effect of particulate matter on paper degradation
  publication-title: Heritage Sci.
– start-page: 53
  year: 1998
  end-page: 64
  ident: bib0074
  article-title: Predicting printing paper life expectancy, Process and product quality conference and trade fair
– volume: 27
  start-page: 10798
  year: 2021
  end-page: 10806
  ident: bib0001
  article-title: How science can contribute to the remedial conservation of cultural heritage
  publication-title: Chem.
– volume: 790
  start-page: 148204
  year: 2021
  end-page: 148214
  ident: bib0082
  article-title: Biological risk assessment in the history and historical documentation library of the university of Milan
  publication-title: Sci. Total Environ.
– volume: 57
  start-page: 1235
  year: 2002
  end-page: 1249
  ident: bib0090
  article-title: Study of foxing stains on paper by chemical methods, infrared spectroscopy, micro-X-ray fluorescence spectrometry and laser induced breakdown spectroscopy
  publication-title: Spectrochim Acta Part B At Spectrosc
– volume: 29
  start-page: 184
  year: 2008
  end-page: 198
  ident: bib0146
  article-title: New antioxidants for treatment of transition metal containing inks and pigments
  publication-title: Restaurator
– year: 1996
  ident: bib0079
  article-title: Pulp bleaching: principles and practice
– volume: 16
  start-page: 123
  year: 1995
  end-page: 142
  ident: bib0113
  article-title: Mass deacidification of archival materials using diethyl zinc
  publication-title: Restaurator
– volume: 28
  start-page: 37
  year: 2009
  end-page: 45
  ident: bib0147
  article-title: Where archival and fine art conservation meet: Applying iron gall ink antioxidant and deacidification treatments to corrosive copper watercolors
  publication-title: The Book and Paper Group Annual
– volume: 32
  year: 2011
  ident: bib0041
  article-title: Sustainability of mass deacidification. Part I: Concept, selection of sample books and pH-determination
  publication-title: Restaurator
– volume: 15
  start-page: 569
  year: 2014
  end-page: 574
  ident: bib0151
  article-title: Titanium dioxide thin film: Environmental control for preservation of paper-art-works
  publication-title: J Cult Herit
– volume: 98
  start-page: 1827
  year: 2013
  end-page: 1837
  ident: bib0024
  article-title: The impact of volatile compounds released by paper on cellulose degradation in ambient hygrothermal conditions
  publication-title: Polym. Degrad. Stab.
– volume: 5
  start-page: 216
  year: 2017
  ident: bib0005
  article-title: A critical review on hemicellulose pyrolysis
  publication-title: Energy Technol.
– volume: 12
  start-page: 445
  year: 2005
  end-page: 447
  ident: bib0100
  article-title: The influence of levelling-off degree of polymerisation on the kinetics of cellulose degradation
  publication-title: Cellulose
– volume: 16
  start-page: 1004
  year: 2021
  end-page: 1010
  ident: bib0152
  article-title: Preventing colour fading in artworks with graphene veils
  publication-title: Nat. Nanotechnol.
– year: 1993
  ident: bib0038
  article-title: Wood chemistry: fundamentals and applications
– volume: 274
  start-page: 466
  year: 1978
  end-page: 468
  ident: bib0083
  article-title: Foxing, a fungal infection of paper
  publication-title: Nature
– volume: 15
  start-page: 247
  year: 1995
  end-page: 262
  ident: bib0077
  article-title: The Role of lignin in the mechanical permanence of paper: Part II. Effect of acid groups
  publication-title: J. Wood Chem. Technol.
– year: 1976
  ident: bib0033
  article-title: The effects of temperature and moisture on the accelerated aging of paper
– volume: 25
  start-page: 5
  year: 1989
  end-page: 81
  ident: bib0133
  article-title: Mass deacidification for libraries: 1989 update
  publication-title: Libr. Technol. Rep.
– volume: 22
  start-page: 1
  year: 2001
  end-page: 19
  ident: bib0093
  article-title: Characterization of foxing stains by chemical and spectrometric methods
  publication-title: Restaurator
– start-page: 361
  year: 1987
  end-page: 472
  ident: bib0114
  article-title: Mass deacidification for libraries
  publication-title: Libr. Technol. Rep.
– volume: 24
  start-page: 227
  year: 2003
  end-page: 239
  ident: bib0125
  article-title: Mass deacidification of paper and books I: Study of the limitations of the gas phase processes
  publication-title: Restaurator
– volume: 184
  start-page: 285
  year: 2016
  end-page: 298
  ident: bib0018
  article-title: Aqueous-phase hydrolysis of cellulose and hemicelluloses over molecular acidic catalysts: Insights into the kinetics and reaction mechanism
  publication-title: Appl. Catal. B
– volume: 19
  start-page: 527
  year: 1949
  end-page: 546
  ident: bib0066
  article-title: The autoxidation of alkali cellulose. Part 1. An experimental study of the kinetics of the reaction
  publication-title: Text. Res. J.
– volume: 156
  start-page: 253
  year: 2003
  end-page: 265
  ident: bib0051
  article-title: Routes of degradation of β-O-4 syringyl and guaiacyl lignin model compounds during photobleaching processes
  publication-title: J. Photochem. Photobiol. A
– volume: 7
  start-page: 1
  year: 2019
  end-page: 14
  ident: bib0135
  article-title: Nano calcium carbonate versus nano calcium hydroxide in alcohols as a deacidification medium for lignocellulosic paper
  publication-title: Heritage Sci.
– volume: 11
  start-page: 1
  year: 1990
  end-page: 21
  ident: bib0140
  article-title: Practical deacidification
  publication-title: Restaurator
– volume: 21
  start-page: 85
  year: 2000
  end-page: 100
  ident: bib0089
  article-title: Foxing - A new approach to an old problem
  publication-title: Restaurator
– volume: 57
  start-page: 163
  year: 2006
  end-page: 167
  ident: bib0160
  article-title: Inactivation of fungi from deteriorated paper materials by radiation
  publication-title: Int. Biodeteriorat. Biodegr.
