Hydrothermal Ageing of Metallocene Polyethylene Films in Presence of Grafted Amine Stabilizers

The hydrothermal degradation at 90°C in distilled water of metallocene linear low density polyethylene films (mLLDPE) has been studied using low density polyethylene (LDPE) for comparison. FTIR spectroscopy, DSC and chemiluminescence techniques were used for investigation of the hydrothermal ageing-...

Full description

Saved in:
Bibliographic Details
Published inArabian Journal for Science and Engineering Vol. 40; no. 1; pp. 69 - 80
Main Authors Setnescu, Radu, Kaci, Mustapha, Dehouche, Nadjet, Setnescu, Tanţa, Nasri, Lounis, Zaharescu, Traian
Format Journal Article
LanguageEnglish
Published Berlin/Heidelberg Springer Berlin Heidelberg 01.01.2015
Subjects
Online AccessGet full text

Cover

Loading…
Abstract The hydrothermal degradation at 90°C in distilled water of metallocene linear low density polyethylene films (mLLDPE) has been studied using low density polyethylene (LDPE) for comparison. FTIR spectroscopy, DSC and chemiluminescence techniques were used for investigation of the hydrothermal ageing-induced changes. The stabilization effect of a commercially available HALS, namely Sanduvor PR 31, able to graft on polyolefin structures has been also studied, as well. It was found that intense oxidation process occurs in the case of LDPE: hydroxyl, carbonyl and unsaturated groups were identified in FTIR spectra. mLLDPE reference films presented considerably higher stability as compared to LDPE ones, this behaviour being assigned to the structural peculiarities. Sanduvor PR 31 induced higher stability in LDPE, possibly by grafting mechanism, but it did not present a significant effect in the case of mLLDPE. Besides a possible antagonist interaction with the process stabilizer or a graft-hindering effect of the alkyl side groups, the intrinsic higher stability of the mLLDPE which offers less active sites for grafting could be supposed to explain this lower effectiveness.
AbstractList The hydrothermal degradation at 90 degree C in distilled water of metallocene linear low density polyethylene films (mLLDPE) has been studied using low density polyethylene (LDPE) for comparison. FTIR spectroscopy, DSC and chemiluminescence techniques were used for investigation of the hydrothermal ageing-induced changes. The stabilization effect of a commercially available HALS, namely Sanduvor PR 31, able to graft on polyolefin structures has been also studied, as well. It was found that intense oxidation process occurs in the case of LDPE: hydroxyl, carbonyl and unsaturated groups were identified in FTIR spectra. mLLDPE reference films presented considerably higher stability as compared to LDPE ones, this behaviour being assigned to the structural peculiarities. Sanduvor PR 31 induced higher stability in LDPE, possibly by grafting mechanism, but it did not present a significant effect in the case of mLLDPE. Besides a possible antagonist interaction with the process stabilizer or a graft-hindering effect of the alkyl side groups, the intrinsic higher stability of the mLLDPE which offers less active sites for grafting could be supposed to explain this lower effectiveness.
The hydrothermal degradation at 90°C in distilled water of metallocene linear low density polyethylene films (mLLDPE) has been studied using low density polyethylene (LDPE) for comparison. FTIR spectroscopy, DSC and chemiluminescence techniques were used for investigation of the hydrothermal ageing-induced changes. The stabilization effect of a commercially available HALS, namely Sanduvor PR 31, able to graft on polyolefin structures has been also studied, as well. It was found that intense oxidation process occurs in the case of LDPE: hydroxyl, carbonyl and unsaturated groups were identified in FTIR spectra. mLLDPE reference films presented considerably higher stability as compared to LDPE ones, this behaviour being assigned to the structural peculiarities. Sanduvor PR 31 induced higher stability in LDPE, possibly by grafting mechanism, but it did not present a significant effect in the case of mLLDPE. Besides a possible antagonist interaction with the process stabilizer or a graft-hindering effect of the alkyl side groups, the intrinsic higher stability of the mLLDPE which offers less active sites for grafting could be supposed to explain this lower effectiveness.
