Ye, F., Meng, F., Luo, T., & Qi, H. (2022). Ultrafast high-temperature sintering of (Y0.2Dy0.2Er0.2Tm0.2Yb0.2)4Hf3O12 high-entropy ceramics with defective fluorite structure. Journal of the European Ceramic Society, 42(11), 4686-4691. https://doi.org/10.1016/j.jeurceramsoc.2022.04.023
Chicago Style (17th ed.) CitationYe, Fuxing, Fanwei Meng, Tianyuan Luo, and Hang Qi. "Ultrafast High-temperature Sintering of (Y0.2Dy0.2Er0.2Tm0.2Yb0.2)4Hf3O12 High-entropy Ceramics with Defective Fluorite Structure." Journal of the European Ceramic Society 42, no. 11 (2022): 4686-4691. https://doi.org/10.1016/j.jeurceramsoc.2022.04.023.
MLA (9th ed.) CitationYe, Fuxing, et al. "Ultrafast High-temperature Sintering of (Y0.2Dy0.2Er0.2Tm0.2Yb0.2)4Hf3O12 High-entropy Ceramics with Defective Fluorite Structure." Journal of the European Ceramic Society, vol. 42, no. 11, 2022, pp. 4686-4691, https://doi.org/10.1016/j.jeurceramsoc.2022.04.023.