– volume: 116
  start-page: 14178
  year: 2012
  end-page: 14182
  ident: bib0061
  article-title: Ferryl-Oxo species produced from fenton's reagent via a two-step pathway: minimum free-energy path analysis
  publication-title: J. Phys. Chem. B
– volume: 6
  start-page: 5307
  year: 2011
  end-page: 5337
  ident: bib0010
  article-title: Paper aging and degradation: recent findings and research methods
  publication-title: Bioresources
– volume: 79
  start-page: 383
  year: 2004
  end-page: 387
  ident: bib0084
  article-title: Surface analysis of paper documents damaged by foxing
  publication-title: Appl. Phys. a-Mater. Sci. Processing
– volume: 18
  start-page: 8198
  year: 2002
  end-page: 8203
  ident: bib0132
  article-title: Nanotechnologies for conservation of cultural heritage: Paper and canvas deacidification
  publication-title: Langmuir
– volume: 48
  start-page: 269
  year: 2021
  end-page: 276
  ident: bib0009
  article-title: Oxidative degradation of paper-A minireview
  publication-title: J. Cult. Herit.
– start-page: 127
  year: 1979
  end-page: 143
  ident: bib0015
  article-title: Influence of cellulose physical structure on thermohydrolytic, hydrolytic, and enzymatic degradation of cellulose
– volume: 1026
  start-page: 9
  year: 2004
  end-page: 18
  ident: bib0101
  article-title: Identification of volatile organic compounds emitted by a naturally aged book using solid-phase microextraction/gas chromatography/mass spectrometry
  publication-title: J. Chromatogr. A
– volume: 14
  start-page: 171
  year: 2007
  end-page: 181
  ident: bib0108
  article-title: Time–temperature superposition method for predicting the permanence of paper by extrapolating accelerated ageing data to ambient conditions
  publication-title: Cellulose
– volume: 23
  start-page: 95
  year: 1932
  end-page: 133
  ident: bib0067
  article-title: 9–the oxidation by gaseous oxygen of cotton impregnated with sodium hydroxide solution
  publication-title: J. Textile Institute Trans.
– volume: 18
  start-page: 768
  year: 2018
  end-page: 778
  ident: bib0080
  article-title: Lignocellulose degradation: An overview of fungi and fungal enzymes involved in lignocellulose degradation
  publication-title: Eng. Life Sci.
– volume: 483
  start-page: 159
  year: 2017
  end-page: 164
  ident: bib0145
  article-title: The nitroxide Tempo inhibits hydroxyl radical production from the Fenton-like reaction of iron(II)-citrate with hydrogen peroxide
  publication-title: Biochem. Biophys. Res. Commun.
– volume: 3
  start-page: 57
  year: 2015
  end-page: 60
  ident: bib0150
  article-title: Research review of nano-TiO
  publication-title: China Cultural Heritage Scientific Res.
– volume: 3
  start-page: 243
  year: 1996
  end-page: 267
  ident: bib0105
  article-title: Prediction of paper permanence by accelerated aging I. Kinetic analysis of the aging process
  publication-title: Cellulose
– year: 1977
  ident: bib0129
  article-title: Methylmagnesium carbonate-an improved nonaqueous deacidification agent
– volume: 95
  start-page: 2300
  year: 2010
  end-page: 2308
  ident: bib0123
  article-title: Mass deacidification and reinforcement of papers and books VI - Study of aminopropylmethyldiethoxysilane treated papers
  publication-title: Polym. Degrad. Stab.
– volume: 26
  start-page: 250
  year: 2005
  end-page: 264
  ident: bib0122
  article-title: Mass deacidification of papers and books III: Study of a paper strengthening and deacidification process with amino alkyl alkoxy silanes
  publication-title: Restaurator
– volume: 92
  start-page: 1893
  year: 1988
  end-page: 1897
  ident: bib0057
  article-title: Kinetics for electron transfer from laser-pulse irradiated colloidal semiconductors to adsorbed methylviologen: dependence of the quantum yield on incident pulse width
  publication-title: J. Phys. Chem.
– volume: 1
  start-page: 921
  year: 2008
  end-page: 926
  ident: bib0144
  article-title: Imidazolium-based ionic liquids for the efficient treatment of iron gall inked papers
  publication-title: ChemSusChem
– volume: 21
  start-page: 55
  year: 2000
  end-page: 76
  ident: bib0075
  article-title: The influence of light on ageing of newsprint paper
  publication-title: Restaurator
– start-page: 22
  year: 2010
  end-page: 26
  ident: bib0158
  article-title: Propiedades del papel de celulosa pura irradiado y envejecido
  publication-title: XXXVII Reunion Anual de la Asociacion Argentina de Tecnologia Nuclear
– volume: 22
  start-page: 2859
  year: 2015
  end-page: 2897
  ident: bib0095
  article-title: Paper conservation methods: a literature review
  publication-title: Cellulose
– volume: 24
  start-page: 4605
  year: 2017
  end-page: 4609
  ident: bib0004
  article-title: Glucose, not cellobiose, is the repeating unit of cellulose and why that is important
  publication-title: Cellulose
– volume: 26
  start-page: 4589
  year: 2019
  end-page: 4599
  ident: bib0044
  article-title: Paper conservation with an aqueous NaOH/urea cellulose solution
  publication-title: Cellulose
– volume: 21
  start-page: 401
  year: 2011
  end-page: 409
  ident: bib0059
  article-title: Oxidative depolymerization of polysaccharides by reactive oxygen/nitrogen species
  publication-title: Glycobiology
– volume: 132
  start-page: 157
  year: 2018
  end-page: 165
  ident: bib0087
  article-title: Analysis of paper foxing by newly available omics techniques
  publication-title: Int. Biodeterior. Biodegrad.
– volume: 107
  start-page: 314
  year: 2014
  end-page: 320
  ident: bib0028
  article-title: Characterization and degradation of poly(vinyl acetate)-based adhesives for canvas paintings
  publication-title: Polym. Degrad. Stab.
– volume: 17
  start-page: 13
  year: 1981
  end-page: 18
  ident: bib0046
  article-title: Generation and reactivities of various types of oxygen radicals
  publication-title: Clin.l Respiratory Physiol.-Bull. Europ. De Physiopathologie Respiratoire
– volume: 101
  start-page: 1249
  year: 2014
  end-page: 1254
  ident: bib0107
  article-title: Deterioration of ancient Korean paper (Hanji), treated with beeswax: A mechanistic study
  publication-title: Carbohydr. Polym.
– volume: 15
  start-page: 1
  year: 1994
  end-page: 25
  ident: bib0116
  article-title: Evaluation of seven mass deacidification treatments
  publication-title: Restaurator
– start-page: 155
  year: 2010
  end-page: 203
  ident: bib0073
  article-title: Natural and accelerated ageing of cellulose and paper: a literature review
  publication-title: Cellulose: structure and properties, derivatives and industrial uses
– volume: 26
  start-page: 63
  year: 2005
  end-page: 75
  ident: bib0124
  article-title: Mass deacidification technology in Germany and its quality control
  publication-title: Restaurator
– year: 1994
  ident: bib0139
  article-title: Information and documentation. Paper for documents. Requirements for permanence
– volume: 46
  start-page: 17
  year: 2017
  end-page: 19
  ident: bib0149
  article-title: Study on anti aging and anti fouling properties of cellulose-TiO
  publication-title: Papermaking equipment and mater.