Author Setnescu, Tanţa
Setnescu, Radu
Zaharescu, Traian
Dehouche, Nadjet
Nasri, Lounis
Kaci, Mustapha
Author_xml – sequence: 1
  givenname: Radu
  surname: Setnescu
  fullname: Setnescu, Radu
  organization: Faculty of Sciences and Arts, Department of Sciences, Valahia University of Targoviste, National R&D Institute for Electrical Engineering (ICPE-CA)
– sequence: 2
  givenname: Mustapha
  surname: Kaci
  fullname: Kaci, Mustapha
  email: kacimu@yahoo.fr
  organization: Laboratory of Advanced Polymeric Materials (LMPA), Faculty of Technology, Abderrahmane Mira University
– sequence: 3
  givenname: Nadjet
  surname: Dehouche
  fullname: Dehouche, Nadjet
  organization: Laboratory of Advanced Polymeric Materials (LMPA), Faculty of Technology, Abderrahmane Mira University
– sequence: 4
  givenname: Tanţa
  surname: Setnescu
  fullname: Setnescu, Tanţa
  organization: Faculty of Sciences and Arts, Department of Sciences, Valahia University of Targoviste, National R&D Institute for Electrical Engineering (ICPE-CA)
– sequence: 5
  givenname: Lounis
  surname: Nasri
  fullname: Nasri, Lounis
  organization: Laboratory of Advanced Polymeric Materials (LMPA), Faculty of Technology, Abderrahmane Mira University
– sequence: 6
  givenname: Traian
  surname: Zaharescu
  fullname: Zaharescu, Traian
  organization: National R&D Institute for Electrical Engineering (ICPE-CA)
BookMark eNp9kLFOwzAQQC1UJNrCB7BlZAn4Ysd2xqqiLVIRlYAVy00ubSrHLnY6lK8nUZmZTie9d9K9CRk575CQe6CPQKl8isCYKFIKPAUuVaquyDiDAlKeKRiRMTAoUkWz_IZMYjxQKkBJNiZfq3MVfLfH0BqbzHbYuF3i6-QVO2OtL9FhsvH2jN3-bIdl0dg2Jo1LNgEjuhIHehlM3WGVzNqmR947s21s84Mh3pLr2tiId39zSj4Xzx_zVbp-W77MZ-u0ZBl0aSVkXstKZlJywG1ZywJzMHlZgeCKiwy5kQJNRSWFrapQGgalkbymdc5zzqbk4XL3GPz3CWOn2yaWaK1x6E9RgxCUKsZy0aNwQcvgYwxY62NoWhPOGqgeWupLS9231ENLrXonuzixZ90Ogz74U3D9R_9Iv6useT0
CitedBy_id crossref_primary_10_1016_j_polymertesting_2018_01_007
crossref_primary_10_1002_ange_202307573
crossref_primary_10_1016_j_matdes_2016_08_065
crossref_primary_10_1039_D3EW00043E
crossref_primary_10_1002_anie_202307573
Cites_doi 10.1016/j.solener.2007.10.002
10.1016/j.polymertesting.2004.05.002
10.1016/0141-3910(88)90069-9
10.1139/t02-074
10.1016/S0141-3910(98)00048-2
10.1007/s13369-011-0065-5
10.1016/j.resconrec.2007.11.003
10.1002/pen.10691
10.2136/sssaj1986.03615995005000010038x
10.1016/j.polymdegradstab.2003.12.004
10.1002/pol.1967.160050514
10.1002/apmc.1997.052520102
10.1016/j.polymertesting.2010.11.016
10.1016/j.polymertesting.2006.04.010
10.1016/0014-3057(75)90179-2
10.1016/S0141-3910(97)00096-7
10.1002/app.10492
10.1002/app.1992.070450614
10.1351/pac197230010267
10.1002/pen.10293
10.1061/(ASCE)1090-0241(2008)134:7(906)
10.1002/actp.1994.010450207
10.1016/S0141-3910(99)00115-9
10.1021/ma60012a006
10.1002/mame.200500096
10.1680/gein.2009.16.3.183
10.1007/978-3-642-80305-5
10.1002/pen.760300403
10.1016/0141-3910(94)90066-3
10.1080/10236660490920246
10.1016/0141-3910(95)00060-Y
10.1680/gein.2009.16.2.71
10.1061/(ASCE)GT.1943-5606.0000207
10.1002/app.1987.070330302
10.1002/mame.200400001
10.1016/j.jmatprotec.2007.10.062
10.1002/pol.1970.150080519
10.1016/S0141-3910(02)00269-0
10.1016/j.matdes.2009.05.038
10.1002/pol.1960.1204213916
ContentType Journal Article
Copyright King Fahd University of Petroleum and Minerals 2014
Copyright_xml – notice: King Fahd University of Petroleum and Minerals 2014
DBID AAYXX
CITATION
7SR
7TB
7U5
8BQ
8FD
FR3
JG9
KR7
L7M
DOI 10.1007/s13369-014-1478-8
DatabaseName CrossRef
Engineered Materials Abstracts
Mechanical & Transportation Engineering Abstracts
Solid State and Superconductivity Abstracts
METADEX
Technology Research Database
Engineering Research Database
Materials Research Database
Civil Engineering Abstracts
Advanced Technologies Database with Aerospace
DatabaseTitle CrossRef
Materials Research Database
Civil Engineering Abstracts
Engineered Materials Abstracts
Technology Research Database
