Effects of Cu/Si on the microstructure and tribological properties of FeCoCrNi high entropy alloy coating by laser cladding

High entropy alloy coatings show great potential for improving the wear resistance of the stainless-steel substrate. However, there are few comparative studies on the tribological properties of high entropy alloy coatings with different elements. In the present study, the FeCoCrNiCux and FeCoCrNiSix...

Full description

Saved in:
Bibliographic Details
Published inWear Vol. 512-513; p. 204533
Main Authors Zhu, Zheng-Xing, Liu, Xiu-Bo, Liu, Yi-Fan, Zhang, Shi-Yi, Meng, Yuan, Zhou, Hai-Bin, Zhang, Shi-Hong
Format Journal Article
LanguageEnglish
Published Elsevier B.V 15.01.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:High entropy alloy coatings show great potential for improving the wear resistance of the stainless-steel substrate. However, there are few comparative studies on the tribological properties of high entropy alloy coatings with different elements. In the present study, the FeCoCrNiCux and FeCoCrNiSix high entropy alloy coatings were designed and prepared by laser cladding. The microstructures of the high entropy coating were analyzed. The tribological properties of the high entropy alloy coatings sliding against Si3N4 balls at room temperature and 600 °C were investigated. The results show that after adding Cu/Si, the tribological properties of the coating change little at room temperature, but increased significantly at high temperature of 600 °C. The FeCoCrNiSi coating has the best tribological performance at 600 °C with an average friction coefficient and wear rate of 0.19 and 0.677 (×10−4 mm3/N·m), respectively. In general, the addition of Cu increases the thermal conduction ability of the coating, improves the toughness and the bonding strength of the coating; the addition of Si refines the grain size, increases the degree of work hardening and improves the wear resistance of the coating. •The effect of Cu/Si on laser cladding FeCoCrNi coatings was investigated.•The addition of Cu/Si in equal molar ratio at room temperature improved wear resistance of FeCoCrNi coating.•At 600 °C, the addition of Cu/Si both improved the tribological properties of FeCoCrNi coating.•The FeCoCrNiSi coating showed the best tribological performance at high temperature (600 °C).