– volume: 5
  start-page: 1955
  year: 2010
  end-page: 2023
  ident: bib0011
  article-title: Deacidification for the conservation and preservation of paper-based works: a review
  publication-title: Bioresources
– start-page: 81
  year: 2008
  end-page: 89
  ident: bib0109
  article-title: A comparison of artificial ageing with 27 years of natural ageing
  publication-title: AICCM Book, Paper and Photographic Materials Symposium
– volume: 27
  start-page: 35
  year: 2006
  end-page: 45
  ident: bib0111
  article-title: Patents for paper deacidification
  publication-title: Restaurator
– volume: 61
  start-page: 203
  year: 2016
  end-page: 208
  ident: bib0029
  article-title: The effect of dust particles on cellulose degradation
  publication-title: Stud. Conserv.
– volume: 107
  start-page: 294
  year: 2014
  end-page: 306
  ident: bib0027
  article-title: Cross-infection effect of polymers of historic and heritage significance on the degradation of a cellulose reference test material
  publication-title: Polym. Degrad. Stab.
– volume: 21
  start-page: 8495
  year: 2005
  end-page: 8501
  ident: bib0134
  article-title: Nanoparticles of Mg(OH)
  publication-title: Langmuir
– volume: 42
  start-page: 327
  year: 1973
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0063
  article-title: Degradation of cellulose by alkaline oxidation
  publication-title: Russ. Chem. Rev.
  doi: 10.1070/RC1973v042n04ABEH002585
– volume: 16
  start-page: 167
  year: 2008
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0043
  article-title: Effect of alkaline treatment on cellulose supramolecular structure studied with combined confocal Raman spectroscopy and atomic force microscopy
  publication-title: Cellulose
  doi: 10.1007/s10570-008-9259-8
– volume: 20
  start-page: 1989
  year: 2013
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0045
  article-title: The influence of alkaline reserve on the aging behavior of book papers
  publication-title: Cellulose
  doi: 10.1007/s10570-013-9978-3
– volume: 233
  start-page: 351
  year: 2002
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0050
  article-title: Photosensitized singlet oxygen and its applications
  publication-title: Coord. Chem. Rev.
  doi: 10.1016/S0010-8545(02)00034-6
– volume: 62
  start-page: 186
  year: 2008
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0088
  article-title: Microfungal biodeterioration of historic paper: Preliminary FTIR and microbiological analyses
  publication-title: Int. Biodeterior. Biodegrad.
  doi: 10.1016/j.ibiod.2008.01.005
– volume: 7
  start-page: 1
  year: 2019
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0135
  article-title: Nano calcium carbonate versus nano calcium hydroxide in alcohols as a deacidification medium for lignocellulosic paper
  publication-title: Heritage Sci.
  doi: 10.1186/s40494-019-0294-6
– volume: 790
  start-page: 148204
  year: 2021
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0082
  article-title: Biological risk assessment in the history and historical documentation library of the university of Milan
  publication-title: Sci. Total Environ.
  doi: 10.1016/j.scitotenv.2021.148204
– volume: 25
  start-page: 104
  year: 2004
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0121
  article-title: Mass deacidification of paper and books - II: Deacidification in the liquid phase using aminosilanes
  publication-title: Restaurator
– volume: 19
  start-page: 527
  year: 1949
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0066
  article-title: The autoxidation of alkali cellulose. Part 1. An experimental study of the kinetics of the reaction
  publication-title: Text. Res. J.
  doi: 10.1177/004051754901900901
– volume: 15
  start-page: 569
  year: 2014
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0151
  article-title: Titanium dioxide thin film: Environmental control for preservation of paper-art-works
  publication-title: J Cult Herit
  doi: 10.1016/j.culher.2013.10.008
– volume: 6
  start-page: 1875
  year: 1964
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0064
  article-title: Mechanism of the oxidative degradation of cellulose in alkaline media—II. Mechanism of the oxidation of cellulose in an alkaline medium by oxygen
  publication-title: Polym. Sci. U.S.S.R.
  doi: 10.1016/0032-3950(64)90285-0
– volume: 22
  start-page: 20
  year: 2001
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0069
  article-title: Study of the photo-oxidation of mass-deacidified papers
  publication-title: Restaurator
– volume: 17
  start-page: 25
  year: 1996
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0127
  article-title: Effect of various deacidification solutions on the stability of cellulose pulps
  publication-title: Restaurator
– volume: 34
  start-page: 287
  year: 1981
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0037
  article-title: The influence of moisture-content and temperature on the aging rate of paper
  publication-title: Appita
– volume: 29
  start-page: 6889
  year: 2022
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0120
  article-title: Evaluation of Bookkeeper mass deacidification based on historical book papers
  publication-title: Cellulose
  doi: 10.1007/s10570-022-04681-9
– volume: 83
  start-page: 1516
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0021
  article-title: The kinetics of the spontaneous, proton-and AlIII-catalysed hydrolysis of 1, 5-anhydrocellobiitol models for cellulose depolymerization in paper aging and alkaline pulping, and a benchmark for cellulase efficiency
  publication-title: Can. J. Chem.
  doi: 10.1139/v05-168
– volume: 11
  start-page: 1
  year: 1990
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0140
  article-title: Practical deacidification
  publication-title: Restaurator
– volume: 108
  year: 2012
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0070
  article-title: Role of cellulose oxidation in the yellowing of ancient paper
  publication-title: Phys. Rev. Lett.
– volume: 25
  start-page: 5
  year: 1989
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0133
  article-title: Mass deacidification for libraries: 1989 update
  publication-title: Libr. Technol. Rep.