Mechanical & Transportation Engineering Abstracts
Solid State and Superconductivity Abstracts
Engineering Research Database
Advanced Technologies Database with Aerospace
METADEX
DatabaseTitleList Materials Research Database

DeliveryMethod fulltext_linktorsrc
Discipline Engineering
EISSN 2191-4281
EndPage 80
ExternalDocumentID 10_1007_s13369_014_1478_8
GroupedDBID 06D
0R~
0VY
23M
29~
2KM
30V
4.4
408
5GY
96X
AAJKR
AAPBV
AARTL
AAYIU
AAYQN
AAZMS
ABPTK
ABTHY
ABULA
ACGFS
ACKNC
ADHHG
ADHIR
AEGNC
AEJHL
AENEX
AEPYU
AETCA
AFWTZ
AFZKB
AGDGC
AGWZB
AGYKE
AHYZX
AIIXL
ALMA_UNASSIGNED_HOLDINGS
AMKLP
AMYQR
ANMIH
AYJHY
BGNMA
C1A
ESBYG
ESX
FFXSO
FRRFC
FYJPI
GGRSB
GJIRD
GX1
HF~
HMJXF
HRMNR
HZ~
I0C
IXD
J9A
KOV
M4Y
NU0
O9-
O93
OK1
P9P
R9I
RLLFE
S1Z
S27
S3B
SEG
SHX
T13
U2A
UG4
VC2
W48
WK8
~A9
AAYXX
CITATION
7SR
7TB
7U5
8BQ
8FD
FR3
JG9
KR7
L7M
ID FETCH-LOGICAL-c321t-d675f7d727741ebcf79e51a5cd1648462e4a76ead0701b8de7a31ca74f0f54543
IEDL.DBID AGYKE
ISSN 1319-8025
IngestDate Fri Apr 12 07:07:50 EDT 2024
Fri Aug 23 03:30:13 EDT 2024
Sat Dec 16 12:12:54 EST 2023
IsPeerReviewed true
IsScholarly true
Issue 1
Keywords Hydrothermal ageing
FT-IR
Metallocene LLDPE
Chemiluminescence
DSC
Language English
LinkModel DirectLink
MergedId FETCHMERGED-LOGICAL-c321t-d675f7d727741ebcf79e51a5cd1648462e4a76ead0701b8de7a31ca74f0f54543
Notes ObjectType-Article-1
SourceType-Scholarly Journals-1
ObjectType-Feature-2
content type line 23
PQID 1660083356
PQPubID 23500
PageCount 12
ParticipantIDs proquest_miscellaneous_1660083356
crossref_primary_10_1007_s13369_014_1478_8
springer_journals_10_1007_s13369_014_1478_8
PublicationCentury 2000
PublicationDate 2015-01-01
PublicationDateYYYYMMDD 2015-01-01
PublicationDate_xml – month: 01
  year: 2015
  text: 2015-01-01
  day: 01
PublicationDecade 2010
PublicationPlace Berlin/Heidelberg
PublicationPlace_xml – name: Berlin/Heidelberg
PublicationTitle Arabian Journal for Science and Engineering
PublicationTitleAbbrev Arab J Sci Eng
PublicationYear 2015
Publisher Springer Berlin Heidelberg
Publisher_xml – name: Springer Berlin Heidelberg
References AminM.U.ScottG.TillekeratneL.M.K.Mechanism of the photo-initiation process in polyethyleneEur. Polym. J.197511858910.1016/0014-3057(75)90179-2
WunderlichB.Heat of fusion of polyethyleneJ. Polym. Sci. A19672598798810.1002/pol.1967.160050514
AdamsJ.H.GoodrichJ.E.Analysis of nonvolatile oxidation products of polypropylene. IIProcess. Degrad. J. Polym. Sci. A197081269127710.1002/pol.1970.150080519
CalvertJ.G.PittsJ.N.Photochemistry1966New YorkWiley
LuongoJ.P.Infrared study of oxygenated groups formed in polyethylene during oxidationJ. Polym. Sci.19994213915010.1002/pol.1960.1204213916
Verdu, J.: Vieillissement des Plastiques. Paris, AFNOR (1984)
RoweK.R.IslamM.HsuanY.Effects of thickness on the aging of HDPE geomembranesJ. Geotech. Geoenviron. Eng.201013629930910.1061/(ASCE)GT.1943-5606.0000207
GuermaziN.ElleuchK.AyediH.F.KapsaP.Aging effect on thermal, mechanical and tribological behaviour of polymeric coatings used for pipeline applicationJ. Mater. Process. Technol.200820340441010.1016/j.jmatprotec.2007.10.062
BoubakriS.ElleuchK.GuermaziN.AyediH.F.Investigations on hygrothermal aging of thermoplastic polyurethane materialMater. Design.2009303958396510.1016/j.matdes.2009.05.038
KaciM.TouatiN.SetnescuR.ZaharescuT.SetnescuT.JipaS.Grafting of hindered amine stabilizer in poly(propylene) films under γ-irradiationMacromol. Mater. Eng.200529080280810.1002/mame.200500096
SetnescuR.JipaS.OsawaZ.Chemiluminescence study on the oxidation of several polyolefins—I. Thermal-induced degradation of additive-free polyolefinsPolym. Degrad. Stab.19986037738310.1016/S0141-3910(97)00096-7
SeebaM.ServensC.PouyetJ.Natural and artificial weathering of low density polyethylene (LDPE): calorimetric analysisJ. Appl. Polym. Sci.1992451049105610.1002/app.1992.070450614
FosterG.N.WassermanS.H.YackaD.J.Oxidation behavior and stabilization of metallocene and other polyolefinsAngew. Makromol. Chem.1997252113210.1002/apmc.1997.052520102
