Suppressing the P2–OP4 phase transition of single-crystal P2-type Ni/Zn/Mn-based layered oxide for advanced sodium-ion batteries
P2-type layered Na0.66Ni0.26Zn0.07Mn0.67O2 (NNZM) is expected to be a competitive alternative to lithium layered oxide due to its high-energy-density, low production cost, and high-speed Na+ ion transport channels. However, it is still necessary to further improve its air stability and cycle life to...
Saved in:
Published in | Powder technology Vol. 448; p. 120314 |
---|---|
Main Authors | , , , , , , , |
Format | Journal Article |
Language | English |
Published |
Elsevier B.V
01.12.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | P2-type layered Na0.66Ni0.26Zn0.07Mn0.67O2 (NNZM) is expected to be a competitive alternative to lithium layered oxide due to its high-energy-density, low production cost, and high-speed Na+ ion transport channels. However, it is still necessary to further improve its air stability and cycle life to meet the needs of practical applications. Single crystals with micron-scale have smaller specific surface area and greater packing density, which can improve air stability and cycle life compared to the traditional polycrystalline. Herein, single-crystal Na0.66Ni0.26Zn0.07Mn0.67O2 (SC-NNZM) is prepared by using Na2MoO4 as the molten salt. Driven by molten salt Na2MoO4, regular hexagonal prism morphology SC-NNZM with a median diameter (D50) of 7.86 μm and the (001) plane-dominated structure is obtained, larger than that (5.05 μm) of single-crystal C-NNZM without Na2MoO4, implying that specific surface area of SC-NNZM is smaller than that of C-NNZM, thereby reducing the contact area of SC-NNZM with the electrolyte, which is good for suppressing both harmful interface side-reactions and phase transitions at high voltages. Therefore, SC-NNZM exhibits 95.44 % capacity retention at 100 mA g−1 after 100 cycles, higher than C-NNZM (86.09 %). Moreover, rate capability of SC-NNZM is also higher than that of C-NNZM. This study provides a new strategy for inducing crystal plane growth that is conducive to the structure stability of single-crystal layered oxide at high voltages.
[Display omitted]
•Single-crystal P2-type layered Na0.66Ni0.26Zn0.07Mn0.67O2 (SC-NNZM) has (001) plane-dominated structure.•SC-NNZM has smaller specific surface area and faster Na+ ion diffusion kinetics.•SC-NNZM has larger the (002) interplanar spacing and smaller lattice strain.•P2–OP4 phase transition of SC-NNZM at high voltage is restrained.•SC-NNZM can delivers excellent cycling stability and rate capability. |
---|---|
ISSN: | 0032-5910 |
DOI: | 10.1016/j.powtec.2024.120314 |