– volume: 184
  start-page: 285
  year: 2016
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0018
  article-title: Aqueous-phase hydrolysis of cellulose and hemicelluloses over molecular acidic catalysts: Insights into the kinetics and reaction mechanism
  publication-title: Appl. Catal. B
  doi: 10.1016/j.apcatb.2015.11.039
– volume: 10
  start-page: 6305
  year: 2015
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0117
  article-title: Oops, I thought that those books had been deacidified
  publication-title: Bioresources
  doi: 10.15376/biores.10.4.6305-6309
– volume: 89
  start-page: 64
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0055
  article-title: Photo-induced degradation of cellulose
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2005.01.003
– volume: 22
  start-page: 2859
  year: 2015
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0095
  article-title: Paper conservation methods: a literature review
  publication-title: Cellulose
  doi: 10.1007/s10570-015-0699-7
– start-page: 4500
  year: 1957
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0039
  article-title: The alkaline degradation of polysaccharides. Part 2. The alkali-stable residue from the action of sodium hydroxide on cellulose
  publication-title: J. Chem. Soc.
  doi: 10.1039/jr9570004500
– volume: 100
  start-page: 809
  year: 2010
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0072
  article-title: Evaluating paper degradation progress. Cross-linking between chromatographic, spectroscopic and chemical results
  publication-title: Appl. Phys. A
  doi: 10.1007/s00339-010-5657-5
– year: 1987
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0138
– volume: 16
  start-page: 1
  year: 1995
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0119
  article-title: The battelle mass deacidification process equipment and technology
  publication-title: Restaurator
– volume: 69
  start-page: 549
  year: 1936
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0097
  article-title: On the behavior of cellulose in hydrochloric acid solution. I. The determination of molecular weight in phosphoric acid solution
  publication-title: Chem. Ber.
– volume: 63
  start-page: 267
  year: 2009
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0157
  article-title: Antifungal effect of different methyl and propyl paraben mixtures on the treatment of paper biodeterioration
  publication-title: Int. Biodeterior. Biodegrad.
  doi: 10.1016/j.ibiod.2008.07.011
– volume: 5
  start-page: 216
  year: 2017
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0005
  article-title: A critical review on hemicellulose pyrolysis
  publication-title: Energy Technol.
  doi: 10.1002/ente.201600667
– volume: 24
  start-page: 227
  year: 2003
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0125
  article-title: Mass deacidification of paper and books I: Study of the limitations of the gas phase processes
  publication-title: Restaurator
– volume: 57
  start-page: 163
  year: 2006
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0160
  article-title: Inactivation of fungi from deteriorated paper materials by radiation
  publication-title: Int. Biodeteriorat. Biodegr.
  doi: 10.1016/j.ibiod.2006.02.003
– volume: 26
  start-page: 250
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0122
  article-title: Mass deacidification of papers and books III: Study of a paper strengthening and deacidification process with amino alkyl alkoxy silanes
  publication-title: Restaurator
– volume: 156
  start-page: 253
  year: 2003
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0051
  article-title: Routes of degradation of β-O-4 syringyl and guaiacyl lignin model compounds during photobleaching processes
  publication-title: J. Photochem. Photobiol. A
  doi: 10.1016/S1010-6030(03)00007-8
– volume: 1
  start-page: 921
  year: 2008
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0144
  article-title: Imidazolium-based ionic liquids for the efficient treatment of iron gall inked papers
  publication-title: ChemSusChem
  doi: 10.1002/cssc.200800111
– volume: 17
  start-page: 13
  year: 1981
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0046
  article-title: Generation and reactivities of various types of oxygen radicals
  publication-title: Clin.l Respiratory Physiol.-Bull. Europ. De Physiopathologie Respiratoire
– volume: 46
  start-page: 17
  year: 2017
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0149
  article-title: Study on anti aging and anti fouling properties of cellulose-TiO2 nanocomposites
  publication-title: Papermaking equipment and mater.
– volume: 51
  start-page: 167
  year: 2003
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0086
  article-title: Isolation of fungal species from test samples and maps damaged by foxing, and correlation between these species and the environment
  publication-title: Int. Biodeterior. Biodegrad.
  doi: 10.1016/S0964-8305(02)00137-3
– volume: 33
  start-page: 48
  year: 2012
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0141
  article-title: Sustainability of mass-deacidification. Part II: Evaluation of alkaline reserve
  publication-title: Restaurator
– volume: 4
  start-page: 66
  year: 1979
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0131
  article-title: The washing and aqueous deacidification of paper
  publication-title: The Paper Conservator
  doi: 10.1080/03094227.1979.9638520
– volume: 107
  start-page: 328
  year: 2014
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0026
  article-title: Emissions from polymeric materials: characterised by thermal desorption-gas chromatography
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2013.12.003
– volume: 5
  start-page: 1955
  year: 2010
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0011
  article-title: Deacidification for the conservation and preservation of paper-based works: a review
  publication-title: Bioresources
  doi: 10.15376/biores.5.3.1955-2023
– volume: 16
  start-page: 143
  year: 1995
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0142
  article-title: Phytate - a potential conservation agent for the treatment of ink corrosion caused by iron gall inks
  publication-title: Restaurator
– volume: 22
  start-page: 1
  year: 2001
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0093
  article-title: Characterization of foxing stains by chemical and spectrometric methods
  publication-title: Restaurator
– year: 2012
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0014
– volume: 61
  start-page: 203
  year: 2016
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0029
  article-title: The effect of dust particles on cellulose degradation
  publication-title: Stud. Conserv.
  doi: 10.1179/2047058414Y.0000000158
– volume: 10
  start-page: 19998
  year: 2020
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0078
  article-title: Influence of lignin content in cellulose pulp on paper durability
  publication-title: Scientific Rep.
  doi: 10.1038/s41598-020-77101-2
– volume: 11
  start-page: 165
  year: 1990
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0128
  article-title: Paper deacidification in large workshops: effectiveness and practicability
  publication-title: Restaurator
– start-page: 53
  year: 1998
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0074
– volume: 96
  start-page: 608
  year: 2011
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0025
  article-title: The effect of volatile organic compounds and hypoxia on paper degradation
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2010.12.017
– volume: 25
  start-page: 1539
  year: 2018
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0032
  article-title: Microstructural model in COMSOL packages with simulation to aging behavior of paper materials
  publication-title: Cellulose
  doi: 10.1007/s10570-018-1682-x
– volume: 6
  start-page: 5555
  year: 2018
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0047
  article-title: Hydrolysis of cellobiose and xylan over TiO2-based catalysts
  publication-title: ACS Sustain Chem Eng
  doi: 10.1021/acssuschemeng.8b00486
– volume: 6
  start-page: 27813
  year: 2016
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0153
  article-title: Metal organic frameworks as sorption media for volatile and semi-volatile organic compounds at ambient conditions
  publication-title: Sci. Rep.
  doi: 10.1038/srep27813
– volume: 26
  start-page: 4589
  year: 2019
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0044
  article-title: Paper conservation with an aqueous NaOH/urea cellulose solution
  publication-title: Cellulose
  doi: 10.1007/s10570-019-02375-3
– volume: 5
  start-page: 113
  year: 2004
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0159
  article-title: The recovery of biodeteriorated books and archive documents through gamma radiation: Some considerations on the results achieved
  publication-title: J Cult Herit
  doi: 10.1016/j.culher.2003.07.003
– volume: 30
  start-page: 203
  year: 1981
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0016
  article-title: A review of paper quality and paper chemistry
  publication-title: Library Trends
– volume: 101
  start-page: 1249
  year: 2014
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0107
  article-title: Deterioration of ancient Korean paper (Hanji), treated with beeswax: A mechanistic study
  publication-title: Carbohydr. Polym.
  doi: 10.1016/j.carbpol.2013.10.033
– volume: 24
  start-page: 89
  year: 1998
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0017
  article-title: Aging and stabilization of alkaline paper
  publication-title: J. Pulp Pap. Sci.