Pospí šilJ.Mechanistic action of phenolic antioxidants in polymers—a reviewPolym. Degrad. Stab.19882018120210.1016/0141-3910(88)90069-9
Al-MalaikaS.OmikoredeE.O.ScottG.Mechanisms of antioxidant action: Mechanochemical transformation products of 2,2,6,6-tetramethyl-4-hydroxy-piperidinoxyl in polypropyleneJ. Appl. Polym. Sci.19873370371310.1002/app.1987.070330302
RimalS.RoweR.K.Diffusion modelling of OIT depletion from HDPE geomembrane in landfill applicationsGeosynth. Int.20091618319610.1680/gein.2009.16.3.183
HeW.LiG.KongL.WangH.HuangJ.XuJ.Application of hydrothermal reaction in resource recovery of organic wastesResour. Conserv. Recycl.20085269169910.1016/j.resconrec.2007.11.003
ViebkeJ.HedenqvistM.GeddeU.W.Antioxidant efficiency loss by precipitation and diffusion to surrounding media in polyethylene hot-water pipesPolym. Eng. Sci.1996362896290410.1002/pen.10691
DörnerG.LangR.W.Influence of various stabilizer systems on the ageing behavior of PE–MD: I. Hot-water ageing of compression molded plaquesPolym. Degrad. Stab.19986242143010.1016/S0141-3910(98)00048-2
AstrucA.BartolomeoP.FayolleB.AudouinL.VerduJ.Accelerated oxidative ageing of polypropylene fibers in aqueous medium under high oxygen pressure as studied by thermal analysisPolym. Test.20042391992310.1016/j.polymertesting.2004.05.002
IlieS.D.SetnescuR.LungulescuE.M.MarinescuV.IlieD.SetnescuT.MareşG.Investigations of a mechanically failed cable insulation used in indoor conditionsPolym. Test.20113017318210.1016/j.polymertesting.2010.11.016
GeddeU.W.IfwarsonM.Molecular structure and morphology of crosslinked polyethylene in an aged hot-water pipePolym. Eng. Sci.19903020221010.1002/pen.760300403
GugumusF.Re-examination of the role of hydroperoxides in polyethylene and polypropylene: chemical and physical aspects of hydroperoxides in polyethylenePolym. Degrad. Stab.199549295010.1016/0141-3910(95)00060-Y
GugumusF.Physico-chemical aspects of polyethylene processing in an open mixer. 2. Functional group formation on PELD processingPolym. Degrad. Stab.200067354710.1016/S0141-3910(99)00115-9
CarlssonD.J.WilesD.M.The photodegradation of polypropylene films. II. Photolysis of ketonic oxidation productsMacromolecules1969258759710.1021/ma60012a006
RoweR.K.HoorA.Predicted temperatures and service lives of secondary geomembrane landfill linersGeosynth. Int.200916718210.1680/gein.2009.16.2.71
SetnescuR.KaciM.JipaS.SetnescuT.ZaharescuT.HebalG.BenhamidaA.DjedjelliH.Chemiluminescence study on irradiated low-density polyethylene containing various photo-stabilisersPolym. Degrad. Stab.20048447548110.1016/j.polymdegradstab.2003.12.004
ViebkeJ.GeddeU.W.Assessment of lifetime of hot-water polyethylene pipes based on oxidation induction time dataPolym. Eng. Sci.1998381244125010.1002/pen.10293
KaciM.HebalG.BenhamidaA.BoukerrouA.DjidjelliH.SadounT.Kinetic study of hindred amine light stabilizer photografting in low density polyethylene films under natural weathering conditionsJ. Appl. Polym. Sci.2002841524153210.1002/app.10492
KaciM.TouatiN.SetnescuR.SetnescuT.JipaS.Characterization by chemiluminescence of unstabilized and HALS-stabilized LDPE films exposed to natural weathering conditionsInt. J. Polym. Anal. Charact.2004928528710.1080/10236660490920246
AvissarR.MahrerY.MarguliesL.KatanJ.Field aging of transparent polyethylene mulches: I. Photometric propertiesSoil Sci. Soc. Am. J.19865020220510.2136/sssaj1986.03615995005000010038x
AlbertssonA.C.BarenstedtC.KarlssonS.Abiotic degradation products from enhanced environmentally degradable polyethyleneActa Polym.1994459710310.1002/actp.1994.010450207
KaciM.HebalG.TouatiM.RabouhiA.ZaidiL.DjidjelliH.Kinetic study of hindered amine light stabilizer photografting in poly(propylene) films under natural weathering and accelerated UV conditions: effect of additive concentrationMacromol. Mater. Eng.200428968168710.1002/mame.200400001
