Effect of Yb2O3 and TiO2 on reaction sintering and properties of magnesium aluminate spinel

Magnesium aluminate spinel with an initial MgO: Al2O3 molar ratio of 2:1 was prepared from its constituent oxides through a solid-state sintering process at temperatures ranging from 1550 to 1700 °C in a normal air atmosphere. The effect of varying amount (0.25–1.0 wt%) of TiO2 and Yb2O3 on densific...