– volume: 11
  start-page: 39
  year: 2003
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0040
  article-title: Alkaline degradation of cellulose: mechanisms and kinetics
  publication-title: J. Polym. Environ.
  doi: 10.1023/A:1024267704794
– volume: 614
  start-page: 451
  year: 2022
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0154
  article-title: Environmentally friendly ZnO/Castor oil polyurethane composites for the gas-phase adsorption of acetic acid
  publication-title: J. Colloid Interface Sci.
  doi: 10.1016/j.jcis.2022.01.123
– volume: 18
  start-page: 768
  year: 2018
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0080
  article-title: Lignocellulose degradation: An overview of fungi and fungal enzymes involved in lignocellulose degradation
  publication-title: Eng. Life Sci.
  doi: 10.1002/elsc.201800039
– year: 1934
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0103
– volume: 3
  start-page: 269
  year: 1996
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0106
  article-title: Prediction of paper permanence by accelerated aging II. Comparison of the predictions with natural aging results
  publication-title: Cellulose
  doi: 10.1007/BF02228806
– volume: 18
  start-page: 8198
  year: 2002
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0132
  article-title: Nanotechnologies for conservation of cultural heritage: Paper and canvas deacidification
  publication-title: Langmuir
  doi: 10.1021/la025964d
– volume: 12
  start-page: 445
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0100
  article-title: The influence of levelling-off degree of polymerisation on the kinetics of cellulose degradation
  publication-title: Cellulose
  doi: 10.1007/s10570-005-2206-z
– volume: 547
  start-page: 370
  year: 2019
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0136
  article-title: The carbonation kinetics of calcium hydroxide nanoparticles: A Boundary Nucleation and Growth description
  publication-title: J. Colloid Interface Sci.
  doi: 10.1016/j.jcis.2019.03.089
– volume: 113
  start-page: 7951
  year: 1991
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0012
  article-title: Reactions of anionic nucleophiles with α-D-glucopyranosyl fluoride in aqueous solution through a concerted, ANDN (SN2) mechanism
  publication-title: J. Am. Chem. Soc.
  doi: 10.1021/ja00021a021
– volume: 15
  start-page: 1
  year: 1994
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0116
  article-title: Evaluation of seven mass deacidification treatments
  publication-title: Restaurator
– volume: 46
  start-page: 137
  year: 2007
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0085
  article-title: Foxing on paper: A literature review
  publication-title: J. Am. Inst. Conserv.
  doi: 10.1179/019713607806112378
– volume: 21
  start-page: 85
  year: 2000
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0089
  article-title: Foxing - A new approach to an old problem
  publication-title: Restaurator
– volume: 48
  start-page: 94
  year: 2001
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0092
  article-title: Observations on the foxing of paper (Reprinted)
  publication-title: Int. Biodeterior. Biodegrad.
  doi: 10.1016/S0964-8305(01)00071-3
– volume: 1026
  start-page: 9
  year: 2004
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0101
  article-title: Identification of volatile organic compounds emitted by a naturally aged book using solid-phase microextraction/gas chromatography/mass spectrometry
  publication-title: J. Chromatogr. A
  doi: 10.1016/j.chroma.2003.11.069
– volume: 26
  start-page: 63
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0124
  article-title: Mass deacidification technology in Germany and its quality control
  publication-title: Restaurator
– volume: 1
  start-page: 176
  year: 2004
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0035
  article-title: The design and operation of a passive humidity-controlled cold storage vault using conventional freezer technology and moisture-sealed cabinets
  publication-title: Society for Imaging Sci. Technol.
– volume: 28
  start-page: 47
  year: 2007
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0102
  article-title: Autocatalytic degradation of cellulose paper in sealed vessels
  publication-title: Restaurator
– year: 1994
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0139
– volume: 8
  start-page: 857
  year: 2014
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0019
  article-title: Review of hemicellulose hydrolysis in softwoods and bamboo
  publication-title: Biofuels Bioprod. Biorefin.
  doi: 10.1002/bbb.1517
– volume: 46
  start-page: 181
  year: 2000
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0091
  article-title: Foxing caused by Fungi: twenty-five years of study
  publication-title: Int. Biodeterior. Biodegrad.
  doi: 10.1016/S0964-8305(00)00063-9
– start-page: 81
  year: 2008
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0109
  article-title: A comparison of artificial ageing with 27 years of natural ageing
– volume: 4
  start-page: 1
  year: 2016
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0030
  article-title: The effect of particulate matter on paper degradation
  publication-title: Heritage Sci.
  doi: 10.1186/s40494-016-0071-8
– volume: 14
  start-page: 1
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0031
  article-title: The effects of heating without water removal and drying on the swelling as measured by water retention value and degradation as measured by intrinsic viscosity of cellulose papermaking fibers
  publication-title: Prog. Pap. Recycl.