RichaudE.FarcasF.FayolleB.AudouinL.VerduJ.Hydroperoxide titration by DSC in thermally oxidized polypropylenePolym. Test.20062582983810.1016/j.polymertesting.2006.04.010
Hariguchi, H.: Bibliography on IR Spectra (in Jpn.). Tokyo, Sankyo Shuppan (1989)
ZweifelH.Stabilization of Polymeric Materials1998BerlinSpringer10.1007/978-3-642-80305-5
ScottG.Atmospheric Oxidation and Antioxidants1993LondonElsevier
MuellerW.JakobI.Oxidative resistance of high-density polyethylene geomembranesPolym. Degrad. Stab.20037916117210.1016/S0141-3910(02)00269-0
ScottG.Mechanism of polymer stabilizationPure Appl. Chem.19723026728910.1351/pac197230010267
GijsmanP.The mechanism of action of hindered amine stabilizers (HAS) as long-term heat stabilizersPolym. Degrad. Stab.19944317117610.1016/0141-3910(94)90066-3
RoweK.R.RimalS.Aging of HDPE geomembrane in three composite landfill liner configurationsJ. Geotech. Geoenviron. Eng.200813490691610.1061/(ASCE)1090-0241(2008)134:7(906)
AllenN.S.EdgeM.Applied Science1992LondonElsevier
KerbouaN.MoussacebK.KaciM.BenachourD.SadounT.RoubaN.Modeling of the kinetic degradation of unstabilized and HALS-stabilized LDPE films in natural agingArab. J. Sci. Eng.20123654155210.1007/s13369-011-0065-5
MittelmanG.DavidsonJ.H.MantellS.C.SuY.Prediction of polymer tube life for solar hot water systems: a model of antioxidant lossSolar Energy20088245246110.1016/j.solener.2007.10.002
Bădilescu, S.; Toader, M.; Giurginca, M.; Tălpuş,V.: Infrared Spectroscopy of Polymers and Additives (in Roum.). Ed Tehnica, Bucharest (1982)
SangamH.P.Kerry RoweR.Effects of exposure conditions on the depletion of antioxidants from high-density polyethylene (HDPE) geomembranesCan. Geotech. J.2002391221123010.1139/t02-074
ASTM D 3895-07: Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry
M. Kaci (1478_CR27) 2004; 289
D.J. Carlsson (1478_CR47) 1969; 2
G. Scott (1478_CR6) 1972; 30
K.R. Rowe (1478_CR21) 2010; 136
S. Boubakri (1478_CR24) 2009; 30
S.D. Ilie (1478_CR33) 2011; 30
G.N. Foster (1478_CR2) 1997; 252
M. Seeba (1478_CR39) 1992; 45
G. Scott (1478_CR5) 1993
N.S. Allen (1478_CR31) 1992
B. Wunderlich (1478_CR38) 1967; 2
S. Al-Malaika (1478_CR7) 1987; 33
W. Mueller (1478_CR16) 2003; 79
M. Kaci (1478_CR28) 2004; 9
P. Gijsman (1478_CR8) 1994; 43
N. Kerboua (1478_CR9) 2012; 36
M. Kaci (1478_CR29) 2005; 290
1478_CR37
F. Gugumus (1478_CR43) 1995; 49
W. He (1478_CR10) 2008; 52
S. Rimal (1478_CR19) 2009; 16
1478_CR1
J.G. Calvert (1478_CR35) 1966
H.P. Sangam (1478_CR17) 2002; 39
M. Kaci (1478_CR26) 2002; 84
R. Setnescu (1478_CR30) 2004; 84
M.U. Amin (1478_CR45) 1975; 11
H. Zweifel (1478_CR3) 1998
J. Pospí šil (1478_CR4) 1988; 20
R. Avissar (1478_CR22) 1986; 50
A.C. Albertsson (1478_CR25) 1994; 45
G. Dörner (1478_CR14) 1998; 62
1478_CR40
J. Viebke (1478_CR11) 1998; 38
J.P. Luongo (1478_CR44) 1999; 42
R.K. Rowe (1478_CR20) 2009; 16
G. Mittelman (1478_CR15) 2008; 82
K.R. Rowe (1478_CR18) 2008; 134
N. Guermazi (1478_CR23) 2008; 203
F. Gugumus (1478_CR41) 2000; 67
J. Viebke (1478_CR12) 1996; 36
U.W. Gedde (1478_CR13) 1990; 30
R. Setnescu (1478_CR32) 1998; 60
E. Richaud (1478_CR36) 2006; 25
J.H. Adams (1478_CR46) 1970; 8
1478_CR42
A. Astruc (1478_CR34) 2004; 23
References_xml – volume: 82
  start-page: 452
  year: 2008
  ident: 1478_CR15
  publication-title: Solar Energy
  doi: 10.1016/j.solener.2007.10.002
  contributor:
    fullname: G. Mittelman
– ident: 1478_CR42
– volume: 23
  start-page: 919
  year: 2004
  ident: 1478_CR34
  publication-title: Polym. Test.
  doi: 10.1016/j.polymertesting.2004.05.002
  contributor:
    fullname: A. Astruc
– ident: 1478_CR40
– volume: 20
  start-page: 181
  year: 1988
  ident: 1478_CR4
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/0141-3910(88)90069-9
  contributor:
    fullname: J. Pospí šil
– volume: 39
  start-page: 1221
  year: 2002
  ident: 1478_CR17
  publication-title: Can. Geotech. J.