– volume: 483
  start-page: 159
  year: 2017
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0145
  article-title: The nitroxide Tempo inhibits hydroxyl radical production from the Fenton-like reaction of iron(II)-citrate with hydrogen peroxide
  publication-title: Biochem. Biophys. Res. Commun.
  doi: 10.1016/j.bbrc.2016.12.174
– volume: 116
  start-page: 7557
  year: 1994
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0013
  article-title: Kinetic isotope effect study of transition states for the hydrolyses of α- and β-glucopyranosyl fluorides
  publication-title: J. Am. Chem. Soc.
  doi: 10.1021/ja00096a012
– volume: 670
  start-page: 110
  year: 2019
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0060
  article-title: A review on Fenton process for organic wastewater treatment based on optimization perspective
  publication-title: Sci. Total Environ.
  doi: 10.1016/j.scitotenv.2019.03.180
– volume: 91
  start-page: 3448
  year: 2006
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0112
  article-title: Mass deacidification of papers and books. IV - A study of papers treated with aminoalkylalkoxysilanes and their resistance to ageing
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2006.04.033
– volume: 48
  start-page: 269
  year: 2021
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0009
  article-title: Oxidative degradation of paper-A minireview
  publication-title: J. Cult. Herit.
  doi: 10.1016/j.culher.2021.01.014
– volume: 25
  start-page: 179
  year: 1996
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0002
  article-title: The chemistry of paper conservation
  publication-title: Chem. Soc. Rev.
  doi: 10.1039/cs9962500179
– volume: 107
  start-page: 314
  year: 2014
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0028
  article-title: Characterization and degradation of poly(vinyl acetate)-based adhesives for canvas paintings
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2013.12.028
– volume: 32
  year: 2011
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0041
  article-title: Sustainability of mass deacidification. Part I: Concept, selection of sample books and pH-determination
  publication-title: Restaurator
– volume: 14
  start-page: 171
  year: 2007
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0108
  article-title: Time–temperature superposition method for predicting the permanence of paper by extrapolating accelerated ageing data to ambient conditions
  publication-title: Cellulose
  doi: 10.1007/s10570-007-9114-3
– volume: 89
  start-page: 913
  year: 2010
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0003
  article-title: An overview of the chemical composition of biomass
  publication-title: Fuel
  doi: 10.1016/j.fuel.2009.10.022
– volume: 252
  start-page: 1159
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0161
  article-title: Investigation of the effects of plasma treatments on biodeteriorated ancient paper
  publication-title: Appl. Surf. Sci.
  doi: 10.1016/j.apsusc.2005.02.045
– volume: 95
  start-page: 2300
  year: 2010
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0123
  article-title: Mass deacidification and reinforcement of papers and books VI - Study of aminopropylmethyldiethoxysilane treated papers
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2010.09.002
– start-page: 127
  year: 1979
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0015
– volume: 10
  start-page: 46
  year: 1986
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0155
  article-title: Fumigation quandary: more overkill or common sense?
  publication-title: Unification Elem. Forces Gauge Theor., Pap. Ben Lee Meml. Int. Conf. Parity Nonconserv., Weak Neutral Curr. Gauge Theor.
– volume: 29
  start-page: 184
  year: 2008
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0146
  article-title: New antioxidants for treatment of transition metal containing inks and pigments
  publication-title: Restaurator
– start-page: 22
  year: 2010
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0158
  article-title: Propiedades del papel de celulosa pura irradiado y envejecido
– volume: 92
  start-page: 1476
  year: 2007
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0058
  article-title: The role of transition metals in oxidative degradation of cellulose
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2007.05.006
– volume: 24
  start-page: 4605
  year: 2017
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0004
  article-title: Glucose, not cellobiose, is the repeating unit of cellulose and why that is important
  publication-title: Cellulose
  doi: 10.1007/s10570-017-1450-3
– volume: 21
  start-page: 55
  year: 2000
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0075
  article-title: The influence of light on ageing of newsprint paper
  publication-title: Restaurator
– volume: 12
  start-page: 16
  year: 1971
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0130
  article-title: Chemistry of the deacidification of paper
  publication-title: Bull. Am. Group. Int. Institute for Conserv. Historic and Artistic Works
  doi: 10.2307/3178991
– volume: 2
  start-page: 175
  year: 1978
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0034
  article-title: The effects of temperature and moisture on the accelerated aging of paper
  publication-title: Restaurator
– volume: 17
  start-page: 1519
  year: 2015
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0065
  article-title: Depolymerization of cellulose to glucose by oxidation–hydrolysis
  publication-title: Green Chem.
  doi: 10.1039/C4GC02151G
– volume: 79
  start-page: 383
  year: 2004
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0084
  article-title: Surface analysis of paper documents damaged by foxing
  publication-title: Appl. Phys. a-Mater. Sci. Processing
  doi: 10.1007/s00339-004-2540-2
– volume: 57
  start-page: 1235
  year: 2002
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0090
  article-title: Study of foxing stains on paper by chemical methods, infrared spectroscopy, micro-X-ray fluorescence spectrometry and laser induced breakdown spectroscopy
  publication-title: Spectrochim Acta Part B At Spectrosc
  doi: 10.1016/S0584-8547(02)00056-3
– volume: 27
  start-page: 35
  year: 2006
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0111
  article-title: Patents for paper deacidification
  publication-title: Restaurator
– volume: 16
  start-page: 1004
  year: 2021
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0152
  article-title: Preventing colour fading in artworks with graphene veils
  publication-title: Nat. Nanotechnol.
  doi: 10.1038/s41565-021-00934-z
– volume: 12
  start-page: 4410
  year: 2017
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0110
  article-title: Deacidification of acidic books and paper by means of non-aqueous dispersions of alkaline particles: A review focusing on completeness of the reaction
  publication-title: Bioresources
  doi: 10.15376/biores.12.2.Hubbe
– volume: 9
  start-page: 54
  year: 2008
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0126
  article-title: Mass deacidification of papers and books: V. Fungistatic properties of papers treated with aminoalkylalkoxysilanes
  publication-title: J Cult Herit
  doi: 10.1016/j.culher.2007.12.002
– start-page: 155
  year: 2010
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0073
  article-title: Natural and accelerated ageing of cellulose and paper: a literature review
  publication-title: Cellulose: structure and properties, derivatives and industrial uses
– year: 2001
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0104
– volume: 21
  start-page: 8495
  year: 2005
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0134
  article-title: Nanoparticles of Mg(OH)2: Synthesis and application to paper conservation
  publication-title: Langmuir
  doi: 10.1021/la050564m
– volume: 16
  start-page: 123
  year: 1995
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0113
  article-title: Mass deacidification of archival materials using diethyl zinc
  publication-title: Restaurator
– volume: 10
  start-page: 40
  year: 1986
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0156
  article-title: Biodeterioration of library materials. Disinfection methods and new alternatives
  publication-title: Unification Elem. Forces Gauge Theor., Pap. Ben Lee Meml. Int. Conf. Parity Nonconserv., Weak Neutral Curr. Gauge Theor.
– volume: 245
  year: 2020
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0020
  article-title: Considerations on factors influencing the degradation of cellulose in alum-rosin sized paper
  publication-title: Carbohydr. Polym.
  doi: 10.1016/j.carbpol.2020.116534
– volume: 27
  start-page: 10798
  year: 2021
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0001
  article-title: How science can contribute to the remedial conservation of cultural heritage
  publication-title: Chem.
  doi: 10.1002/chem.202100675
– volume: 165
  start-page: 784
  year: 2010
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0053
  article-title: Dye sensitized visible light degradation of phenolic compounds
  publication-title: Chem. Eng. J.
  doi: 10.1016/j.cej.2010.10.018
– volume: 1
  start-page: 26
  year: 1994
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0008
  article-title: Kinetics and mechanisms of the low-temperature degradation of cellulose
  publication-title: Cellulose
  doi: 10.1007/BF00818797
– volume: 98
  start-page: 1827
  year: 2013
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0024
  article-title: The impact of volatile compounds released by paper on cellulose degradation in ambient hygrothermal conditions
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2013.05.017
– volume: 19
  start-page: 1149
  year: 2012
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0042
  article-title: Is cellulose degradation due to β-elimination processes a threat in mass deacidification of library books?
  publication-title: Cellulose
  doi: 10.1007/s10570-012-9723-3
– volume: 19
  start-page: 609
  year: 1949
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0068
  article-title: The autoxidation of alkali cellulose
  publication-title: Part 2., Textile Res. J.
  doi: 10.1177/004051754901901003
– volume: 4
  start-page: 19
  year: 2007
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0143
  article-title: Stabilisation of iron gall ink: aqueous treatment with magnesium phytate
  publication-title: e-Preserv. Sci.
– volume: 132
  start-page: 157
  year: 2018
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0087
  article-title: Analysis of paper foxing by newly available omics techniques
  publication-title: Int. Biodeterior. Biodegrad.
  doi: 10.1016/j.ibiod.2018.03.005
– year: 1993
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0038
– volume: 8
  start-page: 2688
  year: 2020
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0054
  article-title: Evaluation of ultraviolet light and hydrogen peroxide enhanced ozone oxidation treatment for the production of cellulose nanofibrils
  publication-title: ACS Sustain. Chem. Eng.
  doi: 10.1021/acssuschemeng.9b06028
– volume: 21
  start-page: 401
  year: 2011
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0059
  article-title: Oxidative depolymerization of polysaccharides by reactive oxygen/nitrogen species
  publication-title: Glycobiology
  doi: 10.1093/glycob/cwq171
– volume: 6
  start-page: 18204
  year: 2016
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0052
  article-title: Production of phenolics via photocatalysis of ball milled lignin–TiO2 mixtures in aqueous suspension
  publication-title: RSC Adv.
  doi: 10.1039/C5RA25954A
– volume: 43
  start-page: 393
  year: 1994
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0096
  article-title: Accelerated aging of papers of pure cellulose - Mechanism of cellulose degradation and paper embrittlement
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/0141-3910(94)90011-6
– volume: 41
  start-page: 1073
  year: 2020
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0062
  article-title: Hydroxyl radicals-mediated oxidative cleavage of the glycosidic bond in cellobiose by copper catalysts and its application to low-temperature depolymerization of cellulose
  publication-title: Chin. J. Catal.
  doi: 10.1016/S1872-2067(20)63569-0
– volume: 27
  start-page: 219
  year: 2006
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0007
  article-title: Methodology and criteria for the evaluation of paper conservation interventions - a literature review
  publication-title: Restaurator
– volume: 274
  start-page: 466
  year: 1978
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0083
  article-title: Foxing, a fungal infection of paper
  publication-title: Nature
  doi: 10.1038/274466a0
– volume: 3
  start-page: 29
  year: 2022
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0148
  article-title: Proper exhibition and preventive protection of books and paper
  publication-title: Library Work and Study
– volume: 23
  start-page: 1431
  year: 1979
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0099
  article-title: Thermal-degradation of cellulose in air and nitrogen at low-temperatures
  publication-title: J. Appl. Polym. Sci.
  doi: 10.1002/app.1979.070230513
– volume: 2017
  start-page: 1
  year: 2017
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0049
  article-title: Structural characterization of lignin and its degradation products with spectroscopic methods
  publication-title: J. Spectroscopy
  doi: 10.1155/2017/8951658
– volume: 28
  start-page: 37
  year: 2009
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0147
  article-title: Where archival and fine art conservation meet: Applying iron gall ink antioxidant and deacidification treatments to corrosive copper watercolors
  publication-title: The Book and Paper Group Annual
– volume: 23
  start-page: 39
  year: 2002
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0118
  article-title: Testing CSC Book Saver (R), a commercial deacidification spray
  publication-title: Restaurator
– year: 2013
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0081
– volume: 27
  start-page: 9
  year: 2006
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0137
  article-title: The effect of sodium and calcium ions in the deacidification of paper - A chemo-physical study using thermal analysis
  publication-title: Restaurator
– year: 1977
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0129
– year: 1996
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0079
– volume: 13
  start-page: 1029
  year: 2021
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0036
  article-title: Paper ageing: The effect of paper chemical composition on hydrolysis and oxidation
  publication-title: Polymers (Basel)
  doi: 10.3390/polym13071029
– year: 1976
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0033
– volume: 3
  start-page: 1339
  year: 2015
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0006
  article-title: Acidolysis of α-o-4 aryl-ether bonds in lignin model compounds: a modeling and experimental study
  publication-title: ACS Sustain. Chem. Eng.
  doi: 10.1021/acssuschemeng.5b00070
– volume: 92
  start-page: 1893
  year: 1988
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0057
  article-title: Kinetics for electron transfer from laser-pulse irradiated colloidal semiconductors to adsorbed methylviologen: dependence of the quantum yield on incident pulse width
  publication-title: J. Phys. Chem.
  doi: 10.1021/j100318a039
– year: 1986
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0098
  article-title: Historic textile and paper materials
  publication-title: Conserv. Characteriz.