  doi: 10.1139/t02-074
  contributor:
    fullname: H.P. Sangam
– volume: 62
  start-page: 421
  year: 1998
  ident: 1478_CR14
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/S0141-3910(98)00048-2
  contributor:
    fullname: G. Dörner
– volume: 36
  start-page: 541
  year: 2012
  ident: 1478_CR9
  publication-title: Arab. J. Sci. Eng.
  doi: 10.1007/s13369-011-0065-5
  contributor:
    fullname: N. Kerboua
– volume: 52
  start-page: 691
  year: 2008
  ident: 1478_CR10
  publication-title: Resour. Conserv. Recycl.
  doi: 10.1016/j.resconrec.2007.11.003
  contributor:
    fullname: W. He
– volume: 36
  start-page: 2896
  year: 1996
  ident: 1478_CR12
  publication-title: Polym. Eng. Sci.
  doi: 10.1002/pen.10691
  contributor:
    fullname: J. Viebke
– volume: 50
  start-page: 202
  year: 1986
  ident: 1478_CR22
  publication-title: Soil Sci. Soc. Am. J.
  doi: 10.2136/sssaj1986.03615995005000010038x
  contributor:
    fullname: R. Avissar
– volume: 84
  start-page: 475
  year: 2004
  ident: 1478_CR30
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/j.polymdegradstab.2003.12.004
  contributor:
    fullname: R. Setnescu
– volume: 2
  start-page: 987
  issue: 5
  year: 1967
  ident: 1478_CR38
  publication-title: J. Polym. Sci. A
  doi: 10.1002/pol.1967.160050514
  contributor:
    fullname: B. Wunderlich
– volume: 252
  start-page: 11
  year: 1997
  ident: 1478_CR2
  publication-title: Angew. Makromol. Chem.
  doi: 10.1002/apmc.1997.052520102
  contributor:
    fullname: G.N. Foster
– volume: 30
  start-page: 173
  year: 2011
  ident: 1478_CR33
  publication-title: Polym. Test.
  doi: 10.1016/j.polymertesting.2010.11.016
  contributor:
    fullname: S.D. Ilie
– volume: 25
  start-page: 829
  year: 2006
  ident: 1478_CR36
  publication-title: Polym. Test.
  doi: 10.1016/j.polymertesting.2006.04.010
  contributor:
    fullname: E. Richaud
– volume: 11
  start-page: 85
  year: 1975
  ident: 1478_CR45
  publication-title: Eur. Polym. J.
  doi: 10.1016/0014-3057(75)90179-2
  contributor:
    fullname: M.U. Amin
– volume: 60
  start-page: 377
  year: 1998
  ident: 1478_CR32
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/S0141-3910(97)00096-7
  contributor:
    fullname: R. Setnescu
– volume: 84
  start-page: 1524
  year: 2002
  ident: 1478_CR26
  publication-title: J. Appl. Polym. Sci.
  doi: 10.1002/app.10492
  contributor:
    fullname: M. Kaci
– volume: 45
  start-page: 1049
  year: 1992
  ident: 1478_CR39
  publication-title: J. Appl. Polym. Sci.
  doi: 10.1002/app.1992.070450614
  contributor:
    fullname: M. Seeba
– volume: 30
  start-page: 267
  year: 1972
  ident: 1478_CR6
  publication-title: Pure Appl. Chem.
  doi: 10.1351/pac197230010267
  contributor:
    fullname: G. Scott
– volume: 38
  start-page: 1244
  year: 1998
  ident: 1478_CR11
  publication-title: Polym. Eng. Sci.
  doi: 10.1002/pen.10293
  contributor:
    fullname: J. Viebke
– volume: 134
  start-page: 906
  year: 2008
  ident: 1478_CR18
  publication-title: J. Geotech. Geoenviron. Eng.
  doi: 10.1061/(ASCE)1090-0241(2008)134:7(906)
  contributor:
    fullname: K.R. Rowe
– volume-title: Atmospheric Oxidation and Antioxidants
  year: 1993
  ident: 1478_CR5
  contributor:
    fullname: G. Scott
– volume: 45
  start-page: 97
  year: 1994
  ident: 1478_CR25
  publication-title: Acta Polym.
  doi: 10.1002/actp.1994.010450207
  contributor:
    fullname: A.C. Albertsson
– volume: 67
  start-page: 35
  year: 2000
  ident: 1478_CR41
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/S0141-3910(99)00115-9
  contributor:
    fullname: F. Gugumus
– volume: 2
  start-page: 587
  year: 1969
  ident: 1478_CR47
  publication-title: Macromolecules
  doi: 10.1021/ma60012a006
  contributor:
    fullname: D.J. Carlsson
– volume: 290
  start-page: 802
  year: 2005
  ident: 1478_CR29
  publication-title: Macromol. Mater. Eng.
  doi: 10.1002/mame.200500096
  contributor:
    fullname: M. Kaci
– volume: 16
  start-page: 183
  year: 2009
  ident: 1478_CR19
  publication-title: Geosynth. Int.
  doi: 10.1680/gein.2009.16.3.183
  contributor:
    fullname: S. Rimal
– volume-title: Stabilization of Polymeric Materials
  year: 1998
  ident: 1478_CR3
  doi: 10.1007/978-3-642-80305-5
  contributor:
    fullname: H. Zweifel
– volume: 30
  start-page: 202
  year: 1990
  ident: 1478_CR13
  publication-title: Polym. Eng. Sci.
  doi: 10.1002/pen.760300403
  contributor:
    fullname: U.W. Gedde
– volume: 43
  start-page: 171
  year: 1994
  ident: 1478_CR8
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/0141-3910(94)90066-3
  contributor:
    fullname: P. Gijsman
– volume: 9
  start-page: 285
  year: 2004
  ident: 1478_CR28
  publication-title: Int. J. Polym. Anal. Charact.
  doi: 10.1080/10236660490920246
  contributor:
    fullname: M. Kaci
– ident: 1478_CR37
– volume-title: Photochemistry
  year: 1966
  ident: 1478_CR35
  contributor:
    fullname: J.G. Calvert
– volume: 49
  start-page: 29
  year: 1995
  ident: 1478_CR43
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/0141-3910(95)00060-Y
  contributor:
    fullname: F. Gugumus
– volume-title: Applied Science
  year: 1992
  ident: 1478_CR31
  contributor:
    fullname: N.S. Allen
– volume: 16
  start-page: 71
  year: 2009
  ident: 1478_CR20
  publication-title: Geosynth. Int.
  doi: 10.1680/gein.2009.16.2.71
  contributor:
    fullname: R.K. Rowe
– volume: 136
  start-page: 299
  year: 2010
  ident: 1478_CR21
  publication-title: J. Geotech. Geoenviron. Eng.
  doi: 10.1061/(ASCE)GT.1943-5606.0000207
  contributor:
    fullname: K.R. Rowe
– volume: 33
  start-page: 703
  year: 1987
  ident: 1478_CR7
  publication-title: J. Appl. Polym. Sci.
  doi: 10.1002/app.1987.070330302
  contributor:
    fullname: S. Al-Malaika
– volume: 289
  start-page: 681
  year: 2004
  ident: 1478_CR27
  publication-title: Macromol. Mater. Eng.
  doi: 10.1002/mame.200400001
  contributor:
    fullname: M. Kaci
– ident: 1478_CR1
– volume: 203
  start-page: 404
  year: 2008
  ident: 1478_CR23
  publication-title: J. Mater. Process. Technol.
  doi: 10.1016/j.jmatprotec.2007.10.062
  contributor:
    fullname: N. Guermazi
– volume: 8
  start-page: 1269
  year: 1970
  ident: 1478_CR46
  publication-title: Process. Degrad. J. Polym. Sci. A
  doi: 10.1002/pol.1970.150080519
  contributor:
    fullname: J.H. Adams
– volume: 79
  start-page: 161
  year: 2003
  ident: 1478_CR16
  publication-title: Polym. Degrad. Stab.
  doi: 10.1016/S0141-3910(02)00269-0
  contributor:
    fullname: W. Mueller
– volume: 30
  start-page: 3958
  year: 2009
  ident: 1478_CR24
  publication-title: Mater. Design.
  doi: 10.1016/j.matdes.2009.05.038
  contributor:
    fullname: S. Boubakri
– volume: 42
  start-page: 139
  year: 1999
  ident: 1478_CR44
  publication-title: J. Polym. Sci.
  doi: 10.1002/pol.1960.1204213916
  contributor:
    fullname: J.P. Luongo
SSID ssj0061873
ssj0001916267
Score 2.0576196
Snippet The hydrothermal degradation at 90°C in distilled water of metallocene linear low density polyethylene films (mLLDPE) has been studied using low density...
The hydrothermal degradation at 90 degree C in distilled water of metallocene linear low density polyethylene films (mLLDPE) has been studied using low density...