– volume: 26
  start-page: 429
  year: 2019
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0071
  article-title: Yellowing and brightness reversion of celluloses: CO or COOH, who is the culprit?
  publication-title: Cellulose
  doi: 10.1007/s10570-018-2200-x
– volume: 116
  start-page: 14178
  year: 2012
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0061
  article-title: Ferryl-Oxo species produced from fenton's reagent via a two-step pathway: minimum free-energy path analysis
  publication-title: J. Phys. Chem. B
  doi: 10.1021/jp310008z
– volume: 15
  start-page: 247
  year: 1995
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0077
  article-title: The Role of lignin in the mechanical permanence of paper: Part II. Effect of acid groups
  publication-title: J. Wood Chem. Technol.
  doi: 10.1080/02773819508009510
– volume: 108
  start-page: 1
  year: 1997
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0056
  article-title: An overview of semiconductor photocatalysis
  publication-title: J. Photochem. Photobiol. A
  doi: 10.1016/S1010-6030(97)00118-4
– volume: 23
  start-page: 95
  year: 1932
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0067
  article-title: 9–the oxidation by gaseous oxygen of cotton impregnated with sodium hydroxide solution
  publication-title: J. Textile Institute Trans.
  doi: 10.1080/19447023208661546
– volume: 6
  start-page: 5307
  year: 2011
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0010
  article-title: Paper aging and degradation: recent findings and research methods
  publication-title: Bioresources
  doi: 10.15376/biores.6.4.5307-5337
– year: 2016
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0048
– volume: 16
  start-page: 209
  year: 1995
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0023
  article-title: Effects of air pollutants on the accelerated ageing of cellulose-based materials
  publication-title: Restaurator
– volume: 107
  start-page: 294
  year: 2014
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0027
  article-title: Cross-infection effect of polymers of historic and heritage significance on the degradation of a cellulose reference test material
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2013.12.019
– volume: 3
  start-page: 243
  year: 1996
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0105
  article-title: Prediction of paper permanence by accelerated aging I. Kinetic analysis of the aging process
  publication-title: Cellulose
  doi: 10.1007/BF02228805
– volume: 24
  start-page: 323
  year: 2016
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0115
  article-title: Critical evaluation of approaches toward mass deacidification of paper by dispersed particles
  publication-title: Cellulose
  doi: 10.1007/s10570-016-1112-x
– volume: 20
  start-page: 1
  year: 1999
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0022
  article-title: The effect of air pollutants on paper stability
  publication-title: Restaurator
– volume: 19
  start-page: 135
  year: 1998
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0076
  article-title: The impact of lignin on paper permanence - A comprehensive study of the ageing behaviour of handsheets and commercial paper samples
  publication-title: Restaurator
– volume: 5
  start-page: 407
  year: 1935
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0094
  article-title: Notes on the causes and prevention of foxing in books
  publication-title: Libr. Q.
  doi: 10.1086/613729
– start-page: 361
  year: 1987
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0114
  article-title: Mass deacidification for libraries
  publication-title: Libr. Technol. Rep.
– volume: 3
  start-page: 57
  year: 2015
  ident: 10.1016/j.polymdegradstab.2022.110228_bib0150
  article-title: Research review of nano-TiO2. Its application prospect in museum's environment for conservation
  publication-title: China Cultural Heritage Scientific Res.
SSID ssj0000451
Score 2.5463643
SecondaryResourceType review_article
Snippet •Chemical principles are used to direct the preservation and conservation of paper cultural relics.•The mechanisms of acidic, alkaline and oxidative...
SourceID crossref
elsevier
SourceType Enrichment Source
Index Database
Publisher
StartPage 110228
SubjectTerms Cellulose chemistry
Conservation
Degradation
Paper cultural relics
Title Chemistry directs the conservation of paper cultural relics
URI https://dx.doi.org/10.1016/j.polymdegradstab.2022.110228
Volume 207
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwpV1NS8NAEB1KBT8OolWxfpQ96DG22Wy6DXqwFEtV7MlCb2G_ApXahrYevPjb3ckmbRUPBSGnJLtkH8Psy_LmDcBVxBMZKUM9SXnkMU2FJ1pGewFNTJNbiqKzKv6XfrM3YE_DcFiCTlELg7LKPPe7nJ5l6_xOPUezno5GdZQlWfqCfywYiVkeZoxjlN98rWQe6J_iZIy-h29vw_VK45VOx5_vGl0Z9BwrFKidDIXxFJuz_7VPre093QPYz0kjabvvOoSSmVRgp1P0aqvA3pqt4BHcLp8Qt7o5sTSPKBRO50ewZJqQVKRmRgrrDTIz45GaH8Og-_Da6Xl5kwRPBUGw8ISSiWCcc22pD28JLoUvhJ_oyAIdikCGEdWaK2aXLH0WSiUCGuqkoYW9qB-cQHkynZhTID7WoTphDGNUN6OkxRQajAktw4YRVbgrIIlV7iCOjSzGcSEVe4t_IRojorFDtArN5fDUWWlsOvC-wD_-ERuxTfubTXH2_ynOYRdbzbvjlwsoL2Yf5tISkoWsZRFXg63243Ov_w0n2OL6
linkProvider Elsevier
linkToHtml http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwpV1La8JAEB5EobaH0tqW2uce2mPQbDauoT1UpKL1cVLwFvYVsFgNag_9990xidrSg1DIacMM2Y9hdrJ88w3AQ8AjGShDHUl54DBNhSPqRjsejUyN2xJFr7v4-4Nae8Texv44B82sFwZplWnuT3L6OlunK5UUzUo8mVSQlmTLF_xjwUjEPFxAdSo_D4VGp9sebBMy85OxhMx10OAAHrc0r3g-_frQKMygl9ikQK0_5MZTnM_-11G1c_y0TuA4rRtJI_m0U8iZWQmKzWxcWwmOdpQFz-Bp84YkG1wSW-kRhdzp9BaWzCMSi9gsSKa-QRZmOlHLcxi1XofNtpPOSXCU53krRygZCcY517b64XXBpXCFcCMdWKx94Uk_oFpzxeyWpct8qYRHfR1VtbAPdb0LyM_mM3MJxMVW1IQbwxjVtSCqM4UaY0JLv2pEGZ4zSEKViojjLItpmLHF3sNfiIaIaJggWobaxjxO1DT2NXzJ8A9_hEdoM_9-Lq7-7-Ieiu1hvxf2OoPuNRzi5PnkNuYG8qvFp7m19clK3qXx9w3wp-Wr
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=Chemistry+directs+the+conservation+of+paper+cultural+relics&rft.jtitle=Polymer+degradation+and+stability&rft.au=Zhang%2C+Xu&rft.au=Yan%2C+Yueer&rft.au=Yao%2C+Jingjing&rft.au=Jin%2C+Shutong&rft.date=2023-01-01&rft.pub=Elsevier+Ltd&rft.issn=0141-3910&rft.eissn=1873-2321&rft.volume=207&rft_id=info:doi/10.1016%2Fj.polymdegradstab.2022.110228&rft.externalDocID=S0141391022004062
thumbnail_l http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=0141-3910&client=summon
thumbnail_m http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=0141-3910&client=summon
thumbnail_s http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=0141-3910&client=summon