SourceID proquest
crossref
springer
SourceType Aggregation Database
Publisher
StartPage 69
SubjectTerms Degradation
Density
Distilled water
Engineering
Grafting
Humanities and Social Sciences
Metallocenes
multidisciplinary
Polyethylenes
Research Article - Chemistry
Science
Spectra
Stability
Stabilization
Title Hydrothermal Ageing of Metallocene Polyethylene Films in Presence of Grafted Amine Stabilizers
URI https://link.springer.com/article/10.1007/s13369-014-1478-8
https://search.proquest.com/docview/1660083356
Volume 40
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwlV1LSwMxEA62XvTgW3wTwZOypdnNZtNjEduiVHqwUC8ueYrYbqXdHuyvd7IP6_PQy8IuYWAzycw3M_kmCF1YYRXRlHvGSuXRBhOeDE3D48zUVWTBYTLHRu7es06f3g7CwQryP1MXyWutrEhmhnrBdQsC5o72UI9QiHx4Ba0WvNPVZvvx7ktmBRBPdq1Sbo8Z4VmdmTi6DgcXX9Y2_xL63TstIOePKmnmfFqbOSFwmvUsdGdOXmuzVNbU_HdHxyX-awttFFgUN_PFs41WTLKD1r90KNxFT513PclIWiM38tnAVzy2uGtSV7FXYClxbzx8N6DvoXtpvQxHU_yS4F7Ga1LGjW5P3FXkGjdHIBkDvnUncucAPPdQv3XzcN3xiisZPBX4JPU0xBc20gB6AIkYqWzUMCERodIQdgGU8Q0VEYPVCZaESK5NJAKiRERt3QJWo8E-qibjxBwgHFpfBTLQslHX1AoiLLXSUsa5DiNL2CG6LFURv-WdN-JFj2U3aTFMWuwmLeaH6LxUVgz7wxU9RGLGs2lMGHMwMwhB4FWpgbjYqNP_JR4tNfoYrQGSCvPczAmqppOZOQW0ksqzYnmeoUp7QODZ95sftDvhyA
link.rule.ids 315,783,787,27936,27937,41093,41535,42162,42604,52123,52246
linkProvider Springer Nature
linkToHtml http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwlV07T8MwELagDMCAeIryNBITKFKdOI47VogSoK06tBITluMHqtSmqGmH8us5p4kCCAbGRKcbzue773wvhK6ttIpoyj1jE-XRJpNeEpqmx5lpqMiCw2SuG7nbY_GQPr2EL0Ufd1ZWu5cpydxSV81uQcBcbQ_1CIXQh6-jDTde3Q3MH_qt6mEFAE--VWlljhnheZqZuG4dDh6-TG3-xvK7c6oQ548kae572rtopwCNuLU65T20ZtJ9tP1llOABeo2XepZ3U00c5ZuBv3hqcdfMXWpdgUnD_el4aeBgxu6jPRpPMjxKcT9vQFLGUT_M3M5wjVsT4IwBiLrS2Q9AiIdo2L4f3MVesTvBU4FP5p6GQMBGGtAJQAaTKBs1TUhkqDTER4A5fENlxECN4MqThGsTyYAoGVHbsACqaHCEauk0NccIh9ZXQRLopNnQ1EoiLbWJpYxzHUaWsDq6KYUm3lcjMkQ1DNlJWICEhZOw4HV0VYpVgCK77IRMzXSRCcKYw4NBCAxvS3mL4kZlf3M8-Rf1JdqMB92O6Dz2nk_RFsCfcPWgcoZq89nCnAPEmCcXuUp9AjxQxvQ
linkToPdf http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwpV1LTxsxEB7RIKFy4NVWvGskTqCFOOv1OscICGl5KIci0UtdPytEskHJ5gC_nvE-FIroAfW4q9FI9oxnPnteAPteeUMtE5Hz2kSszVWkE9eOBHdNk3p0mDxUI19d894N-36b3FZzTid1tnsdkixrGkKXpiw_frD-eFb4Fsc85PmwiDK8BokPMM9CY6QGzHfOf168eGZB-FPMWCqNM6eiCDrTULsj0N_Xgc63mP7tqmb481XItPBE3WX4Xa-hTEC5P5rm-sg8vWrv-B-LXIGlCqWSTqlWqzDnsjVYfNG78BP86j3acVG-NQyUfxz-JSNPrlweYvkGbSjpjwaPDjVhED66d4PhhNxlpF9UPBkXqM_HYUi5JZ0hciaIfEOu7hNC0s9w0z37cdKLqmENkYlbNI8s3jx8ahEOIUZx2vi07RKqEmPxQoYgp-WYSjnqLdoYqoV1qYqpUSnzTY8ojsVfoJGNMrcOJPEtE-vY6nbTMq-o8sxrz7gQNkk95RtwUMtFPpQ9OeSs-3LYNImbJsOmSbEBe7XkJJ6cEA5RmRtNJ5JyHgBonCDDw1oasjrCk39z3HwX9VdY6J925eW364st-IhwKykfcLahkY-nbgchTa53K7V9BvPt7KY
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=Hydrothermal+Ageing+of+Metallocene+Polyethylene+Films+in+Presence+of+Grafted+Amine+Stabilizers&rft.jtitle=Arabian+Journal+for+Science+and+Engineering&rft.au=Setnescu%2C+Radu&rft.au=Kaci%2C+Mustapha&rft.au=Dehouche%2C+Nadjet&rft.au=Setnescu%2C+Tant%CC%A7a&rft.date=2015-01-01&rft.pub=Springer+Berlin+Heidelberg&rft.issn=1319-8025&rft.eissn=2191-4281&rft.volume=40&rft.issue=1&rft.spage=69&rft.epage=80&rft_id=info:doi/10.1007%2Fs13369-014-1478-8&rft.externalDocID=10_1007_s13369_014_1478_8
thumbnail_l http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=1319-8025&client=summon
thumbnail_m http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=1319-8025&client=summon
thumbnail_s http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=1319-8025&client=summon